1.
对某难选铜钼矿石的分选工艺进行研究,浮选过程中矿浆粘度增大,导致精矿产率上升,精矿品位低,浮选困难。试验采用一次粗选、三次精选、三次扫选闭路浮选流程,通过优化药剂制度,较好的回收了金属铜、钼,可获得铜钼混合精矿铜品位18.24%,回收率81.65%,钼品位1.28%,回收率49.61%,浮选指标令人满意。  相似文献   

2.
斑岩型低品位铜钼矿石工艺矿物学研究   总被引:4,自引:0,他引:4  
采用显微镜研究、X-射线衍射分析、电子探针分析等手段,查明了某斑岩型低品位铜钼矿石矿物组成,铜、钼的赋存状态及主要矿物的嵌布特性。根据工艺矿物学研究结果,针对该矿石的性质特点,选矿试验采用铜钼硫混合浮选-铜钼浮选-铜钼分离的原则流程,最终得到良好指标:钼精矿钼品位46.28%,回收率70.26%;铜精矿铜品位22.31%,回收率84.19%;硫精矿硫品位30.24%,回收率69.60%。为了提高矿山的资源利用率,在浮选富集金属矿物之后,应在尾矿中回收钾长石、钠长石。  相似文献   

3.
复杂钼铜铁多金属矿的综合利用研究   总被引:3,自引:0,他引:3  
对某钼铜铁多金属矿矿石进行了工艺矿物学研究,该矿石是以钼为主、并生铜铁的多金属矿.根据矿石的性质,采用钼铜混合浮选混合精矿再分离-尾矿磁选选铁的工艺流程.铜钼混合浮选时,采用煤油、柴油混合捕收剂,有利于提高钼回收率,采用选铜特效捕收剂BK802,有利于提高铜的回收率.铜钼混合精矿分离时,采用煤油作为捕收剂,最终选择BK310进行铜钼分离.对铜钼混选尾矿进行了选铁实验,最适宜的磁场强度为0.12~0.16 T之间.研究结果表明:在原矿铜品位0.082%的情况下,可以得到含铜品位15.16%、铜回收率80.54%的铜精矿;采用新型抑制剂BIC310,一次分离三次精选即得到钼精矿钼品位50.87%,回收率85.94%;磁铁矿单体解离较好,一次粗选后再磨,得到铁精矿铁品位69.47%、铁回收率41.89%的铁精矿.  相似文献   

4.
在对黑龙江某低品位难选斑岩型铜钼矿进行矿石性质研究的基础上,采用铜钼混合浮选-铜钼分离的工艺流程,闭路试验可获得含钼41.49%、钼回收率74.83%的钼精矿和含铜21.04%、铜回收率84.14%的铜精矿。较生产现场,铜精矿铜品位提高了1.58%,铜回收率降低了1.28%,钼精矿钼品位降低了4.36%,钼回收率提高了21.94%。该试验研究结果可以作为现场简化铜钼选别流程,实现铜钼高效分离的技术依据。  相似文献   

5.
《甘肃冶金》2021,43(5)
甲玛铜钼混合精矿因药剂、微细粒泥和辉钼矿紧密吸附,导致钼品位及回收率很难提高,针对这一技术难题,对该含泥铜钼精矿进行了详细的试验研究,最终获得流动性摩擦脱药高浓度浮选新工艺在铜钼混合浮选-抑铜浮钼中应用。采用此工艺进行试验,在铜钼混合精矿钼品位0.52%,铜品位23.37%的情况下,可获得钼精矿钼品位45.19%、作业回收率82.05%,铜精矿铜品位23.58%、作业回收率99.95%的生产指标,为该含泥低品位铜钼矿石的选矿提供了技术依据。该技术理念可作为铜、铅、锌、金、银、钼、硫、铁等依次浮选设计资源依据。  相似文献   

6.
某钼矿石中最主要的有价元素为Mo和Cu,其品位分别为0.032%和0.165%,Fe、S的品位分别为3.05%和1.05%,其他金属元素如Pb、Zn等的品位则相对较低。根据矿石的性质,通过条件试验,确定采用铜钼部分优先浮选—铜钼硫混合浮选—铜钼分离流程,小型闭路试验获得的指标为:铜精矿品位21.66%、回收率84.69%,钼精矿品位46.78%、回收率80.89%,硫精矿品位41.27%,回收率63.67%。  相似文献   

