1.
A series of chitosans with various molecular weights from 1.2 × 103 to 30.0 × 104 were prepared by oxidative degradation with H2O2 and characterized by IR, 13C‐NMR, and gel permeation chromatography. Their carboxylic contents increased with a decrease in molecular weight (Mw). The moisture‐absorption and moisture‐retention capacities of resulting chitosans were dependent on both the molecular weight and the degree of deacetylation (DD). Microcalorimetry was first used to study the kinetics of action of the chitosans on a strain of Staphylococcus aureus at pH 7. The antibacterial activity of the water‐soluble chitosan against S. aureus, Escherichia coli, and Salmonella typhi was evaluated by the conventional agar plate method at pH 7. The water‐soluble product with Mw of 0.45 × 104 from initial chitosan of DD of 90% showed high moisture‐absorption and moisture‐retention capacities, and <2% concentration can completely inhibit the growth of these bacteria. © 2002 Wiley Periodicals, Inc. J Appl Polym Sci 86: 1724–1730, 2002  相似文献   

2.
To render the surface of ultrafiltration membranes biocidal, cellulose membranes were modified with chitosan, a naturally occurring polycationic biocide. Through the use of chitosans of different molecular weights and membranes with different pore sizes, the alteration of the morphological structure of tethered chitosan layers was achieved. The importance of such structural differences in the antimicrobial activity of the prepared membranes against gram‐positive Staphylococcus aureus and gram‐negative Escherichia coli was studied. The antimicrobial efficiency improved with the use of chitosans with higher molecular weights and membranes with smaller pore sizes. This suggested that the surface location of the grafted chitosan chains was more preferential for a higher antimicrobial activity of the surface. Membranes modified with chitosan showed higher antimicrobial efficiency against gram‐positive S. aureus than against gram‐negative E. coli. © 2008 Wiley Periodicals, Inc. J Appl Polym Sci, 2009  相似文献   

3.
In this study, the chitosan and its derivatives were tested for their preservative activities for field natural rubber (NR) latex. A series of chitosans with different molecular weights were obtained by nitrous acid depolymerization. The chemically modified chitosans, N‐carboxymethyl chitosan (NCMCh), N‐sulfated chitosan (NSCh), and N‐(2‐hydroxy)propyl‐3‐trimethylammonium chitosan chloride (NHTACh), were prepared from high and low‐molecular weight chitosans. Preservative activities for field NR latex of these chitosans were investigated based on the measurement of volatile fatty acids (VFA) number of the treated latex. The preservative activities of chitosan increased with decreasing molecular weights. The low‐ molecular weight NSCh and NHTACh exhibited good preservative activity for the latex. By the use of low‐molecular weight NHTACh in combination with octylphenol poly (ethyleneglycolether) (Nonidet P40), the latex was successfully preserved for more than 1 month in the low‐ammonia condition. The results showed an attractive feature to develop the preservative system, which was possible to reduce the concentrations of ammonia and carcinogenic nitrosamine in the NR latex. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2011  相似文献   

4.
Depolymerization of the biopolymer chitosan by an autoclaving process at 121°C and 15 psi was investigated using various treatments. Acetic acid was found to be the most effective solvent in decreasing chitosan viscosity among the six organic acids tested. The rate of viscosity decrease increased with increasing chitosan concentration. The viscosity of 1% chitosan in 1% acetic acid decreased rapidly to 91% of the initial viscosity following the initial 15 min of autoclaving. This decreased gradually to 93% and 94% in 30 and 60 min, respectively, without being adversely affected by the chitosan solution volume. The degree of deacetylation was comparable before and after autoclaving for 60 min. Chitosan at three molecular weights (Mr = 1597, 1110, and 789 kDa) decreased in molecular weight by 46%–51% in the 15‐min treatment, 55%–60% in the 30‐min treatment, and 60%–62% in the 60‐min treatment. The addition of 0.1%–1.0% (v/v) concentrations of hydrogen peroxide to the chitosan solution autoclaved for 15 min decreased viscosity by 94%–98% and molecular weight by 69%–83%. This process is a simple, timesaving, homogeneous depolymerization procedure, and it is possible to prepare partially hydrolyzed chitosan with specified molecular weights by regulating the time of treatment. © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 87: 1890–1894, 2003  相似文献   

