Abstract:Mold wear during the casting of Ti-6Al-4V in a permanent (steel) mold was investigated using a combination of macro- and micro-scale observations and measurements. For this purpose, a steel mold with interchangeable inserts of three candidate mold steels (H13, P20, and 1040) was used. Inserts were removed at regular intervals during casting under prototype-production conditions and inspected to assess mold wear. Two major mold wear types were identified: soldering and “wrinkling.” Soldering was concluded to be a result of local over-heating of the mold, and wrinkling a result of cyclic stresses caused by a combination of solid-state phase transformations and large temperature gradients. The 1040 inserts performed the best; soldering was less severe and wrinkling did not occur. The better performance of the 1040 inserts was attributed to lower mold temperatures and thermal gradients due to the higher thermal conductivity of 1040 relative to H13 or P20.
Keywords:H13 steel  mold wear  P20 steel  permanent mold casting  Ti-6Al-4V  type 1040 steel
本文献已被 SpringerLink 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号