7.
某低品位钼铜矿石选矿试验研究   总被引:1,自引:0,他引:1  
某钼铜矿石是一种以钼为主、并伴生铜矿物的低品位钼铜矿石,原矿含钼仅0.045%、含铜0.025%,无其它有价值的金属元素,试验采用先优先混合浮选将钼铜金属矿物同时富集后,再进行钼铜分离的选矿工艺,取得了钼精矿钼品位53.25%~50.4%(含铜0.30%~1.514%,取决于精选作业次数)、混合浮选开路作业回收率70.09%、分离浮选开路作业回收率55.89%~82.42%、开路作业总回收率为39.17%~57.77%;铜精矿含铜品位22.23%(含钼2.36%)、混合浮选作业回收率46.82%、分离浮选回收率90.45%、开路总回收率为42.35%的较好指标。如果条件允许能够进行闭路浮选试验,可能会取得更好的技术经济指标。  相似文献   

8.
针对某铜钼混合精矿中次生铜含量较高且含泥量大,导致在铜钼分离浮选过程中次生铜矿物难以被抑制,产出的钼精矿不能满足质量要求等问题,进行了预先分选—铜钼分离工艺研究。结果表明:在铜钼混合精矿铜品位为24. 40%、钼品位为0. 46%及最佳的试验条件下,采用预先分选、一次粗选、两次扫选、八次精选、中矿循序返回的浮选流程,可获得钼品位51. 56%、铜品位1. 05%、钼作业回收率74. 29%的钼精矿,铜品位24. 55%、钼品位0. 12%、铜作业回收率99. 97%的铜精矿,实现了高次生铜易泥化铜钼混合精矿中铜钼的有效分离。  相似文献   

9.
福建某低品位铜钼多金属矿含Mo 0.051%、Cu 0.16%,矿石中钼、铜主要以辉钼矿、黄铜矿形态赋存,同时嵌布连生关系复杂,不利于铜钼分离。结合工艺矿物学分离结果确定了硫化矿混合浮选—混合精矿再磨—铜钼与硫分离—铜钼分离的选矿工艺流程,在经优化后的药剂制度条件下全流程闭路试验获得了钼精矿、铜精矿、硫精矿三个产品,钼精矿中Mo回收率达到了80.26%,铜精矿中Cu回收率达到了87.03%,实现了对该低品位铜钼多金属矿中金属资源的综合回收。  相似文献   

10.
某高硫铜钼多金属矿石中铜品位0. 68%、钼品位0. 021%,同时伴生有金、银,且硫高达8. 45%。针对矿石性质,进行了混合浮选药剂制度试验研究。结果表明:C39捕收剂对该矿石的选择适应性好,在大幅减少石灰用量的条件下,可提高混合精矿铜品位及钼、金、银的回收率;闭路试验获得的混合精矿中铜品位23. 180%、钼品位0. 637%、金品位5. 250%、银品位341. 080%,铜回收率90. 75%、钼回收率80. 99%、金回收率76. 60%、银回收率80. 17%,选矿指标理想。  相似文献   

11.
陈磊  马亮 《铜业工程》2021,(4):47-51
The copper grade the low-grade copper-molybdenum ore in Shaanxi is 0.32% and the molybdenum grade is 0.048%.The copper and molybdenum minerals mainly exist in the form of sulfide ore. The properties are complex that there are many kinds of minerals in the ore, which are closely distributed and fine dissemination size. According to the properties of the ore, the technological process of bulk flotation and separation of copper and molybdenum was adopted in the experiment. With lime as regulator and reagent L03 as collector, the mixed concentrate of copper and molybdenum was obtained by the bulk flotation which flow-sheet is one roughing, three refining and two scavenging process. Then regrinding the mixed concentrate, use sodium sulfide as inhibitor of copper minerals, sodium silicate as slurry dispersant and inhibitor of silicate gangue minerals , kerosene as collector, can separate copper and molybdenum with the flow-sheet which one roughing, five refining and three scavenging. The copper concentrate with copper grade of 18.82% and copper recovery rate of 85.35% and molybdenum concentrate with molybdenum grade of 47.14% and molybdenum recovery rate of 79.24% were obtained by the final closed-circuit flotation test process, the indicator is nearly ideal.  相似文献   

12.
新疆某铜矿选厂二期扩能工程采用旋流-静态微泡浮选柱进行铜钼混合粗选、铜钼混合精选、铜钼分离粗选、钼精选等作业,与浮选机扫选作业结合形成柱机联合浮选工艺系统,在原矿铜品位0.65%,钼品位0.046%的情况下,经稳定运行获得了铜精矿品位21.8%、铜回收率91.37%、钼精矿品位50.6%、钼回收率55.68%的浮选指标。较一期浮选机工艺相比,柱机联合浮选工艺流程明显简化,铜钼分离效果得到了提高。  相似文献   

