首页 | 官方网站   微博 | 高级检索  
     

太钢60 t EAF-LF-VD-2.5 t铸锭流程冶炼低钛轴承GGrl5钢的实践
引用本文:邬中华.太钢60 t EAF-LF-VD-2.5 t铸锭流程冶炼低钛轴承GGrl5钢的实践[J].特殊钢,2019,40(1):57-59.
作者姓名:邬中华
作者单位:山西太钢不锈钢股份有限公司技术中心,太原030003
摘    要:

收稿时间:2018-08-23

Practice of Low Titanium Bearing Steel GCrl5 Steelmaking by 60 t EAF-LF-VD-2.5 t Ingot Flowsheet at Taigang
Wu Zhonghua.Practice of Low Titanium Bearing Steel GCrl5 Steelmaking by 60 t EAF-LF-VD-2.5 t Ingot Flowsheet at Taigang[J].Special Steel,2019,40(1):57-59.
Authors:Wu Zhonghua
Affiliation:Technology Center,Shanxi Taigang Stainless steel Co Ltd,Taiyuan 030003
Abstract:With the process measures including using low titanium hot metal, alloys and slagging materials, eccentric bottom tapping and alloying in tapping in EAF steelmaking, using Si-Al compound deoxidation and CaO-MgO-SiO2 -Al2O3 slag series with basicity 3 ~5 in LF refining,30 Pa VD treatment and shielding casting,the analysis results of Φ150 mm forged bar are oxygen content in GCrl5 bearing steel being 4.5 X 10-6 ~9 x 10-6 ,Ti content 0.0010% ~0.0015% with minor 5 μm TiN inclusions to meet the quality requirement for super grade quality low titanium bearing steel.
Keywords:
点击此处可从《特殊钢》浏览原始摘要信息
点击此处可从《特殊钢》下载全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司    京ICP备09084417号-23

京公网安备 11010802026262号