1.
用球-盘磨损装置研究了电刷镀Cu/Ni纳米多层膜的摩擦磨损性能,采用SEM观察了其表面和截面形貌,并比较了该复合膜层与纯镍镀层的摩擦系数随时间的变化趋势、磨损量以及磨痕形貌。结果表明,该纳米多层膜具有较好的抗微动磨损性能,且晶粒细小,组织致密,界面清晰,各子层厚度均匀;该镀层与纯镍镀层的摩擦系数在达到稳定值后无明显变化;该多层膜的微动磨损方式为粘着疲劳磨损。  相似文献   

2.
用单槽脉冲电沉积法在含CuSO4、NiSO4和Na3C6H5O7的镀液中制备了不同调制波长的Cu/Ni纳米多层膜,对其进行了截面形貌观察及显微硬度测量.结果表明,制备的多层膜平整,层间界清晰.其显微硬度在调制波长为100 nm时出现峰值.当调制波长大于100 nm时,多层膜显微硬度的变化符合Hall-Petch关系;当调制波长小于100 nm时,显微硬度开始下降.X射线衍射表明,膜层中存在压应力,Ni层形成了强(100)织构.  相似文献   

3.
本文针对碳钢在海洋环境中腐蚀严重的问题,采用水热法结合化学气相沉积技术及注入润滑油的三步法在碳钢表面制备了Cu/Ni复合仿生超滑表面。研究了仿生超滑表面对碳钢基体的腐蚀防护性能的影响。通过扫描电镜(SEM)、X射线光电子能谱(EDS)分析了碳钢表面水热反应2 h后形成的Cu/Ni涂层的形貌及组成成分;通过接触角测试分析了Cu/Ni疏水表面的润湿性;运用动电位极化曲线和交流阻抗谱(EIS)研究了仿生超滑表面在3.5 wt.%NaCl溶液中的耐蚀性能。结果表明,Cu/Ni膜层呈现微纳米级粗糙结构,Cu/Ni膜层疏水涂层与水滴的接触角为127.8±1°,Cu/Ni仿生超滑表面腐蚀电流密度为2.96×10-7A·cm-2,相比于碳钢基体降低了2个数量级,对碳钢基体具有一定腐蚀防护作用。  相似文献   

4.
以(110)高择优的Cu片为基底,在硫酸盐镀液中采用单槽双脉冲控电位电沉积法制备了Co/Cu纳米多层膜。采用X射线衍射(XRD)和扫描电镜(SEM)分别对多层膜的微观结构和形貌进行了表征。结果表明,Co/Cu多层膜具有良好周期性,多层膜的微结构和表面形貌与表层的金属层紧密相关,也与Co和Cu镀层厚度及其相对厚度、周期数相关。硼酸的加入有利于改善Co/Cu多层膜的层状结构。  相似文献   

5.
蒙乃尔(Monel)合金是一种机械性能和加工性能好、耐腐蚀性强的Ni—Cu合金。Ni—Cu晶态合金镀层有良好的耐腐蚀性、耐磨性和较高的硬度,并具有良好的导电性和可焊性,其综合性能较Ni—P合金优越得多。采用电刷镀技术,利用X光衍射仪等测试手段,对Ni—Cu合金刷镀溶液的配方组成、施镀工艺、镀层组织结构及成份进行了分析研究,从而确定了Ni—Cu镀液的组成及刷镀工艺。  相似文献   

6.
运用扫描电镜、动电位极化和交流阻抗等手段研究了Ni—Cu—P镀层的耐蚀性,对Ni—Cu—P镀层的表面形貌进行了观察,测量了Ni—Cu—P镀层在3.5NaCl溶液中的开路电位、自腐蚀电流密度和电荷转移电阻等。结果表明:Ni—Cu—P镀层均匀、致密、缺陷较少,减少了与3.5%NaCl溶液的直接接触,Ni—Cu—P镀层更容易产生钝化和维持钝化。  相似文献   

7.
一、前言酸性光亮镀铜常被用于Cu—Ni—Cr体系的中间层。但镀酸性光亮铜后的零件表面,有一层有机吸附膜,容易造成铜与镍层之间结合力差的恶果,因此人们普遍采用碱液电解去膜工艺,以保证铜与镍层之间的结合力。但硫酸去膜活化工艺,在生产实践中证明,也是可行的。硫酸化学除膜工艺,与原来碱液电解去膜相比,可以省掉原工艺的电源、加热等设备,溶液成分简单,成本低,溶液稳定,使用寿命长,且能省掉两个清洗槽,一个弱酸活化槽,减少了占地面积,节省了设备。  相似文献   

