A study on low magnetic permeability gas tungsten arc weldment of AISI 316LN stainless steel for application in electron accelerator
Affiliation:1. National Synchrotron Radiation Research Center, 101 Hsin-Ann Road, Hsinchu Science Park, Hsinchu 30076, Taiwan;2. National Tsing Hua University, 101, Section 2 Kuang Fu Road, Hsinchu 30013, Taiwan;1. Fusion Research and Development Directorate, Japan Atomic Energy Agency, 2-166 Obuchi-Omotedate, Rokkasho, Aomori 039-3212, Japan;2. Joining and Welding Research Institute, Osaka University, 11-1 Mihogaoka, Ibaraki, Osaka 567-0047, Japan
Abstract:Low magnetic permeability is an important criterion in selection of the material of construction of beam pipes and vacuum chambers of electron accelerators for safeguarding against distortion of the magnetic field. In the modified design of new 20 MeV/30 mA Injector Microtron for the existing synchrotron radiation sources Indus-1 and Indus-2, AISI 316 LN stainless steel has been identified as the material of construction of its vacuum chamber. Welding of AISI 316LN stainless steel with conventional filler alloys like ER316L and ER317L of AWS A5.9 produces duplex weld metal with 3–8% ferro-magnetic delta ferrite to avoid solidification cracking. The results of the study has demonstrated that GTAW of AISI 316LN SS with high Mn adaptation of W 18 16 5 N L filler produced a crack free non-magnetic weld with acceptable mechanical properties. Moreover, AISI 316LN stainless steel is not required to be solution annealed after the final forming operation for obtaining a low magnetic permeability, thereby avoiding solution annealing of large vacuum chamber in vacuum/controlled atmosphere furnace and associated problems of distortion. Besides Injector Microtron, the study also provides useful input for design of future indigenous accelerators with vacuum chambers of austenitic stainless steel.
Keywords:Accelerator  Austenitic stainless steel  Non-magnetic weld  Delta ferrite free weld  High Mn filler  Solidification cracking
本文献已被 ScienceDirect 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号