Affiliation:1. The Fifth Research Institute, Equipment Academy of the Rocket Force, Beijing 100094, China;2. Science and Technology on Advanced Ceramic Fibers and Composites Laboratory, National University of Defense Technology, Changsha 410073, Hunan Province, China;3. School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 10083, China;1. Tianjin Polytechnic University, Tianjin 300387, PR China;2. Key Laboratory of Advanced Textile Composite Materials of Ministry of Education, Tianjin 300387, PR China;1. Science and Technology on Advanced Ceramic Fibers and Composites Laboratory, National University of Defense Technology, Changsha 410073, China;2. IMDEA Materials Institute, c/Eric Kandel 2, Getafe 28906, Madrid, Spain;3. School of Materials Science and Engineering, Xiangtan University, Xiangtan 411105, China;1. Science and Technology on Advanced Ceramic Fibers and Composites Laboratory, National University of Defense Technology, Changsha, Hunan 410073, PR China;2. Science and Technology on Scramjet Laboratory, College of Aerospace Science and Engineering, National University of Defense Technology, Changsha, Hunan 410073, PR China
Abstract:Carbon fiber-reinforced silicon carbide (C/SiC) nuts and bolts (M8) with different fiber preform structures were prepared by precursor infiltration and pyrolysis. The influences of fiber preform structures on the mechanical properties of C/SiC nuts and bolts, as well as the failure behaviors of threaded joints were studied. A C/SiC nut, which was fabricated by using the preform prepared by stacking 3K carbon fiber cloth followed by stitching, had the highest shearing strength (64.5 MPa). The bolt with the preform prepared by alternatively stacking 3 K carbon fiber cloth and unidirectional layer of carbon fiber tows followed by stitching had the highest extreme tensile strength (243.2 MPa) and shearing strength (106.3 MPa), but low thread tooth bearing ability (3.5 kN) and critical thread engagement length (9 mm). It is suitable for applications emphasizing the extreme tensile or shearing strengths of threaded joints or possessing enough thread engagement length to ensure bolt rupture as the failure mode. The bolt with the perform prepared by stacking 1K carbon fiber cloth followed by stitching had the highest thread tooth bearing ability (5.0 kN) and the lowest critical thread engagement length (6 mm), as well as moderate extreme tensile strength (163.0 MPa) and shearing strength (82.1 MPa). It works effectively for applications concerning thread tooth strength or possessing limited thread engagement length. Therefore, the preform for preparing a C/SiC bolt should be selected according to its application requirements.
Keywords:C/SiC  Bolt  Nut  Mechanical properties
本文献已被 ScienceDirect 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号