13.
斑岩型铜钼矿具有矿石性质复杂、嵌布粒度细、辉钼矿与黄铜矿可浮性相近等特点,导致在浮选过程中铜钼分离困难。利用超声波改变矿浆性质、矿物表面性质及药剂溶液性质。通过对某铜钼矿石采用超声波技术处理强化铜钼浮选分离,纯矿物浮选研究表明,采用超声波处理可以有效实现黄铜矿与辉钼矿的分离。实际矿石分选表明:在磨矿浓度为66.7%、矿浆pH=10.0、石灰用量为450 g/t、水玻璃用量为1 kg/t、YC药剂+丁基黄药用量为160 g/t+50 g/t、2#油30 g/t、磨矿细度 < 0.074 mm占77.2%时,获得混合铜钼精矿钼品位为2.96%,钼回收率为87.44%;铜品位为0.76%,铜回收率为92.77%。对铜钼混合精矿,在矿浆浓度10%下,经超声功率2 000 W处理时间20 min,浮选条件为矿浆pH=10、煤油用量为80 g/t、2#油用量为15 g/t、硫化钠用量为300 g/t,获得最终钼精矿Mo品位为22.19%,作业回收率为95.95%,钼总回收率为83.90%;铜精矿Cu品位为11.88%,作业回收率为98.27%,铜总回收率为91.16%,实现了铜钼矿物良好分离。   相似文献   

14.
针对某锡矿石伴生钼铋铜的综合回收试验研究,根据钼、铋、铜矿的密切共生关系及可浮性特点,制定了钼铋铜混合浮选,混合精矿再磨脱药,最后进行抑铜浮钼铋,钼铋分离的选矿工艺流程,获得钼精矿品位46.07%、回收率75.04%,铋精矿品位16.27%、回收率32.62%,铜精矿品位24.65%、回收率63.03%的良好选矿指标.  相似文献   

15.
铜钼矿的浮选工艺和浮选药剂研究进展   总被引:1,自引:0,他引:1  
就铜钼矿的几种浮选方法进行了综述,介绍了铜钼矿浮选捕收剂及抑制剂的研究进展,指出研究开发新型高效捕收剂及铜钼分离抑制剂是综合回收铜钼矿资源的关键。  相似文献   

16.
新疆富蕴县索尔库都克铜矿具有我国伴生钼的矽卡岩型铜矿,大部分为不含钼的和含钼很低的贫矿的特性,应用浮选柱和浮选机联合设备工艺进行将含钼较低的铜矿进行铜钼分离,经稳定运行取得了铜精矿品位21.76%,铜回收率91.21%,钼精矿品位53.4%,钼回收率63.37%的指标。  相似文献   

17.
某低品位混合铜矿原矿含铜0.32%,其中氧化铜占50.73%,属品位低且氧化率较高的铜矿石。为了充分利用该部分铜矿资源,针对该混合铜矿矿石特点,采用优先浮选硫化铜再活化浮选氧化铜矿,分别通过一粗三精一扫流程工艺,进行了一系列条件试验,并根据条件试验所得的最佳工艺参数进行闭路试验,获得了铜精矿铜品位18.58%、回收率77.55%以及伴生金回收率70.67%的良好指标。该工艺流程和药剂制度简单合理,适用性强,易于实现工业化生产。  相似文献   

18.
大山选矿厂处理矿石主要为铜钼硫化矿,为进一步提高铜、钼回收率指标,充分对资源综合利用。在实验室小型试验的基础上,在大山选矿厂开展工业试验,并对工业试验产品进行了产品分析。通过在混合浮选时添加适量的捕收剂BK404B,在一步精选作业,添加适量的水玻璃,对160m3系统扫选II的泡沫进行选择性再磨。最终工业试验160m3系统铜回收率达88.20%,相比较工业试验之前正常生产一个月铜回收率提高0.42个百分点;钼综合回收率为65.37%,相比较工业试验之前正常生产一个月的累计指标钼综合回收率提高5.36个百分点。  相似文献   

19.
西藏某难选铜铅多金属矿石中多种金属矿物密切共生,硫化物之间嵌连关系较为复杂,且含有大量的次生硫化铜及氧化铜矿物,铜铅分选极为困难。针对该矿石特点,进行了铜铅混合浮选—混合精矿分离、优先浮钼、优先浮铜—再浮铅等多种工艺流程探索试验。结果表明:优先浮铜—再浮铅工艺流程可获得较好指标,闭路试验获得铜品位25.01%、铜回收率81.92%、含铅6.71%的铜精矿,铅品位45.89%、铅回收率70.09%、含铜1.69%的铅精矿,实现了矿石中铜铅的有效分离。  相似文献   

20.
针对某难选氧硫混合型铜矿的特点,利用铜矿物之间可浮性的差异,采用“先硫后氧,先浮选易选氧化铜矿,再浮选难选氧化铜矿”的异步浮选的流程,对含铜3.99%的原矿,在条件优化试验的基础上,开展闭路试验,可以获得浮选硫化铜精矿含铜50.66%,铜回收率25.17%,氧化铜精矿含铜19.68%,回收率54.05%,浮选综合铜精矿回收率达到79.23%。  相似文献   