摘    要:辽宁某钼尾矿粒度较粗,+0.074 mm占75.16%,铁品位为7.26%,铁主要以磁性铁形式存在,在0.074~0.038 mm粒级有一定的富集现象。对该尾矿进行了磁性铁矿物选矿回收试验。结果表明,试样采用一段弱磁选、一段中磁选、中磁选精矿再磨后二段弱磁选、两段弱磁选精矿合并后磁悬浮精选机精选,可获得铁品位59.12%、铁回收率为70.05%的铁精矿。

关 键 词:钼尾矿  磁性铁矿物  磁选  磁悬浮精选机

Experiment on Recycling of Magnetic Iron Mineral in Molybdenum Tailings by Magnetic Separation
Zhang Xianglong,Ren Ruichen,Zhang Shengnan,Lu Feng.Experiment on Recycling of Magnetic Iron Mineral in Molybdenum Tailings by Magnetic Separation[J].Metal Mine,2017,46(5):185-188.
Authors:Zhang Xianglong  Ren Ruichen  Zhang Shengnan  Lu Feng
Affiliation:1.College of Mining Technology,Liaoning Technology University,Fuxin 123000,China;2.Longi Magnet Co.,Ltd.,Fushun 113122,China;3.College of Resources and Environment,Southwest University,Chongqing 400715,China;
Abstract:Molybdenum tailings of Liaoning were comparatively coarse grained,75. 16% above 0. 074 mm. The iron grade of ore was 7. 26% and magnetic iron was its major existence form,there were definite phenomenon of enrichment in grain level range from 0. 074 to 0. 038 mm. Recycling magnetic iron minerals from the tailings was conducted. Results showed that through process including one stage low intensity magnetic separation,one stage middle magnetic separation,and then regrinding middle magnetic separation concentrate and second stage low intensity magnetic separation, concentrates of two stages low intensity magnetic separation mixed and then cleaning by magnetic levitation separator,final iron concentrate obtained with iron grade of 59. 12%,iron recovery of 70. 05%.
Keywords:Molybdenum tailings  Magnetic iron mineral  Magnetic separation  Magnetic levitation separator
本文献已被 CNKI 万方数据 等数据库收录!
点击此处可从《金属矿山》浏览原始摘要信息
点击此处可从《金属矿山》下载全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号