热轧薄板M形板廓缺陷研究
引用本文:王文广,杨孝鹤,艾矫健,张敏.热轧薄板M形板廓缺陷研究[J].轧钢,2011,28(5):11-13.
作者姓名:王文广  杨孝鹤  艾矫健  张敏
作者单位:首钢技术研究院
摘    要:针对首钢京唐公司热轧板带生产中出现的M形板廓缺陷,从板形控制参数预设定和工作辊磨损辊型两方面分析了其产生原因,提出了简单、可行的改进措施,为同类机组技术改进提供了依据。

关 键 词:热轧薄板  板形控制  预设定  磨损辊型  

Study on M-shape Contour Defect of Hot Rolled Sheet Steel
WANG Wen-guang,YANG Xiao-he,AI Jiao-jian,ZHANG Min.Study on M-shape Contour Defect of Hot Rolled Sheet Steel[J].Steel Rolling,2011,28(5):11-13.
Authors:WANG Wen-guang  YANG Xiao-he  AI Jiao-jian  ZHANG Min
Affiliation:WANG Wen-guang1,YANG Xiao-he2,AI Jiao-jian2,ZHANG Min2 (1.Shougang Research Institute of Technology,Beijing 100041,China,2.Shougang Jingtang Iron & Steel United Co.,Ltd.,Caofeidian 063200,China)
Abstract:In view of M-shape contour defect of hot rolled sheet steel in Shougang Jingtang Co.,Ltd.,the main reasons of the defect appearing were analyzed from PCFC preset values and wear roll shape of the work rolls.The simple and available measures were put forward as accordance for other similar units.
Keywords:hot rolled sheet steel  profile control  preset  wear roll shape  