摘    要:在白钨原矿含WO3约为0.06%的情况下,采用常温粗选—粗精矿浓缩—浓浆高温脱药—常温精选工艺,可得到品位为25%左右、回收率为70%的钨精矿。

关 键 词:低品位白钨矿  浮选回收  工艺

Flotation of low grade scheelite
XIN Yatao,DENG Shuangli.Flotation of low grade scheelite[J].Mining & Processing Equipment,2012(2):88-90.
Authors:XIN Yatao  DENG Shuangli
Affiliation:China Molybdenum Co.,Ltd.,Luanchuan 471500,Henan,China
Abstract:While the content of WO3 in scheelite was about 0.06%,the process flow of rough flotation at the room temperature-thickening of coarse concentrate-reagent removing from concentrated slurry at high temperature-cleaning flotation at room temperature was applied,and then tungsten concentrate with the grade of 25% and the recovery rate of 70% was obtained.