排序方式: 共有32条查询结果,搜索用时 0 毫秒
1.
The GaN based blue light emitting diodes (LEDs) with a thin AlInN layer inserted in front of the electron blocking layer (EBL) are experimentally studied. It is found that inserting a thin EBL can improve the light output power and reduce the efficiency droop compared with the conventional AlGaN counterparts. Based on numerical simulation and analysis, the improvement on the electrical and optical characteristics is mainly attributed to the reduction of the electron leakage current, which increases the concentration of carriers in the quantum well (QW) when the thin AlInN layer is used. 相似文献
2.
4Cr13钢激光相变强化机理研究 总被引:1,自引:0,他引:1
4Cr13钢淬火态试样激光淬火后晶粒尺寸保持常规淬火水平 ,是快速加热组织遗传造成的结果。用激光能量密度概念 ,分析了加热工艺参数对 4Cr13钢非平衡组织淬火后显微硬度分布的影响。结果表明 ,原始状态不同的试样 ,有效硬化层深度 (d)与激光能量密度 ρE 存在下列关系 :原始淬火态dX=0 2 32 7·ρ0 4 82 1E mm ;淬火 +低温回火态dY=0 2 2 78·ρ0 4 659E mm ;淬火 +高温回火态dZ=0 1710·ρ0 3 72 6Emm。 4Cr13钢淬火态试样激光淬火后获得了超过常规淬火水平 2 5 %的超高硬度 ,其中马氏体含碳量增加对超高硬度的贡献约占 6 2 3%,马氏体尺寸细化、高密度位错强化等因素的强化作用约占 37 7%。 相似文献
3.
A major challenge in GaN based solar cell design is the lack of holes compared with electrons in the multiple quantum wells (MQWs). We find that GaN based MQW photovoltaic devices with five different Mg-doping concentrations of 0 cm-3, 5×1017 cm-3, 2×1018 cm-3, 4×1018 cm-3 and 7×1018 cm-3 in GaN barriers can lead to different hole concentrations in quantum wells (QWs). However, when the Mg-doping concentration is over 1×1018 cm-3, the crystal quality degrades, which results in the reduction of the external quantum efficiency (EQE), short circuit current density and open circuit voltage. As a result, the sample with a slight Mg-doping concentration of 5×1017 cm-3 exhibits the highest conversion efficiency. 相似文献
4.
5.
6.
7.
8.
软件体系架构(SA)是软件工程专业主修课程。本文通过五子棋软件开发案例,介绍我们给软件工程专业学生教授SA课程方面的经验。通过需求分析加深对软件系统的理解,在此基础上确定软件质量属性的优先级和所采用的、用来实现这些质量属性的战术。设计合适的五子棋软件架构以满足质量属性要求,并对架构进行评估。 相似文献
9.
10.
Ti-18高温高强钛合金研制 总被引:5,自引:1,他引:4
介绍了高温高强钛合金Ti 18(Ti 6Al 4Mo 4Zr 2Sn 1W 0 .2Si)的试制过程 ,对该合金的性能与组织关系进行了讨论。结果表明 ,Ti- 18合金在常温和高温下均具有优异力学性能 :Φ35 0mm饼材 4 0 0℃ / 10 0h持久强度在80 0MPa以上 ,4 0 0℃ / 10 0h/ 380MPa下的残余应变为 0 .0 4 8% ,4 5 0℃时的断裂强度大于 10 0 0MPa ,延伸率δ5在12 %左右。同时该合金具有良好的热稳定性。研究显示 ,Ti 18合金组织类型的差异对高温性能影响不大 ,该合金半成品可采用等轴组织的变形工艺。双重退火可充分发挥Ti 18合金的热强性潜力 ,是合理的热处理制度。 相似文献