Effect of microelements on microstructures and properties of Al-1. 2Mg-1. 3Si-0. 6Cu-0. 3Mn alloy
作者姓名:TIAN  Ni  ZHAO  Xin  LIU  Chun-ming
作者单位:[1]The Key Laboratory for Anisotropy and Texture of Materials (Ministry of Education), Northeastern University, Shenyang 110004, China [2]Automation Institute of Shenyang Aluminum & Magnesium Engineering & Research Institute, Shenyang 110001, China
摘    要:In order to save energy and protect environmentin automobile industry, one of the important methodsis to reduce the automotive weight1 ~4]. Since the a-luminum alloys showsuch as high specific strength,good formability, good corrosion resistance, and re-cycling potential, they are said to be the ideal candi-date to replace heavier materials in the automotiveindustry5 ~7].Recently, the heat -treatable 6000series aluminum alloys have been considered as theperfect light-weight material for au…

关 键 词:铝合金  微量元素  微观结构  可成型性
文章编号:1671-6620(2006)04-0283-05
收稿时间:2006-10-01
修稿时间:2006年10月1日

Effect of microelements on microstructures and properties of Al-1. 2Mg-1. 3Si-0. 6Cu-0. 3Mn alloy
TIAN Ni ZHAO Xin LIU Chun-ming.Effect of microelements on microstructures and properties of Al-1. 2Mg-1. 3Si-0. 6Cu-0. 3Mn alloy[J].Journal of Materials and Metallurgy,2006,5(4):283-287.
Authors:TIAN Ni  ZHAO Xin  LIU Chun-ming
Abstract:The effects of impurity element of Fe and microelements of Zn, Cr and Ti on the constituents, dispcrsoids, grain size, mechanical properties and formability of Al-1. 3Mg-l. 2Si-0. 6Cu-0. 3Mn alloy were investigated in the present work by analyzing microstructures, phase composition, mechanical tests. The results indicated that with the increase of Fe content, the insoluble constituents increased, and the mechanical pmperties and r15 of alloy sheets debased, which can be recovered by the addition of microelements Zn, Cr and Ti. Al-1. 3Mg-1. 2Si-0. 6Cu-0. 3Mn alloy sheets in the T4 temper are difficult to strengthen with paint - bake treatment in automobile factory.
Keywords:6000 series aluminum alloy  constituents  dispersoids  microelement  formability  paint-bake