首页 | 本学科首页   官方微博 | 高级检索  
相似文献
 共查询到20条相似文献,搜索用时 31 毫秒
1.
Hemp fibers and particles, with different sizes and contents, were used to make hybrid composites based on recycled polypropylene (PP). In particular, the effect of maleated polypropylene (MAPP) addition on the morphology and mechanical properties is reported. The results show that better adhesion is obtained with MAPP addition. In general, fiber content and size had a substantial effect on the tensile, flexural, torsion, and impact properties of the resulting composites. Although, adding MAPP to the samples improved the impact strength of the composites, the values were always lower than neat PP. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2012  相似文献   

2.
Composites consisting of a polypropylene (PP) and highly crystalline cellulosic microfibers were prepared by melting mixing with the maleic anhydride grafted polypropylene (MAPP) as a compatibilizer. The results show that even with addition of a small amount of MAPP, the mechanical properties of the composites improved dramatically. The improvement is attributed to stronger interfacial adhesion caused by esterification between anhydride groups of MAPP and hydroxyl groups of cellulose, although the number of the ester bonds is too few to be detected by FT‐IR spectroscopy. It was also found that tensile strength and Young's modulus increased with the increasing MAPP contents in the composites, and the optimum MAPP content is about 10 wt% for the composite with cellulose content of 30 wt%. SEM indicated that the interfacial adhesion between cellulose fibers and PP improved in MAPP‐containing composites. The DSC results showed that MAPP has little effect on melting and crystallization temperatures of PP in the composites. POLYM. COMPOS., 26:448–453, 2005. © 2005 Society of Plastics Engineers  相似文献   

3.
《Polymer Composites》2017,38(5):863-869
Water absorption and mechanical performance of the injection‐molded hybrid composites prepared from different ratios of two polymer blends (57 wt%), two compatibilizers (3 wt%), and two wood species (40 wt%) were investigated. The ratio of polypropylene and high‐impact polystyrene (HIPS) gradually increased in the blend (from 10 to 30 wt%). Styrene–ethylene–butylene–styreneblock copolymer and maleic anhydride‐grafted PP (MAPP) were used as compatibilizer (3 wt%). The shore D hardness of the PP/wood composites was improved by the incorporation of the HIPS. The HIPS/wood flour composites showed higher tensile modulus but lower tensile strength than the PP/wood composites. The water resistance of the PP/wood composites decreased with increasing HIPS content. POLYM. COMPOS., 38:863–869, 2017. © 2015 Society of Plastics Engineers  相似文献   

4.
In an effort to determine to what extent natural fiber/plastic composites were recyclable, this study conducted repetitive processing cycles on wood flour/polypropylene composites through extrusion up to three times followed by injection molding. Mechanical properties of the composites, containing 10–50?wt% wood flour and with/without addition of 3?wt% maleic anhydride polypropylene (MAPP) as coupling agent, were evaluated by conducting tensile test, thermal analysis, and water absorption test. Repetitive processing as well as wood content and coupling agent addition influenced physical properties of the composites. MAPP functioned well in improving fiber-matrix adhesion in terms of mechanical properties. Repetitive processing did not deteriorate the composite’s properties; rather opposite effect was shown. Thermal analysis indicated that the alteration in properties was contributed by the molecular condition of the polypropylene matrix. Water absorption increased with the wood flour content but reduced when MAPP was added and with more processing cycles.  相似文献   

5.
The instrumented Izod and Charpy tests were performed on the sawdust–polypropylene (PP) composites to study the nature of impact resistance in the thermoplastic wood composites. The notched Izod strength was found to increase with filler content in composites containing the Maleic–anhydride–grafted PP (MAPP) additive. The Izod strength even exceeds that of the neat matrix resin at higher filler contents, indicating a methodology for applying the recycled PP and also for reinforcing the thermoplastics with wood powders. While the static tensile results show evidences for the reinforcing role of the wood filler, a fracture mechanics characterization through the Charpy impact tests effects of MAPP under the impact loading rates. The choice of MAPP as the additive was discussed accordingly for application of the sort of materials. © 2001 John Wiley & Sons, Inc. J Appl Polym Sci 81: 1420–1428, 2001  相似文献   

