1.
Vanadium oxide and cerium oxide doped titania–zirconia mixed oxides were explored for oxidative dehydrogenation of ethylbenzene to styrene utilizing carbon dioxide as a soft oxidant. The investigated TiO2–ZrO2 mixed oxide support with high specific surface area (207 m2 g−1) was synthesized by a coprecipitation method. Over the calcined support (550 °C), a monolayer equivalent (15 wt.%) of V2O5, CeO2 or a combination of both were deposited by using wet-impregnation or co-impregnation methods to make the V2O5/TiO2–ZrO2, CeO2/TiO2–ZrO2 and V2O5–CeO2/TiO2–ZrO2 combination catalysts, respectively. These catalysts were characterized using X-ray diffraction (XRD), Raman, scanning electron microscopy (SEM), transmission electron microscopy (TEM), temperature preprogrammed reduction (TPR), CO2 temperature preprogrammed desorption (TPD) and BET surface area methods. All characterization studies revealed that the deposited promoter oxides are in a highly dispersed form over the support, and the combined acid–base and redox properties of the catalysts play a major role in this reaction. The V2O5–CeO2/TiO2–ZrO2 catalyst exhibited a better conversion and product selectivity than other combinations. In particular, the addition of CeO2 to V2O5/TiO2–ZrO2 prevented catalyst deactivation and helped to maintain a high and stable catalytic activity.  相似文献   

2.
In this paper, the CuO/TiO2 catalysts prepared by the deposition–precipitation (DP) method were extensively investigated for CO oxidation reaction. The structural characters of the CuO/TiO2 catalysts were comparatively investigated by TG-DTA, XRD, and XPS measurements. It was shown that the catalytic behavior of CuO/TiO2 catalysts greatly depended on the TiO2-support calcination temperature, the CuO loading amount and the CuO/TiO2 catalysts calcination temperature. CuO supported on the anatase phase of TiO2-support calcined at 400 °C showed better catalytic activity than those supported on TiO2 calcined at 500 and 700 °C. Among all our investigated catalysts with CuO loading from 2% to 12%, the catalyst with 8 wt% CuO loading exhibited the highest catalytic activity. The optimum calcination temperature of the CuO/TiO2 catalysts was 300 °C. The XRD results indicated that the catalytic activity of the CuO/TiO2 catalysts was related to the crystal phase and particle size of TiO2 support and CuO active component.  相似文献   

3.
MnCu/ZrO2T and MnCu/TiO2T (T = calcination temperature) catalysts were prepared by the sol-gel method with a Mn:Cu = 5:1 ratio and calcined at different temperatures, T = 673, 873 and 1073 K. The samples were characterized by X-ray diffraction, measurement of specific surface area, temperature programmed reduction, XPS and FT-IR spectroscopy. For both groups of catalysts, the increase of calcination temperature produced three effects: the segregation of phases, an increase of the crystallinity, and a phase transformation of the support. The catalytic activity was evaluated in total oxidation of ethanol, considered as model molecule of VOC. The MnCu/TiO2 673 and MnCu/ZrO2 873 catalysts showed the best catalytic performance, which was associated with the high dispersion of the MnOx and CuOx active phases. The catalytic activity of MnCu/TiO2 673 catalyst was also favored by its high surface area.  相似文献   

4.
Cu/ZnO/ZrO2 catalysts were prepared by a route of solid-state reaction and tested for the synthesis of methanol from CO2 hydrogenation. The effects of calcination temperature on the physicochemical properties of as-prepared catalysts were investigated by N2 adsorption, XRD, TEM, N2O titration and H2-TPR techniques. The results show that the dispersion of copper species decreases with the increase in calcination temperature. Meanwhile, the phase transformation of zirconia from tetragonal to monoclinic was observed. The highest activity was achieved over the catalyst calcined at 400 °C. This method is a promising alternative for the preparation of highly efficient Cu/ZnO/ZrO2 catalysts.  相似文献   

5.
J.D.A. Bellido 《Fuel》2009,88(9):1673-1034
ZrO2, γ-Al2O3 and ZrO2/γ-Al2O3-supported copper catalysts have been prepared, each with three different copper loads (1, 2 and 5 wt%), by the impregnation method. The catalysts were characterized by nitrogen adsorption (BET), X-ray diffraction (XRD), temperature programmed reduction (TPR) with H2, Raman spectroscopy and electronic paramagnetic resonance (EPR). The reduction of NO by CO was studied in a fixed-bed reactor packed with these catalysts and fed with a mixture of 1% CO and 1% NO in helium. The catalyst with 5 wt% copper supported on the ZrO2/γ-Al2O3 matrix achieved 80% reduction of NO. Approximately the same rate of conversion was obtained on the catalyst with 2 wt% copper on ZrO2. Characterization of these catalysts indicated that the active copper species for the reduction of NO are those in direct contact with the oxygen vacancies found in ZrO2.  相似文献   

