摘    要:
通过对高速线材生产线在生产带肋钢筋盘条时减定径区堆钢原因的分析,对成品孔型和进、出口导卫进行丁改进,从而使因堆钢而造成的平均事故时间由原来的40min/班减少至5min/班。

关 键 词:带肋钢筋 堆钢 改进措施
文章编号:1003-9996(2005)06-0065-02
收稿时间:2004-11-05
修稿时间:2005-05-16

Resolution of the ribbed bar stacking in reducing sizing mill zone of high-speed wire rod rolling line
SI Yong-hong,SUN Ru-lin,ZHAO Zi-yi,YAN De-jian,WU Bo. Resolution of the ribbed bar stacking in reducing sizing mill zone of high-speed wire rod rolling line[J]. Steel Rolling, 2005, 22(6): 65-66
Authors:SI Yong-hong  SUN Ru-lin  ZHAO Zi-yi  YAN De-jian  WU Bo
Abstract:
The causes of ribbed bar stacking in reducing sizing mill zone of high-speed wire rod rolling line were ann lyzed. The accident time caused by stacking of piece reduced from 40rain to 5min per shift after the finishing pass and its inlet and outlet guidc were reformed.
Keywords:ribbed bar   stacking of piece   improvement measures