Al-Ti alloy containing rare earth elements can produce fine, uniform dispersion intermetallic phasethrough rapid solidification (RS) technology. RS Al-Ti-RE alloy can be designed for applications at elevated-temperature since the intermetallic compound has good thermal stability. A transmission electron microscopy investigation shows the intermetallic phase has a diamond cubic structure (a=1.47736nm), with space group Fd3m. The chemical stoichiometry is Al20 Ti2La. The particle is formed from the melting directly, prior to other phases, and the nucleus is formed from icosahedrons composed with twenty tetrahedrons. Twin crystal structure plays an important role in the nucleation stage. 相似文献
2.
采用金相(OM)、透射电镜(TEM)、扫描电镜(SEM)等先进技术研究了快速凝固Al-4Ti-2V-3La合金,确定了基体中弥散分布的细小强化相为单一的Al20(Ti,V)2La相,结构为金刚石立方结构,晶格常数a=1.47nm。该性能接近当前较成熟的热强铝合金,说明快凝Al-Ti-La基合金作为热强铝合金具有潜在的实力。 相似文献
3.
叙述了高速加工技术在模具制造中应用的意义,以及实现高速加工所必需的一些核心技术。通过与常规的电火花加工方式的比较,论述了高速加工的优越性能及高速切削加工对机床的主轴、刀具和CAM软件的要求,指出在型腔模制造过程中,选择加工方式主要取决于型腔的几何形状、材料的硬度和所要求的工艺参数,最后以加工实例说明了高速切削是现代模具加工的发展方向之一。 相似文献
4.
快速凝固Al-Ti-La合金中金属间化合物相Al2 0 Ti2 La的形成是 :在快速凝固过程中形成孪晶 ,以孪晶为晶核从熔体中优先其他化合物相形成并生长 ,该化合物相细小、圆整、弥散、热稳定性好 ,极大的改善了快速凝固Al-Ti合金的热强性能 ,这种金属间化合物相的形成机制是“孪晶形核”理论 相似文献
5.
6.
采用金相,透射电镜,扫描电镜等先进技术研究了快速凝固Al-4Ti-2V-3La合金,确定了基体中弥散分布的细小强化相为单一的Al20(Ti,V)2La相、结构为金旬石立方结构,晶格常数a=1.47mm。 相似文献
7.
8.
9.
10.
以快速凝固A1—4Ti—2V—3La合金作为研究对象,研究合金的显微结构、热稳定性和力学性能。提出为改善Al-Ti—RE基热强合金的显微组织和性能的合金设计原则,应进一步多元化,其中Ni、Cr元素比较理想,它们与Ti的物理性质相近,在α—Al中有较高的极限固溶度和较低的平衡固溶度,在高温有较低的扩散速率,具有较高的表面张力,并能改善熔体的微观不均匀性。 相似文献