排序方式: 共有71条查询结果,搜索用时 15 毫秒
1.
Determination of the Structure of Polyacrylamide/Aluminum Citrate Colloidal Dispersion Gel System 总被引:7,自引:0,他引:7
1 INTRODUCTIONIn recent years,colloidal dispersion gel(CDG)have been attracting more and more in thefield of enhanced oil recovery on account of the cost-effectiveness and high efficiency ofblocking formation.Compared with bulk gel(BG),CDG exhibits lower polymer concentra-tion,undefined shape and selective blocking formation characteristics.The characteris-tics of CDG and BG are related to structure.In the bulk gel a continuous network of polymermolecules is formed predominant through intermolecular cross-linkages.The colloidal 相似文献
2.
胜利孤岛注聚原油破乳剂的筛选与性能评价 总被引:1,自引:0,他引:1
以研究孤岛注聚原油乳状液破乳为目的,通过瓶试法和界面性质的测定,筛选了多种类型的原油破乳剂,考察了破乳剂质量浓度、聚合物和原油组分对破乳效果的影响,探讨了原油乳状液的破乳机理。结果表明,破乳剂BF-069质量浓度在100mg/L,50℃条件下,脱水率达到70%以上,现场温度稍微升高,脱水率达到85%左右,破乳剂BF-069已在胜利油田应用,现场使用效果良好;聚合物质量浓度在50mg/L时,原油乳状液最难破乳;原油中不同组分对破乳效果的影响不同,油水界面性质的测定表明,胶质和沥青质是影响原油破乳的主要因素。 相似文献
3.
采用电导法和相体积法相结合,并借助相图、黏度、光学显微镜,研究了Span80-Tween60/白油/丙烯酰胺/丙烯酸钠/H2O体系形成反相微乳液的过程,以及表面活性剂Span80与Tween60质量比、温度、乙酸钠对体系形成反相微乳液区的影响。结果表明,体系中表面活性剂质量分数小于20%时,电导法与相体积法确定的反相微乳液区边界基本一致;表面活性剂质量分数大于20%时,两方法确定的反相微乳液区边界相差甚远。说明仅由电导率突变不能准确确定反相微乳液区的边界,必须与相体积法相结合来共同确定相区的边界。当质量比m(Span80):m(Tween60)=13:7、温度为25~30℃、乙酸钠质量分数为2%时,体系能形成比较大的反相微乳液区,适合进行微乳液聚合。 相似文献
4.
采用HAAKE流变仪,研究了NaCl质量浓度对低浓度部分水解聚丙烯酰胺(HPAM)与柠檬酸铝(AlCit)交联体系(HPAM/AlCit)流变性、时间效应以及粘度的影响。结果表明,当NaCl质量浓度在5~10g/1时,聚合物质量浓度为0.1g/1的交联体系在一定剪切速率下(500-1500s^-1)表现出胀流性和明显的负触变性;低于或高于该NaCl质量浓度范围,体系只表现出假塑性或牛顿性,并且没有明显的负触变性。交联体系的粘度随NaCl质量浓度的增加先降低后增加,NaCl质量浓度由0.5g/1增加至20g/1,体系粘度逐渐降低;其质量浓度由50g/1增加至100g/1,体系粘度随之增加。笔者对上述实验现象的微观机理进行了初步分析。 相似文献
5.
交联聚合物溶液与聚合物溶液的特性差异 总被引:8,自引:0,他引:8
采用光学显微摄影、动态光散射和核孔膜过滤等方法,研究了低浓度部分水解聚丙烯酰胺(HPAM)与柠檬酸铝(AlCit)形成的交联聚合物溶液(LPS)中交联聚合物线团(LPC)的形态、尺寸、变形性等特性。结果表明,LPC与聚合物线团(PC)相比,在形态、尺寸、变形性能等方面存在明显差异。干燥后的LPS样品中,LPC为球形,PC的形状不清晰。低于某一临界质量浓度(0.200~0.300g/1)时,LPC尺寸略小于PC;高于此浓度后,LPC的尺寸始终大于PC。HPAM/AlCit交联体系的临界质量浓度(0.280g/1)略高于聚合物溶液的临界交叠质量浓度(0.250g/1)。由于分子内的交联作用,与PC相比,LPC的剪切变形能力和水化变形能力有限,LPC较强的抗剪切变形特性使其具有特殊的封堵多孔介质的能力。 相似文献
6.
