摘    要:利用温度和变形实时测量系统,对5A12铝合金板拘束焊变形和外拘束力进行了试验研究,分析了拘束力大小和拘束释放对试板面外变形的影响.结果表明,施加不同的拘束力,试板焊后残余面外变形大小不同,适当的拘束可以有效地控制焊接变形;焊接结束拘束卸载后,焊接件变形出现不同程度的反弹;弹性同复是造成拘束焊残余变形的主要因素;拘束力大...

关 键 词:铝合金  变形  拘束力  弹性回复
收稿时间:2010/1/12 0:00:00

Investigation of out-of-plane welding distortion in aluminum alloy welding with external restraint
XIAO Xiaoming,PENG Yun,ZHANG Jianxun,PEI Yi and TIAN Zhiling.Investigation of out-of-plane welding distortion in aluminum alloy welding with external restraint[J].Transactions of The China Welding Institution,2011,32(5):33-36.
Authors:XIAO Xiaoming  PENG Yun  ZHANG Jianxun  PEI Yi and TIAN Zhiling
Affiliation:State Key Laboratory of Advanced Steel Processes and Products, Central Iron & Steel Research Institute, Beijing 100081, China,State Key Laboratory of Advanced Steel Processes and Products, Central Iron & Steel Research Institute, Beijing 100081, China,State Key Laboratory for Mechanical Behavior of Materials, Xi''an Jiaotong University, Xi''an 710049, China,State Key Laboratory for Mechanical Behavior of Materials, Xi''an Jiaotong University, Xi''an 710049, China and State Key Laboratory of Advanced Steel Processes and Products, Central Iron & Steel Research Institute, Beijing 100081, China
Abstract:The characteristics of constraint force and dynamic welding distortion of aluminum alloy 5A12 with constraint TIG welding were investigated by dynamic temperature and distortion measuring system.The effects of constraint force and its release on out-of-plane welding distortion were analyzed.Research results show that out-of-plane welding distortion is different with the different constraint force,and welding distortion can be controlled by the proper constraint force.the welding distortion will rebound to some extent after the constraint force being released,which is the main factor to result in the residual distortion of constraint welding;the residual distortion of 6 mm thick aluminum alloy 5A12 plate can be well restrained at the constraint force of 0.2 kN,and the loading position is 45 mm form the centerline of weld.
Keywords:aluminum alloy  deformation  constraint force  elastic recovery