6.
A series of catalysts, NiSO4/TiO2–ZrO2 having different TiO2–ZrO2 composition, for acid catalysis was prepared by the impregnation method using an aqueous solution of nickel sulfate. The addition of TiO2 to ZrO2 improved the surface area of the catalyst and enhanced its acidity remarkably because of the formation of new acid sites through the charge imbalance of Ti–O–Zr bonding. The binary oxide, TiO2–ZrO2 calcined above 600 °C resulted in the formation of crystalline orthorhombic phase of ZrTiO4. Therefore, NiSO4/TiO2–ZrO2 calcined at 500 °C exhibited a maximum catalytic activity for acid catalysis, and then the catalytic activity decreased with the calcination temperature. The correlation between catalytic activity and acidity held for both reaction, 2-propanol dehydration and cumene dealkylation. NiSO4 supported on 50TiO2–50ZrO2 (TiO2/ZrO2 ratio = 1) among TiO2–ZrO2 binary oxides exhibited the highest catalytic activity for acid catalysis.  相似文献   

7.
TiO2-Al2O3 mixed oxides with different compositions ranging from 40wt-% to 95wt-% of TiO2 were prepared by sol-gel method and impregnated with different amounts of VO x . Supports and catalysts were characterized by X-ray diffraction (XRD), physisorption, temperature preprogrammed reduction (H2-TPR), and ammonia temperature programmed desorption (NH3-TPD). TiO2 content in the support had obvious effect on the crystal structure, texture characteristic, acid property, and catalytic activity in dehydrogenation of ethylbenzene (EB) with carbon dioxide. The highest catalytic activity was acquired when the TiO2 content was 50 wt-%.  相似文献   

8.
Two series of supported Pd catalysts were synthesized on new mesoporous–macroporous supports (ZrO2, TiO2) labelled M (Zr and Ti). The deposition of palladium was carried out by wet impregnation on the calcined TiO2 and ZrO2 supports at 400 °C (Pd/Zr4, Pd/Ti4) and 600 °C (Pd/Zr6, Pd/Ti6) and followed by a calcination at 400 °C for 4 h. The pre-reduced Pd/MX catalysts were investigated for the chlorobenzene total oxidation and their catalytic properties where compared to those of a reference catalyst Pd/Ti-Ref (TiO2 from Huntsman Tioxide recalcined at 500 °C) and of a palladium supported on the fresh mesoporous–macroporous TiO2 (Pd/Ti). Based on the activity determined by T50, the Pd/Ti and Pd/Ti4 catalysts have been found to be more active than the reference one. Moreover activity decreased owing to the sequence: Pd/TiX  Pd/ZrX and in each series when the temperature of calcination of the support was raised. The overall results clearly showed that the activity was dependant on the nature of the support. The better activity of Pd/TiX compared to Pd/ZrX was likely due to a better reducibility of the TiO2 support (Ti4+ into Ti3+) leading to an enhancement of the oxygen mobility. Production of polychlorinated benzenes PhClx (x = 2–6) and of Cl2 was also observed. Nevertheless at 500 °C the selectivity in HCl was higher than 90% for the best catalysts.  相似文献   

9.
This work investigates the improvement of Ni/Al2O3 catalyst stability by ZrO2 addition for H2 gas production from CH4/CO2 reforming reactions. The initial effect of Ni addition was followed by the effect of increasing operating temperature to 500–700 °C as well as the effect of ZrO2 loading and the promoted catalyst preparation methods by using a feed gas mixture at a CH4:CO2 ratio of 1:1.25. The experimental results showed that a high reaction temperature of 700 °C was favored by an endothermic dry reforming reaction. In this reaction the deactivation of Ni/Al2O3 was mainly due to coke deposition. This deactivation was evidently inhibited by ZrO2, as it enhances dissociation of CO2 forming oxygen intermediates near the contact between ZrO2 and nickel where the deposited coke is gasified afterwards. The texture of the catalyst or BET surface area was affected by the catalyst preparation method. The change of the catalyst texture resulted from the formation of ZrO2–Al2O3 composite and the plugging of Al2O3 pore by ZrO2. The 15% Ni/10% ZrO2/Al2O3 co-impregnated catalyst showed a higher BET surface area and catalytic activity than the sequentially impregnated catalyst whereas coke inhibition capability of the promoted catalysts prepared by either method was comparable. Further study on long-term catalyst stability should be made.  相似文献   

