Abstract: | Alloying of amorphous Fe-Me-Si-B metallic compositions with nickel and molybdenum results in a decrease in the values of saturation magnetization in fields with a magnetic intensity of 0.72 MA/m. The same alloying additions decrease the temperature of formation of new magnetic Fe3B-type phases, which are stable up to 873 ± 5 K. |