5.
The objective of this study is to explore the effect of using different recovery methods and conditions on the yield, solubility, molecular weight, and creep compliance of the regenerated chitosan. The results show that yields obtained by dialysis were higher than those using recovery medium of alkali solutions, organic solvents, or alkali–alcohol–water mixtures. For those chitosans employing alkali solutions as the recovery medium, the higher the alkali concentration used, the higher the yields obtained, although the total quantity of alkali in the solution were the same. Solubilities of regenerated chitosans were similar and independent at the methods of using alkali solution, organic solvent or alkali–alcohol–water mixture or at different concentrations of alkali solution. The molecular weight of regenerated chitosan decreased from 2.37 × 107 to 1.68 × 107 Da proportionally with the concentration of the alkali solution of the recovery medium from 1N to 8N. Creep compliance of regenerated chitosan gel obtained from 65% degree of deacetylation (DD) chitosan was lower than that of either 72 or 89% DD chitosan gel. Of the same DD chitosan, compliance of regenerated chitosan gels obtained by using a higher concentration of alkali solution was lower than that of a lower concentration ones. Hydrogels regenerated from different DD chitosans and/or different recovery mediums have different structure and tactile properties. Therefore, they can be used as wound dressings suited to different applications. © 2002 Wiley Periodicals, Inc. J Appl Polym Sci 84: 193–202, 2002; DOI 10.1002/app.10296  相似文献   

6.
Water‐soluble chitosan oligomer was prepared for finishing polypropylene nonwoven fabrics to impart antimicrobial activity. The weight average molecular weight was 1814 and its degree of deacetylation was 84%. Polypropylene nonwoven fabrics were treated with chitosan oligomer solution by the pad‐dry method. Antimicrobial activity was measured by the shake flask method. The chitosan oligomer showed high antimicrobial activities against Proteus vulgaris, Staphylococcus aureus, and Escherichia coli at 0.01% and 0.05% level, respectively, showing above 90% of reduction rate. Chitosan oligomer was the most effective against Proteus vulgaris. However, it was not effective against Klebsiella pneumoniae and Pseudomonas aeruginosa below the treatment concentration of 1.0%. Fabrics became stiffer and less air permeable with the increase of treatment concentration. Tensile strength of the treated samples was lower than that of the untreated one. Liquid strike‐through time of the sample treated with 0.5% chitosan oligomer solution (3.0 s) was comparable with that of a hydrophilic finished sample available commercially (2.6 s). © 1999 John Wiley & Sons, Inc. J Appl Polym Sci 74: 2911–2916, 1999  相似文献   

7.
Molecular weight determination of 83% degree of deacetylation (DD) chitosan with non‐Gaussian and broad molecular weight distribution by high‐performance size exclusion chromatography (HPSEC) and by capillary viscometry were proposed. The relationships between weight average retention volumes (RVw) of HPSEC and intrinsic viscosities ([η]) measured by capillary viscometer and the weight average molecular weight (Mw) measured by static light scattering were established for routine molecular weight determination of chitosans either by HPSEC or by the capillary viscometry method, respectively. These results showed: relationships of RVw and Mw for different Mw of 83.0% DD chitosans can be expressed by the equation Log Mw = −0.433 RVw + 11.66. The RVw of other DD chitosans do not correlate well with this equation. It indicated that DD of chitosan affected the relationship of RVw and Mw of chitosans studied. The Mark–Houwink constant a decreased from 0.715 to 0.521, as the solution ionic strength increased from 0.01M to 0.30M, whereas constant k increased from 5.48 × 10−4 to 2.04 × 10−3 over the same range of ionic strength solutions. The established RVw and Mw equation and [η] and Mw equation (Mark–Houwink equation) can be routinely used to determine the molecular weight from RVw or [η] of chitosan by HPSEC or by capillary viscometer, respectively, without the need of expensive instrumentation. © 1999 John Wiley & Sons, Inc. J Appl Polym Sci 71: 1905–1913, 1999  相似文献   

8.
Carboxymethyl chitins and chitosans (CM‐chitins, CM‐chitosans) of different substitution sites were prepared under different reaction conditions, and partially depolymerized carboxymethyl chitins of various molecular weights from 24.8 × 104 to 0.26 × 104 were obtained by degrading with chemical reagents. Degree of substitution (DS) was estimated by potentiometric titration. Substitution site was confirmed by infrared and 13C‐NMR spectra. Molecular weights were determined with gel permeation chromatography and gel permeation chromatography combined with laser light scattering (GPC‐LLS). Moisture‐absorption and retention abilities of these compounds were tested in comparison with those of hyaluronic acid (HA). The results reveal that 6‐carboxymethyl group in the molecular structure of chitin and chitosan is a main active site responsible for moisture retention. Although carboxymethylation at OH‐3 and N position is not essential, they contribute to the ability. Moisture‐retention ability is also related to molecular weight; that is, higher molecular weight helps to improve moisture‐retention ability. 6‐O‐CM‐chitin (chitosan) with a DS above 0.8 and molecular weight higher than 24.8 × 104 has the potential to substitute for HA for use in cosmetics and clinical medicine. © 2002 Wiley Periodicals, Inc. J Appl Polym Sci 83: 1233–1241, 2002  相似文献   