10.
Supported nickel catalysts of composition Ni/Y2O3–ZrO2 were synthesized in one step by the polymerization method and compared with a nickel catalyst prepared by wet impregnation. Stronger interactions were observed in the formed catalysts between NiO species and the oxygen vacancies of the Y2O3–ZrO2 in the catalysts made by polymerization, and these were attributed to less agglomeration of the NiO during the synthesis of the catalysts in one step. The dry reforming of ethanol was catalyzed with a maximum CO2 conversion of 61% on the 5NiYZ catalyst at 800 °C, representing a better response than for the catalyst of the same composition prepared by wet impregnation.  相似文献   

11.
In this present study, the nanocrystalline ZrO2 particles synthesized by the solvothermal method were calcined in reductive (H2), inert (N2) and oxidative (O2 and air) atmospheres prior to impregnation with tungsten (W) in order to produce the W/ZrO2 (WZ) catalysts. Based on the ESR measurement, it revealed that only the ZrO2 samples calcined in H2 and N2 exhibited the F-center (single charged oxygen vacancy) at g = 2.003. None of Zr3+ defect was detected for all calcined ZrO2 samples. After impregnation with tungsten, the WZ catalysts were also characterized. It was present as the polycrystal, which can be seen by the selected area electron distribution (SAED). However, the presence of Zr3+ defect was evident in all WZ catalysts, while the F-center was absent. The highest Zr3+ intensity detected in the WZ catalyst using ZrO2 under H2 calcination atmosphere can be attributed to the transformation of F-center to Zr3+ defect. It revealed that the WZ-H2 catalyst exhibited the highest conversion under transesterification of triacetin and methanol among other WZ catalysts. This can be attributed to the high surface acidity, which was probably induced by large amounts of Zr3+ defect.  相似文献   

12.
《Catalysis communications》2011,12(15):1224-1228
Acetylation of glycerol with acetic acid was investigated over ZrO2, TiO2–ZrO2, WOx/TiO2–ZrO2 and MoOx/TiO2–ZrO2 solid acid catalysts to synthesize monoacetin, diacetin and triacetin having interesting applications as bio-additives for petroleum fuels. The prepared catalysts were characterized by means of XRD, BET surface area, ammonia-TPD and FT-Raman techniques. The effect of various parameters such as reaction temperature, molar ratio of acetic acid to glycerol, catalyst wt.% and time-on-stream were studied to optimize the reaction conditions. Among various catalysts investigated, the MoOx/TiO2–ZrO2 combination exhibited highest conversion (~ 100%) with best product selectivity, and a high time-on-stream stability.  相似文献   

13.
The NOx storage and reduction (NSR) catalysts Pt/K/TiO2–ZrO2 were prepared by an impregnation method. The techniques of XRD, NH3-TPD, CO2-TPD, H2-TPR and in situDRIFTS were employed to investigate their NOx storage behavior and sulfur-resisting performance. It is revealed that the storage capacity and sulfur-resisting ability of these catalysts depend strongly on the calcination temperature of the support. The catalyst with theist support calcined at 500 °C, exhibits the largest specific surface area but the lowest storage capacity. With increasing calcination temperature, the NOx storage capacity of the catalyst improves greatly, but the sulfur-resisting ability of the catalyst decreases. In situ DRIFTS results show that free nitrate species and bulk sulfates are the main storage and sulfation species, respectively, for all the catalysts studied. The CO2-TPD results indicate that the decomposition performance of K2CO3 is largely determined by the surface property of the TiO2–ZrO2 support. The interaction between the surface hydroxyl of the support and K2CO3 promotes the decomposition of K2CO3 to form –OK groups bound to the support, leading to low NOx storage capacity but high sulfur-resisting ability, while the interaction between the highly dispersed K2CO3 species and Lewis acid sites gives rise to high NOx storage capacity but decreased sulfur-resisting ability. The optimal calcination temperature of TiO2–ZrO2 support is 650 °C.  相似文献   

14.
Al2O3 was modified with TiO2 and ZrO2 using organometallic precursors and is used in the preparation of supported platinum catalysts. The catalysts have been characterised by nitrogen adsorption, hydrogen chemisorption and X-ray diffraction and were tested for their activity in the hydrodechlorination of chlorobenzene. The investigations show that support modification controls the catalyst deactivation remarkably and the catalysts were found to be highly active and selective. This revised version was published online in July 2006 with corrections to the Cover Date.  相似文献   

15.
Zirconia-supported and bulk-mixed vanadiumantimonium oxide catalysts were used for the oxidation of o-xylene to phthalic anhydride. X-ray diffraction, Raman spectroscopy and photoelectron spectroscopy were used for characterization. It was found that vanadium promotes the transition of tetragonal to monoclinic zirconia. The simultaneous presence of Sb and V on zirconia at low coverage led to a preferential interaction of individual V and Sb oxides with the zirconia surface rather than the formation of a binary Sb-V oxide, while at higher Sb-V contents the formation of SbVO4 took place. Sb-V/ZrO2 catalysts showed high activity for o-xylene conversion and better selectivity to phthalic anhydride as compared to V/ZrO2 catalysts. However, their selectivity to phthalic anhydride was poor in comparison to a V/TiO2 commercial catalyst. The improved selectivity of the Sb-containing catalysts is attributed to the blocking of non-effective surface sites of ZrO2, the decrease of the total amount of acid sites and the formation of surface V-O-Sb-O-V structures.  相似文献   

