首页 | 本学科首页   官方微博 | 高级检索  
     

Low-temperature sintering and microwave dielectric properties of Li2MgTi3O8 ceramics doped with BaCu(B2O5)
引用本文:包燕,陈国华,侯美珍,韩作鹏,邓开能,杨云,袁昌来,周昌荣,刘心宇.Low-temperature sintering and microwave dielectric properties of Li2MgTi3O8 ceramics doped with BaCu(B2O5)[J].中南工业大学学报(英文版),2012,19(5):1202-1205.
作者姓名:包燕  陈国华  侯美珍  韩作鹏  邓开能  杨云  袁昌来  周昌荣  刘心宇
作者单位:[1]School of Materials Science and Engineering, Guilin University of Electronic Technology, Guilin 541004, China [2]Guangxi Key Laboratory of Information Materials,Guilin University of Electronic Technology, Guilin 541004, China
基金项目:Foundation item: Project(2010GXNSFA013029) supported by the Natural Science Foundation of Guangxi Province, China; Project(101059529) supported by National Undergraduate Innovation Program of the Ministry of Education of China
摘    要:

关 键 词:微波介电性能  陶瓷烧结  低温烧结  B掺杂  扫描电子显微镜  X射线衍射仪  低温共烧陶瓷  微观结构

Low-temperature sintering and microwave dielectric properties of Li2MgTi3O8 ceramics doped with BaCu(B2O5)
Yan Bao, Guo-hua Chen, Mei-zhen Hou, Zuo-peng Han, Kai-neng Deng, Yun Yang, Chang-lai Yuan, Chang-rong Zhou and Xin-yu Liu.Low-temperature sintering and microwave dielectric properties of Li2MgTi3O8 ceramics doped with BaCu(B2O5)[J].Journal of Central South University of Technology,2012,19(5):1202-1205.
Authors:Yan Bao  Guo-hua Chen  Mei-zhen Hou  Zuo-peng Han  Kai-neng Deng  Yun Yang  Chang-lai Yuan  Chang-rong Zhou and Xin-yu Liu
Abstract:The influences of BaCu(B2O5) (BCB) addition on sintering, microstructure and microwave dielectric properties of Li2MgTi3O8 ceramics were investigated using X-ray diffractometry, scanning electron microscopy and microwave dielectric measurements. The experimental results show that a small amount of BaCu(B2O5) addition can effectively reduce the sintering temperature to 900 °C, and induce only a limited degradation of the microwave dielectric properties. Typically, the best microwave dielectric properties of ɛ r=24.5, Q×f =24 622 GHz, τ f=4.2×10−6 °C−1 are obtained for 1.0% BCB-doped Li2MgTi3O8 ceramics sintered at 900 °C for 3 h. The BCB-doped Li2MgTi3O8 ceramics can be compatible with Ag electrode, which may be a strong candidate for low temperature co-fired ceramics applications.
Keywords:ceramics  dielectrics  low-temperature co-fired ceramics  microwave dielectric properties