6.
The oscillatory shear rheological properties, mechanical performance, shrinkage, and morphology of polypropylene (PP)‐talc composites chemically coupled by maleic‐anhydride‐grafted polypropylene (MAPP) were studied. The samples were prepared in a co‐rotating L/D = 40, 25 mm twin‐screw extruder. Tensile tests carried out on injection‐molded samples showed a reinforcing effect of talc up to 20 wt% on PP. Upon using MAPP, the mechanical performance of PP‐30% talc showed a maximum of about 10% increase in tensile strength at 1.5 wt% of MAPP. A Newtonian plateau (η0) at the terminal zone was observed for the complex viscosity curve of pure PP and PP‐talc composites plotted against frequency up to 30 wt%. Upon increasing the talc content to 40 and 50 wt%, the complex viscosity at very low shear rates sharply increased and showed yield behavior that might be due to the formation of a network of filler agglomerates in the melt. Analysis of viscosity behavior in the power‐law region revealed that the flow behavior index‐n‐decreased from 0.45 for 10 wt% of talc down to about 0.4 for 40 wt% of talc. Upon increasing the talc content to 50 wt%, n decreased to a value even lower than that of the neat PP resin. The frequency of the crossover point represents molecular mobility and relaxation‐time behavior. The crossover frequency of the composites was nearly constant up to 30 wt% of talc and decreased at higher filler loadings. The optimum amount of coupling agent could be correlated with the minimum point in crossover frequency and crossover modulus. The shrinkage behavior of the composites with and without MAPP resin was studied and correlated with the rheological properties. J. VINYL ADDIT. TECHNOL., 2010. © 2010 Society of Plastics Engineers  相似文献   

7.
Hybrid composites of polypropylene (PP), reinforced with short banana and glass fibers were fabricated using Haake torque rheocord followed by compression molding with and without the presence maleic anhydride grafted polypropylene (MAPP) as a coupling agent. Incorporation of both fibers into PP matrix resulted in increase of tensile strength, flexural strength, and impact strength upto 30 wt% with an optimum strength observed at 2 wt% MAPP treated 15 wt% banana and 15 wt% glass fiber. The rate of water absorption for the hybrid composites was decreased due to the presence of glass fiber and coupling agent. The effect of fiber loading in presence of coupling agent on the dynamic mechanical properties has been analyzed to investigate the interfacial properties. An increase in storage modulus (E′) of the treated‐composite indicates higher stiffness. The loss tangent (tan δ) spectra confirms a strong influence of fiber loading and coupling agent concentration on the α and β relaxation process of PP. The nature of fiber matrix adhesion was examined through scanning electron microscopy (SEM) of the tensile fractured specimen. Thermal measurements were carried out through differential scanning calorimetry (DSC) and the thermogravimetric analysis (TGA), indicated an increase in the crystallization temperature and thermal stability of PP with the incorporation of MAPP‐treated banana and glass fiber. POLYM. COMPOS., 31:1247–1257, 2010. © 2009 Society of Plastics Engineers  相似文献   

8.
Binary composites of high‐crystalline fibrous cellulose with polypropylene (PP) or maleic anhydride‐grafted polypropylene (MAPP) were prepared by melt‐mixing with different contents of cellulose from 0 to 60 wt %. Ternary composites of cellulose with PP and MAPP were also prepared to investigate the effects of MAPP as a compatibilizer between cellulose and PP. Scanning electron microscopy revealed that the addition of MAPP generates strong interactions between a PP matrix and cellulose fibers: All cellulose fibers are encapsulated by layers of the matrix and connected tightly within the matrix. Thus, the tensile strength and Young's modulus of MAPP‐containing composites increase with an increase in MAPP and cellulose content, in contrast to the decrease in tensile strength of a PP‐based binary composite with an increase in cellulose. Cellulose fibers act as a nucleating agent for the crystallization of PP, which is promoted by the addition of MAPP through an increase of the crystallization temperature of PP in the composite. Accordingly, both cellulose and MAPP facilitate the thermooxidative stability of PP composites in the following order: MAPP/cellulose > PP/MAPP/cellulose > PP/cellulose > PP. Relative water absorption increases with an increase in cellulose content, decreasing with the addition of MAPP. MAPP‐containing cellulose composites have high potential for applications as environmentally friendly materials. © 2002 Wiley Periodicals, Inc. J Appl Polym Sci 87: 337–345, 2003  相似文献   

