摘    要:介绍了影响W6Mo5 Cr4V2高速钢淬硬层深度的因素,包括含碳量,合金元素铬、钨、钼,淬火介质以及工件尺寸.简述了提高这种钢淬硬层深度的方法.

关 键 词:高速钢  淬硬层  硬度

Factors Influencing Hardened Case Thickness of W6Mo5Cr4V2 HSS
LU Hong-mei,CHENG Shun-min,ZHANG An,ZHAO Wei.Factors Influencing Hardened Case Thickness of W6Mo5Cr4V2 HSS[J].Heat Treatment,2011,26(4):52-55.
Authors:LU Hong-mei  CHENG Shun-min  ZHANG An  ZHAO Wei
Affiliation:LU Hong-mei,CHENG Shun-min,ZHANG An,ZHAO Wei Shanghai Tool Works Co.,Ltd.,Shanghai 200093,China
Abstract:The factors influencing hardened case thickness of W6Mo5Cr4V2 HSS were introduced,including carbon content,alloying elements such as chromium,tungsten and molybdenum,quenching medium and part size.Besides,the measures to increase the hardened case thickness of W6Mo5Cr4V2 HSS were briefly described.
Keywords:HSS  hardened case  hardness  