首页 | 本学科首页   官方微博 | 高级检索  
     

赤铁矿选矿工艺研究
引用本文:王亚彬,周平,裴斌.赤铁矿选矿工艺研究[J].矿冶,2012,21(3):28-29.
作者姓名:王亚彬  周平  裴斌
作者单位:昆明理工大学,昆明,650093
摘    要:云南某铁矿铁平均品位为38.1%,主要以赤铁矿和褐铁矿形式存在,有害元素硫、砷的含量极低,砷含量为0.002%,硫含量为0.01%,对矿石的利用不造成影响。矿石中磷含量高,磷平均含量为0.44%对矿石的影响较大。采用强磁选和重选方法对矿石进行了研究,探索一个合理可行的流程,在提高铁的品位和回收率的基础上降低磷和硅的含量。

关 键 词:氧化铁  重选  强磁选
收稿时间:2011/9/29 0:00:00
修稿时间:2011/9/30 0:00:00

The technology research of haematite separation
wangyabin,zhouping and peibin.The technology research of haematite separation[J].Mining & Metallurgy,2012,21(3):28-29.
Authors:wangyabin  zhouping and peibin
Affiliation:(Kunming University of Science and Technology,Kunming 650093,China)
Abstract:The average iron grade of an iron ore in Yunnan is 38.1%,mainly occurring in the form of hematite and limonite with very low content of harmful elements sulfur(0.002%) and arsenic(0.01%),which has no impact on the utilization of the ore.The phosphorus content in the ore is high with average content of 0.44% with relatively large influence on the ore.High-intensity magnetic separation and gravity separation are adopted to study the ore and a feasible process is explored,which can improve the grade and recovery of iron and reduce the content of silicon and phosphorus as well.
Keywords:iron oxide  gravity separation  high-intensity magnetic separation
本文献已被 CNKI 万方数据 等数据库收录!
点击此处可从《矿冶》浏览原始摘要信息
点击此处可从《矿冶》下载全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