80 t转炉冶炼SCM435钢留渣操作技术研究
引用本文:霍志斌,赵彦岭,王建林,王秋坤.80 t转炉冶炼SCM435钢留渣操作技术研究[J].特殊钢,2018,39(5):14-17.
作者姓名:霍志斌  赵彦岭  王建林  王秋坤
作者单位:邢台钢铁有限责任公司炼钢厂,邢台054027
摘    要:试验研究了转炉冶炼SCM435钢时留渣操作(留渣分数1/3~2/3渣量)对石灰加入量、平衡碱度的留渣炉数和终渣碱度的影响,总结了留渣操作的注意事项。80 t转炉实施留渣操作后,留渣率达到68.9%,成品P含量≤0.015%的比例比从留渣前的49.3%提高到62.2%,同时石灰消耗降低了4.5 kg/t、每炉渣中铁损失减少230 kg。

收稿时间:2018-04-03

A Study on Remaining Slag Operation of 80 t BOF Steelmaking Steel SCM435
Huo Zhibin,Zhao Yanling,Wang Jianlin,Wang Qiukun.A Study on Remaining Slag Operation of 80 t BOF Steelmaking Steel SCM435[J].Special Steel,2018,39(5):14-17.
Authors:Huo Zhibin  Zhao Yanling  Wang Jianlin  Wang Qiukun
Affiliation:Steelmaking Works, Xingtai Iron and Steel Co Ltd, Xingtai 054027
Abstract:The effect of remaining slag operation (remaining slag fraction 1/3 ~ 2/3 slag amount) of BOF steelmaking steel SCM435 on lime adding amount, remaining slag heats of equilibrium basicity and end slag basicity is tested and studied, and the points for attention in slag remaining operation are summarized. As the 80t BOF remaining slag operation is put into practice, the remaining slag rate is up to 68. 9% , the ratio of P content ≤ 0. 015% in product increases from original 49. 3% to 62. 2% , and the lime consumption decreases by 4. 5 kg/t, and the iron loss in slag decreases by 230 kg.