界面剪切黏度对原油乳状液稳定性的影响 总被引:6,自引:2,他引:4
对孤东一号联合站及孤东四号联合站(简称孤东1#及孤东4#)两种原油及其分离组分(饱和分、芳香分、胶质、沥青质)配成模拟油,测定了模拟油与碱水〔w(Na2CO3)=1 2%〕体系的界面剪切黏度。原油浓度越大,界面剪切黏度越大;沥青质模拟油/碱水界面剪切黏度最大,在油/碱水间形成了一定强度的界面膜,膜的强度大于饱和分、芳香分、胶质的界面膜强度;孤东4#沥青质模拟油/碱水的界面剪切黏度大于孤东1#沥青质的界面剪切黏度。在剪切速率为0 3rad·s-1时,原油及胶质的油/碱水界面剪切黏度不随时间变化。 相似文献
7.
核微孔滤膜评价交联聚合物溶液封堵性质的研究 总被引:18,自引:2,他引:16
交联聚合物溶液(LPS)是由低浓度部分水解聚丙烯酰胺(HPAM)和交联剂柠檬酸铝(AlCit)形成的.提出了一种新的快速有效地评价交联聚合物溶液的方法,即用核微孔滤膜模拟油藏的微孔介质,以交联聚合物溶液通过核孔波膜的能力——封堵因子评价LPS的形成过程和封堵性能.封堵因子越小,封堵程度越大.实验结果表明,HPAM溶液的封堵因子较大,对孔径为1.2μm核孔膜的封堵程度小,HPAM与交联剂刘AlCit反应形成的LPS对核孔膜的封堵程度随反应时间的增加而增加.因此,该评价方法可以用来评价聚合物与交联剂是否发生交联反应形成LPS. 相似文献
8.
The vacuum residual from Iranian Light crude oil are separated into a series of 16 narrow fractions according to the molecular weight by the supercritical fluid extraction and fractional (SFEF) technology. The chemical element and the UV spectrum of each fraction are analyzed. The effects of several factors on the interfacial tension are investigated, which are the fraction concentration in oil phase, the ratio of oil component, the salts dissolved in the water phase and the pH value. The interfacial tension decreases rapidly as the concentration of the residual fraction in the oil increases, showing a higher interfacial activity of the fraction. The interfacial tension changes, as the amount of absorption or the state of the fractions in the interface changes resulting from different ratios of oil, different kinds or concentrations of salts in water, and different pH values. It is concluded that the intrfacial tension changes regularly, corresponding to the regular molecular parameters of the vacuum residual fractions. 相似文献
9.
研究了[Bpy]Br-2AlCl3离子液体催化联苄与十二烯-1的烷基化反应。通过离子液体结构组成分析与实验结果对照,表明在离子液体中各种阴离子配体之间相互转化,使之酸性可调,从而具有不同程度的催化活性。使用离子液体催化剂可以降低芳烃/十二烯-1摩尔比(n(Aromatics)/n(Dodecene-1))、缩短反应时间,且产物易分离。离子液体可循环使用3次以上。较佳的反应条件为:反应温度25~30℃、n(Aromatics):n(Dodecene-1)=1:2、反应时间1h。 相似文献
10.
盐浓度对交联聚合物线团形态的影响 总被引:16,自引:1,他引:15
用核孔膜过滤法 (过滤体积对过滤时间作图 )、动态光散射法 (DLS)和扫描电镜法 (SEM )研究了交联反应前后盐 (NaCl)浓度变化对低浓度HPAM与AlCit形成的交联聚合物溶液 (LPS)中交联聚合物线团 (LPC)形态的影响。所用HPAM相对分子质量 1.1× 10 7~ 1.4× 10 7,LPS中HPAM与Al的质量比 2 0∶1,HPAM浓度 0 .1或 0 .2 g/L ,交联反应温度 40℃ ,时间 7天。实验结果表明 :①LPC的平均水力半径Rh(DLS测定值 )随交联反应时盐浓度的增大先减小后增大 ,盐浓度由 0 .5 g/L增加到 2 g/L时Rh 由 45 0nm迅速减小到 2 5 0nm ,盐浓度增加到 2 0 g/L时Rh达到最小值 16 0nm ,此后随盐浓度的继续增加Rh 有所增大 ;盐浓度 0 .5和 2 .0 g/L时Rh 的SEM测定值分别为45 0和 2 5 0nm ,与DLS结果一致。②交联反应完成后改变LPS的盐浓度 ,也可改变LPC的Rh 值 ,但改变幅度较小 ;盐浓度 0 .5 g/L时形成的LPS ,当盐浓度增加至 2 g/L时 ,Rh 值由 45 0nm减小至 35 9nm ,大于盐浓度 2 g/L时形成的LPS的Rh 值 (2 46nm) ;盐浓度 2 g/L时形成的LPS ,当盐浓度减少至 0 .5 g/L时 ,Rh 值由 2 46nm增大至32 6nm ,小于盐浓度 0 .5g/L时形成的LPS的Rh 值 (4 5 0nm)。用盐浓度改变引起LPC水化层厚度改变 ,线团收缩或舒张解释盐浓度改变时Rh 测定值的 相似文献