Electrical Properties and Relaxor Phase Evolution of Li‐Modified BNT‐BKT‐BT Lead‐Free Ceramics
Authors:Ye‐Jing Dai  Zhe Zhao  Xiao‐Wen Zhang  Si‐Hui Wang
Affiliation:1. Key Laboratory of Advanced Ceramics and Machining Technology, Ministry of Education, School of Materials Science and Engineering, Tianjin University, Tianjin, China;2. The State Key Laboratory of New Ceramics and Fine Processing, School of Materials Science and Engineering, Tsinghua University, Beijing, China
Abstract:By conventional ceramics sintering technique, the lead‐free 0.85Bi0.5Na0.5(1?x)Li0.5xTiO3‐0.11Bi0.5K0.5TiO3‐0.04BaTiO3 (x =0–0.15) piezoelectric ceramics were obtained and the effects of Li dopant on the piezoelectric, dielectric, and ferroelectric properties were studied. With increasing Li addition, the temperature‐dependent permittivity exhibited the normal ferroelectric‐to‐ergodic relaxor (FE‐to‐ER) transition temperature (TFEER, abbreviated as TF‐R) decreasing down to room temperature. The increasing Li content also enhanced the diffuseness of the FE‐to‐ER transition behavior. For composition with x = 0.15, a large unipolar strain of 0.37% (urn:x-wiley:00027820:media:jace14247:jace14247-math-0001 = Smax/Emax = 570 pm/V) was achieved under 6.5 kV/mm applied electric field at room temperature. Both unipolar and bipolar strain curves related to the temperature closely, and when the temperature reached the TF‐R, the normalized strain urn:x-wiley:00027820:media:jace14247:jace14247-math-0002 achieved a maximum value (e.g., for x = 0.10, urn:x-wiley:00027820:media:jace14247:jace14247-math-0003 = 755 pm/V) owing to the electric‐field‐induced ER‐to‐FE state transition.
Keywords:strain  relaxors  ferroelectricity/ferroelectric materials  lead‐free ceramics
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司    京ICP备09084417号-23

京公网安备 11010802026262号