16.
Glycosylation reactions are most commonly encountered in nature. Synthetically, glycosylations are carried out with Lewis acid catalysts or mineral acids. However an environmental threat associated with catalysts has encouraged process modification by alternative development of solid catalysts based glycosylation reactions, which are commercially viable as well. In this contribution comparative study of glycosidic bond formation of 1,2,3,4,6-penta-o-acetyl-β-d-glucopyranoside with various alcohols over variety of reaction promoters/catalyst like p-toluene sulphonic acid, HCl, H2SO4 and MgO–ZrO2 were taken up to evaluate the performance of this potential promoter/catalysts systems. The best catalyst for the selective synthesis of alkyl-β-d-glucopyranosides was MgO–ZrO2 which remains active upto three runs. This replacement of homogeneous acid catalysts by heterogeneous base catalyst shows alkyl-β-d-glucopyranoside as major product at comparatively low temperature range. The effects of variety of parameters were studied in a batch reactor. The mechanism of the reaction over basic mixed metal oxide at 363 K is put forth.  相似文献   

17.
《Catalysis communications》2011,12(15):1165-1170
Dry reforming of methane has been studied over Co/ZrO2 catalysts promoted with different metal additives (La, Ce, Mn, Mg, K) aiming to improve the performance of the catalysts and increase their resistance to coking. Scanning electron microscopy studies and different activity levels of the catalysts clearly show that the type of the promoter significantly affected the metal dispersion properties and catalytic performances of Co/ZrO2 catalysts. La-modified catalyst exhibited high stability, but moderate activity. It showed no severe coke deposition. Ce-doped Co/ZrO2 displayed the highest activity among all the catalysts prepared and had a very limited activity loss.  相似文献   

18.
The SAPO-34/ZrO2 composite catalysts using ZrO2 as a binder were prepared and their performance was investigated for the dimethyl ether to olefins (DTO) reaction. The composite catalysts showed higher catalytic lifetimes than the free SAPO-34 catalyst, while maintaining high selectivity toward light olefins. This suggests that the binder-filled space between the SAPO-34 crystals can provide additional diffusion paths for mass transfer. In the SAPO-34/ZrO2 composite catalysts with different ZrO2 contents, the SAPO-34(11 wt%)/ZrO2 composite catalyst showed the highest catalytic lifetime. It can be concluded that ZrO2 is one of the best binders for the preparation of SAPO-34/binder composite catalysts.  相似文献   

19.
Photodegradation of phenol was investigated with two types of oxidant agents in water, oxygen and hydrogen peroxide, at two different reaction pH with a series of nanosized iron-doped anatase TiO2 catalysts with different iron contents. The catalysts have been prepared by a sol–gel/microemulsion method. Firstly, iron-doped titania catalysts were studied with respect to their activity behavior when oxygen was used as oxidant agent in the photocatalytic degradation of aqueous phenol in comparison with un-doped reference catalysts. Secondly, two catalysts (TiO2 and 0.7 wt.% Fe-doped TiO2) were selected to extend the study for the employment of hydrogen peroxide as oxidant at different concentrations and two initial reaction pHs. An enhancement of the photocatalytic activity is observed only for relatively low doping level (ca. 0.7 wt.%) in catalyst calcined at 450 °C preferably using hydrogen peroxide as oxidant agent which is attributable to the partial introduction of Fe3+ cations into the anatase structure. Nevertheless, it has been demonstrated that catalyst surface properties can play an important role during phenol photodegradation process on the basis of the analysis of differences found in the photoactivity as a function of reaction pH.  相似文献   

20.
The CO methanation was studied over zeolite NaY supported Ni, Co3O4, ZrO2 catalysts. The XRD, N2 physisorption and SEM analysis were used in order to characterize the catalysts. Catalytic activities were carried out under a feed composition of 1% CO, 50% H2 and 49% He between the 125 °C to 375 °C. Except for the Ni/Co3O4/NaY catalyst, all catalysts gave high surface area because of the presence of zeolite NaY. Average pore diameter of the catalysts fell into the mesopore diameter range. The highest CO methanation activity was obtained with Ni/ZrO2/NaY catalyst at which the CO methanation was started after 175 °C and 100% CO conversion was obtained at 275 °C using the same catalyst.  相似文献   