Abstract: | The Si-TaSi2 eutectic in situ composite, which has highly-aligned and uniformly-distributed TaSi2 fibers in the Si matrix, can be obtained when the solidification rate changes from 0.3 to 9.0 mm/min. It is very interesting that one or two TaSi2 fibers are curved when the solidification rate reaches 6.0 mm/min, although it is very brittle in general. The formation mechanism of the curved fiber is discussed and mechanical properties of the TaSi2 fibers are examined by nanoindentation. It is found that the har... |