8.
用射频磁控溅射方法制备多层膜,研究了双层膜NiO/NiFe的矫顽力Hc和交换耦合场Hex与反铁磁层NiO、铁磁层NiFe厚度的关系。结果表明:NiO厚度为70nm时,Hex最大;Hc随NiO厚度增大而增大。当NiFe厚度增加时,Hex近似线性减小;而矫顽力则随NiFe厚度增大开始有缓慢增加,然后才减小。对于NiO(70nm)/NiFe(t1nm)/Cu(2.2nm)/NiFe(t2nm)自旋阀多层膜材料,研究了NiFe膜厚度对磁阻效应的影响。结果表明:被钉扎层NiFe的厚度为3nm时,自由层NiFe的厚度为5nm时,MR值分别最大,约为1.6%。  相似文献   

9.
张卫国  姜莹  姚素薇 《化工学报》2008,59(2):503-507
采用单槽控电位双脉冲技术在n-Si(111)晶面上制备了[Ni80Fe20/Cu]n多层膜,用SEM观测了多层膜的断面形貌,利用X射线衍射(XRD)表征了多层膜的超晶格结构。采用四探针法研究了多层膜的巨磁电阻(GMR)性能,结果表明,多层膜的GMR值随着Cu层厚度的变化发生周期性振荡,随着NiFe层厚度的增加先增大后减小;当样品结构为[NiFe(1.6 nm)/Cu(2.6 nm)]80时,GMR值可达6.4%;多层膜的最低饱和磁场仅为750Oe。磁滞回线测试结果表明,反铁磁耦合多层膜具有较小的矩形比,更适宜作为磁头材料。  相似文献   

10.
以改性后的堇青石为惰性载体,采用浸渍法制备了一系列Cu系催化剂,活性考察表明,Cu—Mn—Ni—Ce—O/Al2O3/CC催化剂低温活性比较高,反应温度在150℃时转化率达50.46%,300℃达到100%。BET、XPS和TPR测试表明,助剂Mn、Ni和Ce的添加,增大了Cu系催化剂比表面积和平均孔径,使催化剂更易被还原,催化剂表面的元素以Cu^2+、Mn^4+、Mn^3+、Ni^2+和Ce^4+价态的氧化态物种存在。  相似文献   

11.
It is well established that a wide range of drugs of abuse acutely boost the signaling of the sympathetic nervous system and the hypothalamic–pituitary–adrenal (HPA) axis, where norepinephrine and epinephrine are major output molecules. This stimulatory effect is accompanied by such symptoms as elevated heart rate and blood pressure, more rapid breathing, increased body temperature and sweating, and pupillary dilation, as well as the intoxicating or euphoric subjective properties of the drug. While many drugs of abuse are thought to achieve their intoxicating effects by modulating the monoaminergic neurotransmitter systems (i.e., serotonin, norepinephrine, dopamine) by binding to these receptors or otherwise affecting their synaptic signaling, this paper puts forth the hypothesis that many of these drugs are actually acutely converted to catecholamines (dopamine, norepinephrine, epinephrine) in vivo, in addition to transformation to their known metabolites. In this manner, a range of stimulants, opioids, and psychedelics (as well as alcohol) may partially achieve their intoxicating properties, as well as side effects, due to this putative transformation to catecholamines. If this hypothesis is correct, it would alter our understanding of the basic biosynthetic pathways for generating these important signaling molecules, while also modifying our view of the neural substrates underlying substance abuse and dependence, including psychological stress-induced relapse. Importantly, there is a direct way to test the overarching hypothesis: administer (either centrally or peripherally) stable isotope versions of these drugs to model organisms such as rodents (or even to humans) and then use liquid chromatography-mass spectrometry to determine if the labeled drug is converted to labeled catecholamines in brain, blood plasma, or urine samples.  相似文献   

12.
2001—2002年国外塑料工业进展   总被引:7,自引:0,他引:7  
收集了2001年7月到2002年6月有关国外塑料工业的相关期刊资料,介绍了2001年到2002年国外塑料工业的发展情况,提供了世界各地域塑料原材料的产量及构成比,日本,美国,加拿大,德国,法国,比利时,墨西哥,芬兰,西班牙等国家的树脂产量,消费量及增长率,以及日本,西欧,北美等地区的不同品种塑料原料消费量和增长率统计,按通用热塑性树脂(聚乙烯,聚丙烯,聚苯乙烯,聚氯乙烯,ABS树脂),工程塑料(尼龙,聚碳酸酯,聚甲醛,热塑性聚酯,聚苯醚),通用热固性树脂(酚醛,聚氨酯,不饱和树脂,环氧树脂),特种工程塑料(聚苯硫醚,液晶聚合物,聚醚醚酮)不同品种的顺序,对树脂的产量,消费量及合成工艺,产品应用开发,树脂品种的延伸及应用的进一步扩展等有关技术作了详细的介绍。  相似文献   