9.
Polyethylene terephthalate (PET) waste was converted into carbon and the feasibility of utilizing it as a reinforcing filler material in a polypropylene (PP) matrix was investigated. The carbon produced by the pyrolysis of waste PET at 900°C in nitrogen atmosphere contains high carbon content (>70 wt%). PP/carbon composites were produced by melt blending process at varying loading concentrations. Scanning electron microscopy images at the fractured surface revealed that the carbon filler has better compatibility with the PP matrix. The mechanical, thermal, and rheological properties and surface morphology of the prepared composites were studied. The thermogravimetric analysis studies showed that the thermal stability of the PP/carbon composites was enhanced from 300 to 370°C with 20 wt% of carbon. At lower angular frequency (0.01 rad/s), the storage modulus (G′) of PP was 0.27 Pa and those of PP with 10 and 20 wt% carbon was 4.06 and 7.25 Pa, respectively. Among the PP/carbon composite prepared, PP with 5 wt% carbon showed the highest tensile strength of 38 MPa, greater than that of neat PP (35 MPa). The tensile modulus was enhanced from 0.9 to 1.2 GPa when the carbon content was increased from 0 to 20 wt%.  相似文献   

10.
《Polymer Composites》2017,38(8):1749-1755
Wood flour (WF)‐filled composites based on a polypropylene (PP)/recycled polyethylene terephthalate (r‐PET) matrix were prepared using two‐step extrusion. Maleic anhydride grafted polypropylene (MAPP) was added to improve the compatibility between polymer matrices and WF. The effects of filler and MAPP compatibilization on the water absorption, mechanical properties, and morphological features of PP/r‐PET/WF composites were investigated. The addition of MAPP significantly improved mechanical properties such as tensile strength, flexural strength, tensile modulus, and flexural modulus compared with uncompatibilized composites, but decreased elongation at break. Scanning electron microscopic images of fracture surface specimens revealed better interfacial interaction between WF and polymer matrix for MAPP‐compatibilized PP/r‐PET/WF composites. MAPP‐compatibilized PP/r‐PET/WF composites also showed reduced water absorption due to improved interfacial bonding, which limited the amount of absorbable water molecules. These results indicated that MAPP acts as an effective compatibilizer in PP/r‐PET/WF composites. POLYM. COMPOS., 38:1749–1755, 2017. © 2015 Society of Plastics Engineers  相似文献   

11.
The preparation and characterization of modified and unmodified polypropylene (PP)–wood powder (WP) composites were done under fixed processing conditions. Different techniques were used to study the effect of both WP size and content, as well as compatibilizer content, on the properties of the composites. The results point to the fact that, WP settles in the amorphous part of the matrix and creates new crystalline phases or zones. Scanning electron microscopy micrographs show a relatively even distribution of WP in the PP matrix, which contributes to improvements observed in the properties of the material. Hg‐porosimetry results indicate that the PP matrix, which has a low pore volume, filled the pores in the WP particles. This reduced the total volume of pores in the PP–WP composites. This observation was also supported by a general decrease in gas permeability of the material. Thermal analysis results indicate that the presence of both WP and maleic anhydride grafted polypropylene (MAPP) leads to an increase in enthalpy (crystallinity) values, but to a decrease in lamellar thickness in the composites. The thermal stability of the composites improves somewhat compared to that of PP. There were distinctive differences between the results for composites containing different WP particle sizes, as well as for composites prepared in the presence and absence of MAPP. It is clear from the results that the presence of MAPP generally improves the tensile properties of the composites. Larger WP particles gave rise to better tensile properties, in the presence and absence of MAPP. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 100: 4173–4180, 2006  相似文献   

12.
Hybrid composites of Polypropylene (PP) reinforced with intimately mixed short banana and glass fibers were fabricated using Haake twin screw extruder followed by compression molding with and without the presence maleic anhydride grafted polypropylene (MAPP) as a coupling agent. Incorporation of both the fibers into PP matrix resulted in an increase in tensile, flexural and impact strength with an increasing level of fiber content upto 30 wt% at banana: glass fiber ratio of 15:15 wt% and 2 wt% of MAPP. The rate of water absorption for the hybrid composites decreased due to the presence of glass fiber and coupling agent. The effect of fiber loading in presence of coupling agent on the dynamic mechanical properties has also been analyzed to investigate the interfacial properties. An increase in the storage modulus (E′) of the treated composite indicates higher stiffness. The tan δ spectra confirms a strong influence of fiber contents and coupling agent on the α and β relaxation processes of PP. The nature of fiber matrix adhesion was examined through scanning electron microscopy (SEM) of the tensile fractured specimen. Thermal measurements were carried out employing differential scanning calorimetry (DSC) and the thermogravimetric analysis (TGA) which indicated a decrease in the crystallization temperature and thermal stability of PP with the incorporation of MAPP treated banana and Glass fiber.  相似文献   