9.
Lactic acid fermentation was used to extract chitin from prawn shell (Nephrops norvegicus) at two different scales of operation. The fermentation products were characterized and compared with chitin extracted from the same source by a chemical method. Chitosans produced from the obtained chitins were evaluated in terms of their intrinsic viscosity, molecular weight and degree of acetylation (DA). The fermentation removed 690 g kg?1 and 770 g kg?1 of inorganic matter, 490 and 440 g kg?1 of protein and 540 and 770 g kg?1 of lipids from the shells at laboratory and pilot plant scales, respectively. However, the functional properties such as the DA of the chitin, the molecular weight and the DA of the chitosans were similar to those obtained for the chemically‐obtained chitin and its chitosan. Despite the incomplete extraction of chitin this biological process could be useful to produce chitin and chitosan in a more environment‐friendly approach. Copyright © 2004 Society of Chemical Industry  相似文献   

10.
A cationic moiety, N‐(3‐chloro‐2‐hydroxypropyl)trimethyl ammonium chloride (CHPTAC), was incorporated onto chitosan in an aqueous alkaline solution. Thus, modified chitosan was prepared. A series of modified chitosans with different molecular weights and charge densities were synthesized through the alteration of the molar ratio of CHPTAC to chitosan in the reaction mixture. The synthesized modified chitosans were thereafter characterized by a variety of physicochemical characterization techniques to confirm that modification did take place. Furthermore, the feasibility of applying modified chitosans as flocculants was assessed, and they were compared with the native chitosan in model colloidal suspensions of kaolin and iron‐ore powder. The results indicated that the unmodified chitosan itself was a good flocculating agent. The flocculation performance of the chitosan could be altered by the incorporation of the CHPTAC moiety. Studies showed that not all the modified chitosans had superior flocculation performance versus the native chitosan. Among the different grades, the modified chitosan with a moderate molecular weight and a moderate charge density showed the best flocculation performance in both model suspensions. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010  相似文献   

11.
A series of chitosans with different molecular weights and degrees of acetylation (DAs) are reacted with nitric oxide (NO) to form [NONO]? groups. The effects of molecular weight and DA on NO release are investigated by Griess assay. Heterogeneous reaction of NH2 groups of chitosan with NO was shown to be influenced greatly by the crystalline form of chitosan. Total NO release exhibited a bell‐shaped distribution at different DAs ranging from 6 to 95%, peaking at about 50%. When DA is held constant, total NO release is directly proportional to the molecular weight. X‐ray diffraction patterns indicate that the total NO release of chitosan‐NO adducts is in general agreement with the intensity of reflections at low Bragg angles (2θ = 8.6°–11.1°), and in turn, a relaxed hydration crystalline form and NO molecules could penetrate this crystal and react with the chitosan molecules. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010  相似文献   

12.
In this article we describe our preliminary work involving the use of depolymerized, low molecular weight chitosan nanoparticles as carriers for proteins and peptides. We hypothesized that the molecular weight of chitosan could favorably modulate the particle and protein release characteristics for the delivery of certain bioactive macromolecules. Our primary objectives were to develop nanoparticle formulations that were stable and reproducible across a range of chitosan molecular weights and then characterize the physicochemical and in vitro release properties as functions of the polymer size. Using depolymerized fragments generated by NaNO2 degradation of different chitosan salts, we prepared nanoparticle formulations based on ionotropic gelation with sodium tripolyphosphate (TPP). Regardless of the formulation, the nanoparticle size decreased with decreasing molecular weight and the ζ‐potential values remained unchanged. Similar comparisons were made with the encapsulation of insulin and tetanus toxoid as model proteins. The results indicated that the quantity of TPP in a given formulation has a greater effect on the protein encapsulation than the chitosan molecular weight. In fast release environments (i.e., buffered media), there was no significant molecular weight effect that could be discerned. These data lead to the conclusion that, under these experimental conditions, the chitosan molecular weight has a measurable effect on the particle properties, although this effect is modest relative to other formulation parameters (e.g., TPP content, type of protein loaded). Because these subtle differences could have dramatic effects physiologically, work is currently underway to elucidate the possible applications of depolymerized chitosans for peptide delivery in vivo. © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 12: 2769–2776, 2003  相似文献   

