齐大山选矿分厂磁选精矿剪切絮凝正浮选研究
引用本文:苑宏倩,韩跃新,李艳军,刘杰,王泽红.齐大山选矿分厂磁选精矿剪切絮凝正浮选研究[J].金属矿山,2011,40(4):50-53.
作者姓名:苑宏倩  韩跃新  李艳军  刘杰  王泽红
作者单位:东北大学
基金项目:国家高技术研究发展计划(863计划)项目
摘    要:针对齐大山铁矿选矿分厂反浮选工艺不能有效回收微细粒铁矿物,导致尾矿品位较高的现象,在实验室以石油磺酸钠作为捕收剂和絮凝剂,进行了齐大山铁矿选矿分厂磁选精矿剪切絮凝正浮选研究。结果表明:使磁选精矿发生剪切絮凝的适宜条件为磨矿细度-0.037 mm占85%,矿浆pH=3,石油磺酸钠用量5 kg/t,水玻璃用量300 g/t,搅拌强度2 200 r/min,剪切絮凝时间6 min。在此条件下将磁选精矿剪切絮凝后进行1粗3精1扫闭路浮选,获得了精矿铁品位为66.80%,回收率为95.93%,尾矿铁品位仅5.03%的较好指标。

关 键 词:磁选精矿  剪切絮凝  正浮选  石油磺酸钠

Study on Shear Flocculation and Flotation of Magnetic Separation Concentrate in Qidashan Iron Ore
Yuan Hongqian,Han Yuexin,Li Yanjun,Liu Jie,Wang Zehong.Study on Shear Flocculation and Flotation of Magnetic Separation Concentrate in Qidashan Iron Ore[J].Metal Mine,2011,40(4):50-53.
Authors:Yuan Hongqian  Han Yuexin  Li Yanjun  Liu Jie  Wang Zehong
Affiliation:Northeastern University;
Abstract:Due to the high grade of flotation tailings that caused by the low recovery of fine particles in floatation process of Qidashan Iron Mine, Petroleum Sulfonate was used as collector and flocculating agent to make the shear flocculation and flotation tests on Qidashan magnetic separation concentrate in laboratory test.The results indicated that the optimum conditions for the shear flocculation and flotation are the grinding fineness of -0.037 mm 85%, pulp pH at 3, the dosage of Petroleum Sulfonate as 5 kg/t, water glass of 300 g/t, stirring intensity of 2 200 r/min, and shear time at 6 min.Under this condition, a good iron concentrate index with Fe grade of 66.80% and Fe recovery of 95.93% and Fe grade of tailings 5.03% only were obtained firstly by the shear flocculation of magnetic separation concentrate, then following by one closed-circuit flotation process of one-roughing, one-scavenging and three-cleaning.
Keywords:Magnetic separation concentrate  Shear Flocculation  Flotation  Petroleum Sulfonate