13.
软木纤维增强PP复合材料的研究   总被引:9,自引:0,他引:9  
采用软木纤维作为增强材料提高聚丙烯性能。为了改善软木纤维和聚丙烯母体之间的相容性,用马来酸酐接枝聚丙烯(MAPP)对软木纤维进行接枝处理,用MAPP或用三元乙丙橡胶(EPDM)对软木纤维进行改性处理。结果表明,与未经处理木纤维的复合材料相比,三种处理方法都使复合材料的热性能、加工性能和力学性能有了较大的提高。用MAPP接枝和用MAPP表面处理木纤维的方法比用EPDM表面处理木纤维的方法在提高复合材料热性能、加工流动性和拉伸强度方面更为显著。用EPDM表面处理木纤维在改善复合材料的冲击强度、断裂伸长率上更明显。此外,木纤维在复合材料中的浓度对复合材料其它性能的影响,以及MAPP接枝木纤维和MAPP处理木纤维的不同实验结果也进行了评价。  相似文献   

14.
Nanocomposites polypropylene (PP) with 3 and 7 wt % of clay were prepared by melt mixing. Four types of maleic anhydride grafted PP (MAPP) in broad range of MA groups content (0.3–4 wt %) and molecular weights (MW) were used as polar compatibilizers. The effect of the MAPP kind on both the clay dispersion and miscibility with PP was studied. The mixed intercalated/exfoliated morphologies of nanocomposites in the presence of all studied compatibilizers were revealed by XRD and TEM. The oligomer compatibilizer with 4 wt % of MA groups increases the intercalation ability of polymer into clay galleries but this one has limited miscibility with PP and worsens crystalline structure of polymer matrix. The MAPPs with 0.3–1.3% of MA are characterized by the lower intercalation ability but well cocrystallize with PP. Maximum reinforcing effect is attained using high MW MAPP with 0.6% MA and for nanocomposite with 7 wt % (3.8 vol %) of clay it averages almost 1.7 times relative to neat PP and 1.3 times relative to noncompatibilized composite. Dynamic storage moduli of nanocomposites compatibilized by MAPPs with 0.3–1.3% of MA containing 7 wt % of clay increase up to 1.4–1.5 around 30–75°C and over the whole temperature range remain higher compared with both neat PP and uncompatibilized composite. On the contrary, the oligomer MAPP with 4 wt % of MA groups decreases the thermal–mechanical stability of nanocomposite at high temperature compared with both PP and uncompatibilized composites. The study of nanocomposites flammability showed that creating complex composites containing both layered silicate and relatively small amount of magnesium hydroxide can be a successful approach to reduce the combustibility of PP‐based nanocomposites. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci 2007  相似文献   

15.
Blends of maleated polypropylene (MAPP) with high contents of waste rubber powder, namely ground tire rubber and waste ethylene propylene diene monomer (EPDM) powder, were used as impact modifiers for polypropylene (PP) based composites with different reinforcements (hemp, talc, and milled glass fiber). Adding reinforcements led to increase in modulus (tensile, flexural, and torsion moduli) of PP, while its impact strength decreased noticeably. Impact modification of PP‐based composites was successfully performed via inclusion of MAPP/waste rubber compounds, especially compounds containing waste EPDM powder. Inclusion of such impact modifiers increased impact strength of composites over 80%. The effects of impact modification were more significant for hemp‐ and glass‐filled composites compared to composites containing talc. However, slight decrease in tensile, flexural, and torsion moduli (up to 30%) of the composites was also observed after inclusion of impact modifiers. POLYM. COMPOS., 35:2280–2289, 2014. © 2014 Society of Plastics Engineers  相似文献   

