摘    要:Chemical modification (CM) and deposition-precipitation (DP) methods were used for the dispersion of active Au nanoparticles on mesoporous silica materials in this work. XRD, TEM, N2 adsorption isotherms and UV-Vis absorption spectra were used to characterize in detail Au-SBA-15 materials prepared by the two methods. The analysis results showed that high loading (1.7%, by mass) and uniform Au nanoparticles (approximately 3 nm) were dispersed in the channels of mesoporous SBA-15 by the CM method. While for the DP method, most of Au nanoparticles with the size of 10—15nm were aggregated outside of the channels of SBA-15 and the actual loading of Au was only 0.38% (by mass).

关 键 词:化学药品修饰  沉积物沉淀  金毫微粒  介孔分子筛  分子筛合成
收稿时间:26 October 2006
修稿时间:2006-10-26

Dispersion of active Au nanoparticles on mesoporous SBA-15 materials
ZHOU Lihui,HU Jun,XIE Songhai,LIU Honglai.Dispersion of active Au nanoparticles on mesoporous SBA-15 materials[J].Chinese Journal of Chemical Engineering,2007,15(4):507-511.
Authors:ZHOU Lihui  HU Jun  XIE Songhai  LIU Honglai
Affiliation:a State Key Laboratory of Chemical Engineering and Department of Chemistry, East China University of Science and Technology, Shanghai 200237, China b Department of Chemistry, Fudan University, Shanghai 200433, China
Abstract:Chemical modification (CM) and deposition-precipitation (DP) methods were used for the dispersion of active Au nanoparticles on mesoporous silica materials in this work. XRD, TEM, N2 adsorption isotherms and UV-Vis absorption spectra were used to characterize in detail Au-SBA-15 materials prepared by the two methods.The analysis results showed that high loading (1.7%, by mass) and uniform Au nanoparticles (approximately 3 nm)were dispersed in the channels of mesoporous SBA-15 by the CM method. While for the DP method, most of Au nanoparticles with the size of 10-15 nm were aggregated outside of the channels of SBA-15 and the actual loading of Au was only 0.38% (by mass).
Keywords:SBA-15  Au-SBA-15  Au nanoparticles  deposition-precipitation  chemical modification