江西某硫尾矿中白钨矿的浮选回收试验
引用本文:罗文,邵辉. 江西某硫尾矿中白钨矿的浮选回收试验[J]. 金属矿山, 2016, 45(7): 186-188. DOI: 10.3969/j.issn.1001-1250.2016.07.036
作者姓名:罗文  邵辉
作者单位:武汉理工大学资源与环境工程学院,湖北 武汉 430070
摘    要:江西某硫尾矿中有用矿物主要为白钨矿,WO3含量为0.22%。为确定该尾矿中白钨矿的回收工艺,在实验室进行了选矿试验。结果表明:试样采用1粗3精3扫常温浮选,常温精矿以水玻璃为脱药剂在90 ℃下搅拌脱药,再采用1粗4精3扫加温浮选流程处理,最终得到WO3品位为67.03%、回收率为76.17%的白钨精矿。

关 键 词:硫尾矿  白钨矿  常温浮选  加温浮选  

Recovery Research on Scheelite Ore of Sulfur Tailings in Jiangxi
Luo Wen,Shao Hui. Recovery Research on Scheelite Ore of Sulfur Tailings in Jiangxi[J]. Metal Mine, 2016, 45(7): 186-188. DOI: 10.3969/j.issn.1001-1250.2016.07.036
Authors:Luo Wen  Shao Hui
Affiliation:College of Resource and Environment Engineering,Wuhan University of Technology,Wuhan 430070,China
Abstract:The sulfur tailings from Jiangxi contain 0.22% WO3 .For determining the recovery process of scheelite from tailings,the mineral processing experiments were investigated in lab.The results show the scheelite concentrate with WO3 grade of 67.03% and recovery of 76.17% can be got by adopting the normal temperature flotation of single-stage roughing,three-stage cleaning,three-stage scavenging,sodium silicate as reagent removal agent,stirring at 90 ℃,then the heating flotation of cleaning flowsheet of single-stage roughing,four-stage cleaning and three-stage scavenging process.
Keywords:Sulfur tailings  Scheelite  Normal temperature flotation  Heating temperature flotation