16.
Blends of recycled polypropylene (PP) and starch (S) with the compositions polypropylene 83 wt%–starch 17 wt% (PP83/S17) (blend 1a), polypropylene 68.8 wt%–starch 31.2 wt% (PP 68.8/S 31.2) (blend 2a) and polypropylene 89.5 wt%–starch 10.5 wt% (PP 89.5/S 10.5) (blend 3a) were synthesized. Maleated polypropylene (MAPP) was used as a compatibilizer. The compositions of the compatibilized blends were PP73/S15/MAPP12 (blend 1b), PP55/S25/MAPP20 (blend 2b) and PP85/S10/MAPP5 (blend 3b). The occurrence of a reaction between MAPP and starch was studied using Fourier transform infrared analysis. Thermal and rheological properties such as the complex viscosity, storage and loss modulus of the blends with a compatibilizer were found to be higher than those of the blends without a compatibilizer. The compatibilized and uncompatibilized blends, as well as recycled PP, were characterized using differential scanning calorimetry, thermogravimetric analysis and cone-and-plate rheometry. The storage and loss modulus values of blend 3b were observed to be the best. The best compatibilizing effect was exhibited by blend 3b at a loading of 5 wt% MAPP because this compatibilizer content yielded the highest complex viscosity and visco-elastic behavior. The presence of a functional compatibilizer enhanced the interactions between starch and recycled PP, which was confirmed by a rise in the melt viscosity, storage modulus and thermal stability. These blends were also characterized in terms of their water uptake by performing water absorption tests. Blend 2b containing 20 % MAPP was observed to absorb the maximum amount of water at 25 °C.  相似文献   

17.
In this study, the hybrid composites were prepared by stacking jute/PP nonwoven and flax/MAPP woven fabrics in defined sequences. Polypropylene (PP) and maleic anhydride grafted polypropylene (MAPP) were used as matrix materials. Jute and flax fibers were treated with alkali solution in order to improve the interface properties of the resultant composites. The mechanical properties of these hybrid composites were analyzed by means of tensile, flexural, and drop‐weight impact tests. The effect of fabric stacking sequence on the mechanical properties of the composites was investigated. The stacking of nonwovens at the top and in alternate layers has resulted in maximum flexural strength, flexural stiffness, and impact force. It was also shown that hybrid composites have improved tensile, flexural, and impact properties in comparison to neat PP matrix. POLYM. COMPOS., 36:2167–2173, 2015. © 2014 Society of Plastics Engineers  相似文献   

18.
The purpose of this work was to study how viscose fiber behaves in polypropylene (PP) matrix when maleated polypropylene (MAPP) is used as a coupling agent. The influences of processing conditions on composite properties was of interest. Composites were characterized by FTIR and mechanical testing. The most notable result was the effect of the MAPP concentration on the tensile strength of the composites; the tensile strength increased from 40 to 69 MPa when MAPP was added in amounts up to 6 wt % of the fiber weight. The interaction between MAPP and fiber was confirmed with FTIR. © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 87: 1895–1900, 2003  相似文献   

19.
The main objective of this research was to study the potential of waste polypropylene and waste wood for making wood plastic composites (WPCs). The effects of nanoclay (NC), microcrystalline cellulose (MCC), and coupling agent (MAPP) on the mechanical and thermal properties were also studied. The results showed that mechanical properties of the composites made with MCC were significantly superior to those of unfilled. Addition of MAPP could enhance the mechanical and thermal properties of the blends, due to the improvement of interface bond between the filler and matrix. The significant improvements in tensile properties of the blends composites made with MAPP and NC were further supported by SEM micrographs. The thermogravimetric analysis indicated that the addition of 5 wt% MAPP and 3 wt% NC significantly increased the thermal stability of the blends compared to the pure PP. MCC could not improve the thermal stability. The experimental results demonstrated that the waste materials used are promising alternative raw materials for making low cost WPCs.  相似文献   

20.
The effect of two compatibilizers, i.e. ethylene diamine dilaurate (EDD) and maleic anhydride grafted polypropylene (MAPP) on the mechanical properties, water absorption, morphology, and thermal properties of silica‐filled polypropylene (PP/Sil) composites were studied. The results show that the tensile, impact and flexural strengths (up to 2 php), Young's modulus, and elongation at break (Eb) increased with increasing EDD content. However, increasing MAPP content increases the tensile strength, Young's modulus, impact and flexural strengths, and water absorption resistance. At a similar compatibilizer content, EDD exhibits higher Eb, impact and flexural strengths but lowers tensile strength, Young's modulus, and water absorption resistance compared with MAPP. Scanning electron microscopy study of tensile fractured surfaces exhibits the evidence of better silica‐PP adhesion with MAPP and EDD compared with the similar composites but without compatibilizer. Fourier transform infra red spectra provide an evidence of interaction between EDD or MAPP with PP/Sil composites. Termogravimetry analysis results indicate that the addition of EDD or MAPP slightly increases the thermal stability of PP/Sil composites. Differential scanning calorimetry also indicates that PP/Sil composites with EDD or MAPP have higher heat fusion (ΔHf(com)) and crystallinity (Xcom) than similar composites but without compatibilizer. POLYM. COMPOS., 2008. © 2008 Society of Plastics Engineers  相似文献   

设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号