Reaction control of TiB2 formation from titanium metal and amorphous boron
Authors:Hideaki Itoh  Tsuneaki Matsudaira  Shigeharu Naka  Hiroshi Hamamoto
Affiliation:(1) Synthetic Crystal Research Laboratory, Faculty of Engineering, Nagoya University, Furo-cho, Chikusa-ku, 464 Nagoya, Japan;(2) Toyota Central Research and Development Laboratories, Inc., Nagakute-cho, 480-11 Aichi Pref., Japan
Abstract:TiB2 powder was synthesized by a controlled formation reaction from titanium metal and amorphous boron. Precursory TiB2 formed by the pretreatment of the mixed powder (mole ratio: B/Ti=2.0) at 600° C for 60 min in an argon stream. Hollow TiB2 powder with an average grain size of 15mgrm was obtained by subsequent heat treatment above 900° C for more than 60 min in an argon stream. The formation reaction of TiB2 powder was further controlled by pretreatment of the mixed powder at 600° C for 60 min in a hydrogen and argon stream and subsequent heat treatment at 1000° C for 360 min in an argon stream, when hollow-free TiB2 powder was formed by a milder formation reaction between amorphous boron and the reformed titanium metal with hydrogen diffused lattice.
Keywords:
本文献已被 SpringerLink 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号