Autogenous shrinkage of high-strength concrete containing silica fume under drying at early ages
Authors:Yang Yang  Ryoichi Sato
Affiliation:a College of Construction Engineering and Architecture, Zhejiang University of Technology, No. 6 District, Zhaohui, Hangzhou 310032, China
b Department of Civil and Environmental Engineering, Hiroshima University, 1-4-1, Kagamiyama, Higashi-Hiroshima 739-8527, Japan
Abstract:The present study investigated experimentally autogenous shrinkage of high-strength concrete containing silica fume under drying at early ages. The influence of drying on hydration of cementitious materials in the high-strength concrete with water-binder ratios of 0.25, 0.35 and 0.45 was evaluated based on bound water content (BWC), which was exposed to drying at the ages of 0.5, 1.0 and 3.0 days, respectively. By establishing the relationship between the BWC and autogenous shrinkage strain under sealed conditions, autogenous shrinkage strain under drying conditions and drying shrinkage strain were separated from total shrinkage strain, and, then, the contribution of autogenous shrinkage in total shrinkage was discussed. The results showed that the percentage of autogenous shrinkage was macroscopically 50-20% based on the present method, while that was 70-30% based on the conventional superposition principle (SP). The latter resulted in overestimating autogenous shrinkage strain under drying conditions.
Keywords:High-strength concrete  Silica fume  Autogenous shrinkage  Drying shrinkage  Early age