阳极氧化工艺条件对氮化钽烧结体电性能的影响
引用本文:刘莲云,段世钰,黄凯,朱鸿民.阳极氧化工艺条件对氮化钽烧结体电性能的影响[J].有色金属(冶炼部分),2012(9):51-54.
作者姓名:刘莲云  段世钰  黄凯  朱鸿民
作者单位:1. 北京科技大学冶金与生态工程学院,北京100083;北京交通大学理学院,北京100044
2. 山东省冶金设计院股份有限公司,济南,250101
3. 北京科技大学冶金与生态工程学院,北京,100083
基金项目:国家自然科学基金资助项目(51004008,21071014);国家基础研究发展计划(973计划)项目(2007CB613301)
摘    要:用纳米氮化钽粉末烧结制备了氮化钽烧结体,分析了烧结体的物相结构,研究了形成液种类、形成液浓度、温度、电流密度以及赋能电压等条件对氮化钽阳极氧化膜电性能的影响。结果表明,该烧结体是由纯氮化钽组成的,氮化钽阳极块体阳极氧化过程的最佳赋能工艺:磷酸溶液浓度0.01%,形成液温度55℃,电流密度40mA/g,形成电压小于16V。

关 键 词:氮化钽烧结体  电性能  阳极氧化
收稿时间:2/21/2012 1:38:38 PM
修稿时间:2/21/2012 1:38:38 PM

Effect of Anodizing Process Conditions on Electrical Characteristics of Sintered Tantalum Nitride Anodes
Liu Lianyun,Duan Shiyu,Huang Kai and Zhu Hongmin.Effect of Anodizing Process Conditions on Electrical Characteristics of Sintered Tantalum Nitride Anodes[J].Nonferrous Metals(Extractive Metallurgy),2012(9):51-54.
Authors:Liu Lianyun  Duan Shiyu  Huang Kai and Zhu Hongmin
Affiliation:1(1.School of Metallurgical and Ecological Engineering,University of Science and Technology Beijing,Beijing 100083,China; 2.School of Science,Beijing Jiaotong University,Beijing 100044,China; 3.Shandong Province Metallurgical Engineering Co.,Ltd,Jinan 250101,China)
Abstract:Sintered tantalum nitride anodes were prepared with tantalum nitride nanopowders.The sintered anode slugs were examined by XRD.The effects of formation solution in terms of its variety,concentration and temperature,current density and formation voltage on electrical characteristics were studied.The results show that the anode slugs are made of pure tantalum nitride phase,and the optimum anodizing process conditions including H3PO4 concentration of 0.01%,temperature of formation solutions of 55 ℃,current density of 40 mA/g and the formation voltage of less than 16 V.
Keywords:sintered tantalum nitride anodes  electrical characteristics  anodization