13.
The antibacterial activities of chitosan and its water‐soluble derivatives on E. coli were studied according to four influencing factors in vitro. The antibacterial study showed that chitosan, O‐hydroxyethyl chitosan (O‐HECS), and O‐carboxymethyl chitosan (O‐CMCS) could inhibit the growth of the microbial. To study the antibacterial mechanism, plasmid DNA pBR322 and pUC18 were selected to be the probes to find out the binding abilities of chitosans. Results showed that raw chitosan had a high binding ability with the plasmids and the influencing degrees were stable. The effects of chitosan derivatives on plasmids might be affected by space effect and static effect. With appropriate concentrations and molecular weights, the derivatives might have strong abilities to combine with DNA. The degree of influence of chitosan and its derivatives on plasmids had nothing to do with time. The experiment focusing on the relationship between chitosans and mRNA showed that O‐CMCS would hinder the synthesis of mRNA, and this may give some proof to its antibacterial mechanism. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 103: 3521–3528, 2007  相似文献   

14.
Formed-in-place (FIP) ultrafiltration (UF) membranes were formed from dilute solutions of chitosans with different molecular weights in 1% acetic acid on a macroporous titanium dioxide substrate. The ultrafiltration properties were characterized by investigating the rejection and permeability of a 1.0 g/L bovine serum albumin (BSA) solution at various pH and ionic strength conditions. The membrane stability to the crossflow shear and to the ionic strength was investigated. There was very little dependence of the membrane-formation capability and the membrane properties on the chitosan molecular weight. In contrast, pH had a marked effect on membrane surface properties, membrane stability, and membrane morphology. © 1998 John Wiley & Sons, Inc. J Appl Polym Sci 67: 513–519, 1998  相似文献   

15.
Chitosan, a cationic polysaccharide, was heterogeneously deacetylated with a 47% sodium hydroxide solution and followed by a homogeneous reacetylation with acetic anhydrides to control the N-acetyl content of the chitosan having a similar molecular weight. The chitosans having different degrees of N-acetylation were complexed with sodium alginate, an anionic polysaccharide, and the formation behavior of polyelectrolyte complexes (PECs) was examined by the viscometry in various pH ranges. The maximum mixing ratio (Rmax) increased with a decrease in the degree of N-acetylation of the chitosan at the same pH, and with a decrease in pH at the same degree of N-acetylation. Similarly, N-acylated chitosans were also prepared. The N-acyl chitosans scarcely affected the formation behavior of PECs with sodium alginates. For the application of the PECs produced, the microencapsulation of a drug was performed and the release property of drug was tested. The microcapsules were prepared in one step by the extrusion of a solution of guaifenesin and sodium alginate into a solution containing calcium chloride and chitosan through interpolymeric ionic interactions. The drug release during the drug-loaded microcapsules storage in saline was found to depend on the pH where the microcapsules were formed and the kind of N-acyl groups introduced to the chitosan. © 1997 John Wiley & Sons, Inc. J Appl Polym Sci 63: 425–432, 1997  相似文献   

16.
Low molecular weight chitosan with weight‐average molecular weight from 161 to 22,000Da were obtained by sonolysis. Optimal conditions for sonolysis were described. The influence of sonolysis condition and the molecular parameters of initial chitosan on the degradation rate and degradation rate constant were investigated in detail. Weight‐average molecular weight (Mw) and molecular weight dispersion (Mw/Mn) of samples were measured by gel permeation chromatography. The structure of degraded chitosan were characterized by Fourier transform infrared, X‐ray diffraction, and electrospray ionization mass spectrometry. For a given sonolysis time, the decrease in molecular weight has been found to be greatest at lowest reaction temperature and lowest chitosan concentration. Molecular weight of samples decreased exponentially with increasing sonication time at early stages. The action mode of ultrasound on the splitting of molecular chain of chitosan has been discussed. The degree of deacetylation of the main hydrolysis products almost unchanged compared with the initial chitosan. The decrease of molecular weight led to transformation of crystal structure but the chemical structures of residues were not modified. Ultrasonic treatment on chitosan is an alternative, safe method to prepare chitosan having different molecular weights, which are more suitable for biomedical and food applications. © 2008 Wiley Periodicals, Inc. J Appl Polym Sci, 2008  相似文献   