13.
2002~2003年国外塑料工业进展   总被引:12,自引:0,他引:12  
收集了2002年7月-2003年6月国外塑料工业的相关期刊资料,介绍了2002年-2003年国外塑料工业的发展情况,提供了世界各大地区塑料的产量、增长率及所占份额,美国、德国、日本、韩国、法国、比利时、中国台湾、加拿大、巴西、西班牙等国家和地区的树脂产量及消费量,各国、各地区塑料原材料的产量、进出口量、国内消费量及人均消费量,以及日本的塑料原材料的生产情况。按通用热塑性树脂(聚乙烯、聚丙烯、聚苯乙烯、聚氯乙烯、ABS树脂)、工程塑料(聚酰胺、聚碳酸酯、聚甲醛、热塑性聚酯、聚苯醚)、通用热固性树脂(酚醛、聚氨酯、不饱和树脂、环氧树脂)、特种工程塑料(聚苯硫醚、液晶聚合物、聚醚醚酮)的品种顺序.对树脂的产量、消费量、供需状况及合成工艺、产品开发、树脂品种的延伸及应用的进一步扩展等有关技术作了详细的介绍。  相似文献   

14.
15.
16.
针对石油钻井钻屑污染物治理的需要,开发了具有新颖结构的多层双锥液固逆流浸洗塔,整体上具有液固两相多级逆流传质浓度分布特征,级内呈现液固流态化良好的混合传递特性。釆用脉冲示踪法进行了颗粒停留时间分布实验研宄,结果显示多釜串联模型符合其结构与流动混合特征,以理论级数N作为模型参数可以很好地表达颗粒物性及操作参数对过程的影响。在研究范围内,内径100mm的24层双锥塔理论级数在6.11~11.0,随液固比增大而增大、随颗粒粒径增大而减小的趋势。该塔在理论级数6.93的操作条件下连续逆流浸洗,钻屑平均停留时间4.23min残留COD浓度77mg·L-1,与6级间歇逆流平衡浸洗钻屑残留COD浓度56 mg.L-1的实验结果相近,为多釜串联模型用于多层双锥塔浸洗传质模型研究与过程放大提供了实验依据。  相似文献   

17.
2009~2010年世界塑料工业进展   总被引:1,自引:0,他引:1  
收集了2009年7月~2010年6月世界塑料工业的相关资料,介绍了2009~2010年世界塑料工业的发展情况,提供了世界塑料产量、消费量及全球各类树脂的需求量及产能情况.按通用热塑性树脂(聚乙烯、聚丙烯、聚苯乙烯、聚氯乙烯、ABS树脂),工程塑料(尼龙、聚碳酸酯、聚甲醛、热塑性聚酯、聚苯醚),特种工程塑料(聚苯硫醚、液晶聚合物、聚醚醚酮),通用热固性树脂(酚醛、聚氨酯、不饱和聚酯树脂、环氧树脂)不同品种的顺序,对树脂的产量、消费量、供需状况及合成工艺、产品应用开发、树脂品种的延伸及应用的进一步扩展等技术作了详细介绍.  相似文献   

18.
2004~2005年国外塑料工业进展   总被引:1,自引:0,他引:1  
收集了2004年7月-2005年6月国外塑料工业的相关资料,介绍了2004年~2005年国外塑料工业的发展情况。提供了世界几大区域塑料的产量、增长率及所占份额;美国、德国、日本、韩国、法国、比利时、印度、西班牙、中国台湾、加拿大、巴西、英国等国家和地区的不同树脂的产量及消费量;各国、各地区塑料原料的产量、进出口量、国内消费量和人均消费量;日本塑料原料的生产情况。按通用热塑性树脂(聚乙烯、聚丙烯、聚苯乙烯、聚氯乙烯、ABS树脂)、工程塑料(聚酰胺、聚碳酸酯、聚甲醛、热塑性聚酯、聚苯醚)、通用热固性树脂(酚醛、聚氨酯、不饱和树脂、环氧树脂)、特种工程塑料(聚苯硫醚、液晶聚合物、聚醚醚酮、聚砜)的品种顺序,对树脂的产量、消费量、供需状况及合成工艺、产品开发、树脂品种的延伸及应用的扩展作了详细的介绍。  相似文献   

19.
20.
建立了测定地球化学样品中包括As、Cr、Ge、V等18种微量、痕量元素的ICP-MS方法。地化试样用HF-HNO3混酸分解后,以1 1 HNO3溶解干渣。由于制样不使用盐酸,避免了Cl对As、Cr、Ge、V的质谱干扰。用国家一级地球化学标准物质GBW 07309制备溶液优化仪器工作参数,并用于校准。方法测定限(6s)为:0.007~6.4μg/g,精密度(RSD%,n=12)为:29%~9.4%,经过国家一级地球化学标准物质的分析验证,结果与标准值吻合。方法已应用于国土资源调查的试样分析。  相似文献   