首页 | 本学科首页   官方微博 | 高级检索  
     

GRAIN REFINEMENT IN BULK UNDERCOOLED Ni-BASED ALLOY
引用本文:Li,Delin Yang,Gencang Zhou,Yaohe Northwestern Polytechnical University,Xi'an 710072,China. GRAIN REFINEMENT IN BULK UNDERCOOLED Ni-BASED ALLOY[J]. 中国有色金属学会会刊, 1993, 0(4)
作者姓名:Li  Delin Yang  Gencang Zhou  Yaohe Northwestern Polytechnical University  Xi'an 710072  China
作者单位:Li,Delin Yang,Gencang Zhou,Yaohe Northwestern Polytechnical University,Xi'an 710072,China
基金项目:Financilly suported by the National Natural Science Foundation of China
摘    要:
Fluxing of 5 g bulk melt Ni77Si13B10 permits high undercoolings to be attained prior to nu-cleation onset.Investigations of grain refinement in the bulk undercooled alloy as a function ofundercooling,recalescence behavior and cooling rate have been reported.A significant inhomo-geneity of reduction in grain size of a bulk sample is observed,which is caused by the different so-lidification conditions:(1)recalescence process,and(2)the followed plateau in which the heatrelease and extraction rates are equal.It is concluded that the homogeneous refined microstructurecan be achieved if the initial undercooling prior to nucleation,or cooling rate after recalescence isfurther increased.


GRAIN REFINEMENT IN BULK UNDERCOOLED Ni-BASED ALLOY
Li,Delin Yang,Gencang Zhou,Yaohe Northwestern Polytechnical University,Xi'an ,China. GRAIN REFINEMENT IN BULK UNDERCOOLED Ni-BASED ALLOY[J]. Transactions of Nonferrous Metals Society of China, 1993, 0(4)
Authors:Li  Delin Yang  Gencang Zhou  Yaohe Northwestern Polytechnical University  Xi'an   China
Affiliation:Li,Delin Yang,Gencang Zhou,Yaohe Northwestern Polytechnical University,Xi'an 710072,China
Abstract:
Fluxing of 5 g bulk melt Ni77Si13B10 permits high undercoolings to be attained prior to nu- cleation onset.Investigations of grain refinement in the bulk undercooled alloy as a function of undercooling,recalescence behavior and cooling rate have been reported.A significant inhomo- geneity of reduction in grain size of a bulk sample is observed,which is caused by the different so- lidification conditions:(1)recalescence process,and(2)the followed plateau in which the heat release and extraction rates are equal.It is concluded that the homogeneous refined microstructure can be achieved if the initial undercooling prior to nucleation,or cooling rate after recalescence is further increased.
Keywords:Ni-based alloy  high undercooling  recalescence  grain refinement
本文献已被 CNKI 等数据库收录!