热轧带钢尾部红褐色柳叶状氧化铁皮缺陷分析 |
| |
引用本文: | 张昭,李建龙,王强.热轧带钢尾部红褐色柳叶状氧化铁皮缺陷分析[J].甘肃冶金,2016(6):34-37. |
| |
作者姓名: | 张昭 李建龙 王强 |
| |
作者单位: | 酒钢宏兴股份有限公司碳钢薄板厂,甘肃 嘉峪关,735100 |
| |
摘 要: | 针对热轧带钢尾部红褐色柳叶状氧化铁皮缺陷,分析了缺陷形貌特征及分布规律,经过现场试验跟踪,确定了缺陷产生来源,采取了相应的控制措施,该缺陷得到消除。
|
关 键 词: | 氧化铁皮缺陷 红褐色柳叶状 除鳞效果 |
Analysis the Defects of Red Brown Willow Leaf Shape Iron Oxide Scales on the Tail of Hot Rolled Strip |
| |
Abstract: | This article aims at the defects of the red brown willow shaped iron oxide in the tail of the hot rolling strip , The morphology characteristics and distribution of defects are analyzed. After field test tracking,identify the source of defects. he corresponding control measures are taken.The defect is eliminated. |
| |
Keywords: | iron oxide defect the red brown willow shaped scale removal effect |