17.
The objective of the study was to explore the effect of the degree of deacetylation (DD) of the chitosan used on the degradation rate and rate constant during ultrasonic degradation. Chitin was extracted from red shrimp process waste. Four different DD chitosans were prepared from chitin by alkali deacetylation. Those chitosans were degraded by ultrasonic radiation to different molecular weights. Changes of the molecular weight were determined by light scattering, and data of molecular weight changes were used to calculate the degradation rate and rate constant. The results were as follows: The molecular weight of chitosans decreased with an increasing ultrasonication time. The curves of the molecular weight versus the ultrasonication time were broken at 1‐h treatment. The degradation rate and rate constant of sonolysis decreased with an increasing ultrasonication time. This may be because the chances of being attacked by the cavitation energy increased with an increasing molecular weight species and may be because smaller molecular weight species have shorter relaxation times and, thus, can alleviate the sonication stress easier. However, the degradation rate and rate constant of sonolysis increased with an increasing DD of the chitosan used. This may be because the flexibilitier molecules of higher DD chitosans are more susceptible to the shear force of elongation flow generated by the cavitation field or due to the bond energy difference of acetamido and β‐1,4‐glucoside linkage or hydrogen bonds. Breakage of the β‐1,4‐glucoside linkage will result in lower molecular weight and an increasing reaction rate and rate constant. © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 90: 3526–3531, 2003  相似文献   

18.
Chitosan solutions of the same 83% degree of deacetylation (DD) but different weight average molecular weights (Mws) (78–914 kDa) in 0.01M HCl containing different concentrations of urea (0–6M) were prepared. Intrinsic viscosity ([η]) and weight average molecular weight (Mw) of chitosan were measured with a capillary viscometer and light scattering, respectively. Mark–Houwink exponent a was used as the parameter of conformational index. The Mark–Houwink exponent a increased with increasing concentrations of urea. When solutions contained 0, 2, 3, 4, and 6M urea, the value of a increased from 0.715 to 0.839, 0.894, 1.000, and 1.060, respectively. This indicates the occurrence of urea‐induced conformational transitions of chitosans. The break point shifted from 223 kDa in solutions containing no urea to 280 kDa in 2M urea solutions, to 362 kDa in 4M urea solutions and further to 481 kDa in 6M urea solutions. © 2000 John Wiley & Sons, Inc. J Appl Polym Sci 75: 452–457, 2000  相似文献   

19.
This report describes how the degree of deacetylation and molecular weight of chitosan and the concentrations of sodium chloride and malic acid affect the formation of lyotropic chitosan liquid crystals. Chitosan samples of various degrees of deacetylation were prepared from β‐chitin that was isolated from squid pens. They were degraded by ultrasonic irradiation to various molecular weights. The critical concentrations forming chitosan liquid crystals were determined with a polarized microscope. A chitosan sample with a degree of deacetylation of 67.2–83.6% formed cholesteric lyotropic liquid crystals when it was dissolved in 0.37–2.59M malic acid. The critical concentrations increased with increasing degrees of deacetylation of chitosan. They decreased with increasing molecular weights or increasing concentrations of sodium chloride and malic acid. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci, 2007  相似文献   

20.
An increase in the depolymerization of chitosan was found with an increased concentration of sodium perborate. Acetic anhydride was added to reacetylated chitosan in a molar ratio per gulcosamine unit, and the amide I band of IR spectra changed with the addition of acetic anhydride. Sixteen chitosans with various molecular weights (MWs) and degrees of deacetylation (DODs) were prepared. X‐ray diffraction patterns indicated their amorphous and partially crystalline states. Increases in the chitosan MW and DOD increased the tensile strength (TS). TS of the chitosan films ranged from 22 to 61 MPa. However, the elongation (E) of chitosan films did not show any difference with MW. TS of chitosan films decreased with the reacetylation process. However, E of chitosan films was not dependent on DOD. The water vapor permeabilities (WVPs) of the chitosan films without a plasticizer were between 0.155 and 0.214 ng m/m2 s Pa. As the chitosan MW increased, the chitosan film WVP increased, but the values were not significantly different. Moreover, the WVP values were not different from low DOD to high DOD. © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 89: 3476–3484, 2003  相似文献   