首页 | 本学科首页   官方微博 | 高级检索  
     


Effect of Mn Addition on Microstructural Modification and Cracking Behavior of Ferritic Light-Weight Steels
Authors:Seok Su Sohn  Byeong-Joo Lee  Sunghak Lee  Jai-Hyun Kwak
Affiliation:1. Center for Advanced Aerospace Materials, Pohang University of Science and Technology, Pohang, 790-784, Korea
2. Department of Materials Science and Engineering, Pohang University of Science and Technology, Pohang, 790-784, Korea
3. Sheet Products & Process Research Group, Technical Research Laboratories, POSCO, Kwangyang, 545-090, Korea
Abstract:In the present study, effects of Mn addition on cracking phenomenon occurring during cold rolling of ferritic light-weight steels were clarified in relation to microstructural modification involving κ-carbide, austenite, and martensite. Four steels were fabricated by varying Mn contents of 3 to 12 wt pct, and edge areas of steel sheets containing 6 to 9 wt pct Mn were cracked during the cold rolling. The steels were basically composed of ferrite and austenite in a band shape, but a considerable amount of κ-carbide or martensite existed in the steels containing 3 to 6 wt pct Mn. Microstructural observation of the deformed region of fractured tensile specimens revealed that cracks which were initiated at ferrite/martensite interfacial κ-carbides readily propagated along ferrite/martensite interfaces or into martensite areas in the steel containing 6 wt pct Mn, thereby leading to the center or edge cracking during the cold rolling. In the steel containing 9 wt pct Mn, edge cracks were found in the final stage of cold rolling because of the formation of martensite by the strain-induced austenite to martensite transformation, whereas they were hardly formed in the steel containing 12 wt pct Mn. To prevent or minimize the cracking, it was recommended that the formation of martensite during the cooling from the hot rolling temperature or during the cold rolling should be suppressed, which could be achieved by the enhancement of thermal or mechanical stability of austenite with decreasing austenite grain size or increasing contents of austenite stabilizers.
Keywords:
本文献已被 SpringerLink 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号