全文获取类型
收费全文 | 111篇 |
免费 | 7篇 |
专业分类
综合类 | 28篇 |
化学工业 | 24篇 |
金属工艺 | 11篇 |
建筑科学 | 20篇 |
矿业工程 | 3篇 |
能源动力 | 2篇 |
轻工业 | 1篇 |
石油天然气 | 4篇 |
一般工业技术 | 12篇 |
冶金工业 | 13篇 |
出版年
2023年 | 4篇 |
2022年 | 3篇 |
2021年 | 3篇 |
2020年 | 5篇 |
2019年 | 2篇 |
2018年 | 4篇 |
2017年 | 1篇 |
2016年 | 1篇 |
2015年 | 2篇 |
2014年 | 7篇 |
2013年 | 3篇 |
2012年 | 3篇 |
2011年 | 7篇 |
2010年 | 4篇 |
2009年 | 3篇 |
2008年 | 3篇 |
2007年 | 5篇 |
2006年 | 4篇 |
2005年 | 3篇 |
2004年 | 4篇 |
2003年 | 2篇 |
2002年 | 1篇 |
2001年 | 2篇 |
2000年 | 12篇 |
1999年 | 3篇 |
1998年 | 1篇 |
1997年 | 1篇 |
1996年 | 2篇 |
1995年 | 3篇 |
1994年 | 6篇 |
1993年 | 2篇 |
1992年 | 1篇 |
1991年 | 3篇 |
1990年 | 1篇 |
1989年 | 1篇 |
1988年 | 2篇 |
1987年 | 2篇 |
1986年 | 1篇 |
1980年 | 1篇 |
排序方式: 共有118条查询结果,搜索用时 0 毫秒
1.
The electrical properties of La0.6Sr0.4Co1-yFeyO3 (LSCF, y=0-1.0) cathode materials were measured by DC four probes, X-ray photo-electron spectrum (XPS) was also introduced to determine the chemical state of Co, F.e ions in LSCF. It is found that the electrical conductivity of each sample has a maximum value with increasing temperature. XPS analysis shows that Co ion has three different chemical states, corresponding to two with Fe ion. The analyses indicates that the small-polaron hopping mechanism dominates the electron conduction at low temperature, while at high temperature, the three factors such as the thermally activated disproportionation of Co^3+ ions into Co^2+ and Co^4+ pairs, the ionic compensation of oxygen vacancies formed at high temperatures, and Fe^4+ ions charge compensation preferential to Co^4+, all contribute to electrical conduction. 相似文献
2.
Porous β-tricalcium phosphate bioceramic (PTCP) has important roles in surgical implants because of good biocompatibility. But the low compressive strength of the ceramic limits its application. The preparation of PTCP was improved with the adjustment of the constituents and the sintering-process. A new type of PTCP material with high compressive strength was made. The compositions, microstructure and properties of PTCP were analyzed by TG-DSC, XRD, TEM, SEM and so on. The result indicates that stearic acid burns sufficiently and gives out carbon dioxide and water vapor when slowly heated between 200 ℃ and 400 ℃ so that the porous structure like coral in β-TCP bioceramic is formed. Through crystallization at 470 ℃ and 570 ℃, more CaO-P2O5 glass-cement is converted into crystallite-glass, which is beneficial for improving the compressive strength of β-TCP bioceramic.PTCP can form a support action in bone imperfect section with good solubility. 相似文献
3.
Aluminium nitride-silicon nitride-silicon carbide (AIN-Si3N4-SiC) composite ceramics were prepared to increase the bending strength and improve the phase structure of Si3N4-based ceramics. The ceramics were made by reactive sintering in N2 atmosphere at 1 360 ℃, using Al as sintering additive. The phase composing of ceramics was identified with an X-ray diffractometer and the microstructure of the materials was studied by scanning electron microscopy. The results indicate that the phase structure is affected remarkably and the interface modality is changed. The interface between Si3N4 and SiC becomes blurry and that between SiC and AlN matches more better at the same time. But the liquid-phase appears during the reactive sintering along with the addition of AI by which the melting point of Si is decreased. The appearance of liquid Si decreases the bending strength of the ceramics. Lower temperature nitrification technic was introduced to avoid the appearance of liquid-phase Si. The optimum addition of Al was investigated by XRD and SEM analysis in order to obtain the maximal bending strength of materials. 相似文献
4.
