首页 | 本学科首页   官方微博 | 高级检索  
     

内蒙古某金矿阶段磨矿—阶段浮选试验研究
引用本文:任慧,刘杰,王勋,杨新华.内蒙古某金矿阶段磨矿—阶段浮选试验研究[J].矿产保护与利用,2021,41(2):106-111.
作者姓名:任慧  刘杰  王勋  杨新华
作者单位:1.东北大学 资源与土木工程学院, 辽宁 沈阳 110819
摘    要:内蒙古某金矿山原矿金品位为2.83 g/t,其中金银矿物嵌布粒度细且与脉石矿物连生紧密,不利于单体解离。为了进一步实现金矿的高效富集,在工艺矿物学研究基础上确定了阶段磨矿—阶段浮选工艺流程,并进行了详细的浮选试验。结果表明:(1)矿石中含有少量银金矿和碲银矿,主要载金矿物为黄铁矿和磁黄铁矿,其中黄铁矿中金含量为62.20 g/t,占矿石中金总量的41.61%,磁黄铁矿中金含量为32.30 g/t,占矿石中金总量的23.77%,脉石矿物以石英、绿帘石、绿泥石、长石和云母等矿物为主。(2)以"丁基黄药+丁铵黑药"为主要捕收剂,5460为辅助捕收剂,在一段磨矿细度为-0.074 mm占90%、二段磨矿细度为-0.038 mm占75%的条件下,采用两次粗选三次精选两次扫选、中矿顺序返回的闭路工艺流程,获得了金品位38.00 g/t、回收率80.06%的精矿产品,较原浮选流程中金矿品位提高13.8%个百分点,回收率提高6.75个百分点,有效实现了金矿的富集。 

关 键 词:金矿    阶段磨矿    浮选    富集
收稿时间:2021-03-18

Experimental Study on Stage Grinding and Stepwise Flotation of a Gold Ore in Inner Mongolia
REN Hui,LIU Jie,WANG Xun,YANG Xinhua.Experimental Study on Stage Grinding and Stepwise Flotation of a Gold Ore in Inner Mongolia[J].Conservation and Utilization of Mineral Resources,2021,41(2):106-111.
Authors:REN Hui  LIU Jie  WANG Xun  YANG Xinhua
Affiliation:1.School of Resource and Civil Engineering, Northeastern University, Shenyang 110819, China2.Shandong Gold Smelting Co., Ltd, Yantai 26144, China
Abstract:In a gold mine in Inner Mongolia, the gold grade in the raw ore is 2.83 g/t. The gold occurred as fine disseminated particles in gold ore, and the embedding relationship between gold and gangue minerals was close, indicating the recovery of gold minerals was difficult. In order to realize the effective concentration of the gold ore, the process flow of stage grinding and separation was determined on the basis of process mineralogy tests, and the flotation condition tests were carried out. Results demonstrated that the gold ore contains a slight amount of precious minerals such as electrum and hessite. The main gold-bearing minerals are pyrite and pyrrhotite. The gold content in pyrite was 62.20 g/t and distribution 41.61%, and that in pyrrhotite was 32.30 g/t and 23.77%. The gangue minerals mainly were quartz, epidote, chlorite, feldspar and mica. The flotation test results showed that the concentrate with gold grade of 38.00 g/t and recovery of 80.06 % was obtained under using butyl xanthate + butylamine dithiophosphate as main collector and 5460 as auxiliary collector, and the first stage grinding fineness of -0.074 mm 90% and the second stage grinding fineness of -0.038 mm 75% with closed-circuit flowsheet containing two roughing, two cleaning and three scavenging, and the middling returned in sequence. In addition, compared with the original flotation process, the gold grade and recovery of concentrate were increased by 13.8% and 6.75%, respectively. 
Keywords:
本文献已被 CNKI 万方数据 等数据库收录!
点击此处可从《矿产保护与利用》浏览原始摘要信息
点击此处可从《矿产保护与利用》下载全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号