龙烟鲕状赤铁矿石选矿试验研究
引用本文:郭秀平,庞玉荣,田江涛,庞雪敏.龙烟鲕状赤铁矿石选矿试验研究[J].金属矿山,2013,43(3):82-85.
作者姓名:郭秀平  庞玉荣  田江涛  庞雪敏
作者单位:河北省地矿中心实验室
摘    要:龙烟矿区宣龙式鲕状赤铁矿石的鲕粒由粒度为0.005~0.001 mm的隐晶质赤铁矿构成,赤铁矿中的铁占到总铁量的96.19%,有害元素S、P含量低。以工艺流程简洁、能耗低、可操作性强为目标,研究了该矿石的开发利用方案。结果表明,采用还原焙烧-磨矿-弱磁粗选-粗精矿再磨-弱磁精选流程处理,可获得铁品位62.46%、回收率83.56%的铁精矿。

关 键 词:鲕状赤铁矿  还原焙烧  弱磁选  磁选柱

Experimental Study of the Beneficiation of Longyan Oolitic Hematite Ore
Guo Xiuping , Pang Yurong , Tian Jiangtao , Pang Xuemin.Experimental Study of the Beneficiation of Longyan Oolitic Hematite Ore[J].Metal Mine,2013,43(3):82-85.
Authors:Guo Xiuping  Pang Yurong  Tian Jiangtao  Pang Xuemin
Affiliation:Central Laboratory of Geology and Mineral Resources of Hebei Province;
Abstract:Xuanlong-type oolitic hematite consists of aphanitic hematite with particle size of 0.005 ~ 0.001 mm, and iron element in hematite accounts for 96.19% of the total iron, and the contents of harmful elements S , P are low. The exploitation scheme for the ore is investigated to find out a process with feature of simple process, low energy consumption and good operability as a goal. The results show that iron concentrate with Fe grade of 62.46% and recovery rate of 83.56% was achieved by adopting the process of reduction roasting-grinding-rough low intensity magnetic separation-regrinding of rough concentrate-cleaning of low intensity magnetic separation.
Keywords:Oolitic hematite ore  Reduction roasting  Low intensity magnetic separation  Magnetic separation column