以0.21的水灰比成型活性粉末混凝土(RPC)基体,研究低水灰比RPC基体水化相在高温蒸压养护条件下的长期水化规律。采用酸不溶物含量表征基体的水化程度,采用显微维氏硬度表征RPC基体在养护过程中的结构性能,并通过X射线粉末衍射与扫描电子显微镜/能量色散谱分析RPC基体的物相与形貌变化。结果表明:高温蒸压养护过程中,RPC基体水化程度在0~96 h的养护期内快速提升,硬度随养护时间增加提升明显;长期养护时(168~312 h),基体的水化速率缓慢,基体内水泥熟料的水化趋于停滞。长期高温蒸压养护过程中,低水灰比RPC基体中晶态水化产物极少,由于缺乏晶态转化的空间,基体中的絮状水化硅酸钙凝胶无明显晶化现象,在长期高温水热条件下具有良好的稳定性,在核废料存储材料领域具有应用前景。 相似文献
5.
氯氧镁水泥浆体水化相及其对强度指标影响初探 总被引:3,自引:0,他引:3
本文力图从合成氯氧镁水泥的纯相入手,研究浆体的基本水化相及其相变规律。研究表明,用正确的配比,采用人工合成的方法,可以得到氯氧镁水泥的基本水化相,即5·1·8和3·1·8,并指出了这两种水化相的变化规律。采用不同浓度的MgCl_2溶液配制的氯氧镁水泥浆体,其水化相主要是5·1·8和Mg(OH)_2,采用半定量的计算方法,可以得到这两种水化相之比与浆体强度的对应关系,因而正确选择水化相的比例,可以获得最佳强度的水泥浆体。 相似文献
6.
7.
分析了影响塑料拉伸试验结果的因素,除塑料的组成、分子结构和内部缺陷等因素直接影响拉伸性能外,试验仪器、试样制备、试样装夹、试验环境、拉伸速率、数据处理、操作人员等因素亦影响试验结果。这些外部因素对试验结果的影响,经过认真操作和严格控制是可以降低或避免的,从而可提高试验结果的准确性。 相似文献
8.
9.
La1-xSrxCo1-yFeyO3系(LSCF)钙钛矿结构氧化物是一类性能优异的离子-电子混合导体,同时具有良好的化学稳定性和催化活性,有望作为中低温下工作的固体氧化物燃料电池阴极材料的候选材料.本文考察了La0.6Sr0.4Co1-yFeyO3(y=0.2~0.8)系材料的导电机制.XPS光电子能谱分析表明,除了存在小极化子导电机制外,同时还可能存在以下几种机理:1)热激发引起Co3 离子的电荷歧化;2)高温下氧空位生成导致的离子补偿;3)Fe4 较Co4 优先进行电荷补偿. 相似文献
10.
La0.6Sr0.4Co1-yFeyO3系阴极材料制备及表征 总被引:5,自引:1,他引:4
La1-xSrxCo1-yFeyO3系(LSCF)钙钛矿结构氧化物是一类性能优异的离子-电子混合导体,同时具有良好的化学稳定性和催化活性,有望作为中低温条件下工作的固体氧化物燃料电池阴极材料的候选材料.本文采用固相反应法制备了多孔La0.6Sr0.4Co1-yFeyO3(y=0.2~0.8)氧化物陶瓷,通过XRD,TG/DTA等测试技术研究了LSCF的结构与制备过程,采用直流四探针法测试了样品的电导率,同时考察了这类组成样品的热膨胀系数.结果表明,这类组成的电导率都有着相同的变化趋势,即先随温度升高而增大,至极大值后又开始降低.分析表明,除了存在小极化子导电机制外,同时还可能存在以下几种机理:1)热激发引起Co3 离子的电荷歧化;2)高温下氧空位生成导致的离子补偿;3)Fe4 较Co4 优先进行电子补偿. 相似文献