炼油厂湿硫化氢的腐蚀与设备防护 |
| |
引用本文: | 王菁辉,赵文轸.炼油厂湿硫化氢的腐蚀与设备防护[J].石油化工腐蚀与防护,2008,25(2):27-30. |
| |
作者姓名: | 王菁辉 赵文轸 |
| |
作者单位: | 1. 西安交通大学材料科学与工程学院,陕西,西安,710049;中国石化集团洛阳石油化工工程公司,河南,洛阳,471003 2. 西安交通大学材料科学与工程学院,陕西,西安,710049 |
| |
摘 要: | 文章就HCl-H2S-H2O,HCN-H2S-H2O,H2S_H2O和CO2-H2S-H2O等湿硫化氢腐蚀体系的形成、腐蚀发生的部位、腐蚀机理、腐蚀影响因素以及从材料或设备角度应该采取的防护措施等进行了介绍。
|
关 键 词: | 湿硫化氢 腐蚀 腐蚀机理 防护措施 |
Wet Hydrogen Sulfides Corrosion in Oil Refinery and Equipment Protection |
| |
Affiliation: | Wang Jinghui, Zhao Wenzhen(1. Material Science and Engineering School of Xi'an fiaotong University ( Xi'an, Shaanxi 710049) ; 2. Luoyang Petrochemical Engineering Corporation/SINOPEC ( Luoyang, Henan 471003)) |
| |
Abstract: | Here introduced are the formation of wet hydrogen sulfides such as HCl-H2S-H2O,HCN-H2S-H2O,H2S_H2O和CO2-H2S-H2O, the corrosion locations, corrosion mechanism, impact factors as well protection measures for equipment and materials. |
| |
Keywords: | wet hydrogen sulfide corrosion corrosion mechanism protection measures |
本文献已被 维普 万方数据 等数据库收录! |
|