烧结温度对TiO2压敏陶瓷非线性和介电性质的影响
引用本文:孟凡明,孙兆奇.烧结温度对TiO2压敏陶瓷非线性和介电性质的影响[J].功能材料,2006,37(7):1149-1152,1159.
作者姓名:孟凡明  孙兆奇
作者单位:安徽大学,物理与材料科学学院,信息材料与器件重点实验室,安徽,合肥,230039
摘    要:基于一次烧结工艺,通过改变烧结温度,制备5种组分相同、(Sr,Bi,Si,Ta)掺杂的TiO2陶瓷试样.借助于伏安特性、介电频率特性、损耗频率特性及非线性系数的测定,研究烧结温度对TiO2基压敏陶瓷压敏和介电性质的影响.结果表明,在1200~1400℃范围内,随着烧结温度的降低,陶瓷的压敏电压降低、介电常数增大,同时非线性系数有所减小.兼顾陶瓷压敏和介电特性,烧结温度选择1350℃为宜.

关 键 词:压敏陶瓷  TiO2  电性能  缺陷  varistors  TiO2  electrical  property  defect
文章编号:1001-9731(2006)07-1149-04
收稿时间:2005-09-13
修稿时间:2005-09-132005-12-15

Influence of sintering temperature on nonlinear electrical behavior anddielectric properties of TiO2-based varistor ceramics
MENG Fan-ming,SUN Zhao-qi.Influence of sintering temperature on nonlinear electrical behavior anddielectric properties of TiO2-based varistor ceramics[J].Journal of Functional Materials,2006,37(7):1149-1152,1159.
Authors:MENG Fan-ming  SUN Zhao-qi
Affiliation:Anhui Key Laboratory of Information Materials and Devices, School of Physics and Materials Science, Anhui University, Hefei 230039,China
Abstract:Based on the single sintering process, five disk samples of (Sr, Bi, Si, Ta)-doped TiO2-based varistor ceramics were fabricated, by sintering separately at the temperatures of 1200 to 1400 ℃ for 2.5h. The influence of sintering temperature on the nonlinear electrical behavior and dielectric properties of these samples were investigated by measuring the characteristics of J-V, dielectric constant, dielectric loss and nonlinear coefficient. It was found that, between 1200 and 1400℃, both breakdown electrical field and nonlinear coefficient decreased and dielectric constant increased gradually with decreasing sintering temperature. It is suggested that the sintering temperature should be about 1350℃ considering both nonlinear electrical behavior and dielectric properties of TiO2-based varistor ceramics.
Keywords:TiO2  electrical property  defect