首页 | 本学科首页   官方微博 | 高级检索  
     

Hot compression deformation behavior of MB26 magnesium alloy
引用本文:杜志惠 张绪虎 方西亚 张晓娟 陈永来 张宇玮. Hot compression deformation behavior of MB26 magnesium alloy[J]. 中国有色金属学会会刊, 2007, 17(A01): 400-404
作者姓名:杜志惠 张绪虎 方西亚 张晓娟 陈永来 张宇玮
作者单位:[1]Aerospace Research Institute of Materials and Processing Technology, Beijing 100076, China [2]Central South University, Changsha 410083, China
摘    要:The flow stress features of MB26 magnesium alloy were studied by isothermal compression at 300-450 ℃ and strain rate of 0.001^-1 s J with Gleeble 1500 thermal simulator. In addition, the deformation activation energy Q was calculated. The results show that the strain rate and deformation temperature have obvious effect on the true stress. The peak value of flow stress becomes larger with increasing strain rate at the same temperature, and gets smaller with the increasing deformation temperature at the same strain rate. The alloy shows partial dynamic recrystallization. The flow stress of MB26 magnesium alloy during high temperature deformation can be represented by Zener-Hollomon parameter including the Arrhemius term. The temperatt, re range of 350-400℃ is suggested for hot-forming of this alloy.

关 键 词:镁合金 热压缩成型技术 流体压力 物理特征
收稿时间:2007-07-15
修稿时间:2007-09-10

Hot compression deformation behavior of MB26 magnesium alloy
DU Zhi-hui, ZHANG Xu-hu, FANG Xi-ya, ZHANG Xlao-juan , CHEN Yong-lai, ZHANG Yu-wei. Hot compression deformation behavior of MB26 magnesium alloy[J]. Transactions of Nonferrous Metals Society of China, 2007, 17(A01): 400-404
Authors:DU Zhi-hui   ZHANG Xu-hu   FANG Xi-ya   ZHANG Xlao-juan    CHEN Yong-lai   ZHANG Yu-wei
Abstract:
Keywords:MB26 magnesium alloy   hot compression deformation   flow stress