摘    要:利用冻融循环法制备了羧基化多壁碳纳米管(MWCNTs)/聚乙二醇(PEG)-聚乙烯醇(PVA)复合水凝胶。考察了不同质量配比下MWCNTs/PEG-PVA复合水凝胶的微观形貌变化,并研究了复合凝胶的溶胀性能、拉伸强度、热稳定及导电性能。结果表明,加入MWCNTs后MWCNTs/PEG-PVA复合凝胶仍具有多孔的三维网状结构但孔径尺寸变小。当MWCNTs与PVA的质量比大于1.0∶100时,MWCNTs/PEG-PVA复合凝胶的孔洞均匀性降低。随着MWCNTs量的增加,MWCNTs/PEG-PVA复合凝胶的溶胀度及拉伸强度均先升高后降低。当MWCNTs与PVA的质量比为1.0∶100时,MWCNTs/PEG-PVA复合凝胶的溶胀度达到最大(1450%),孔隙率最高(75.8%),拉伸强度及断裂伸长率达到最大值,分别为0.97 MPa和384.0%。MWCNTs的加入提高了MWCNTs/PEG-PVA复合凝胶的热稳定性,MWCNTs/PEG-PVA复合凝胶的初始热分解温度从235℃上升至260℃;随着MWCNTs量的增加,MWCNTs/PEG-PVA复合凝胶的电导率从1.10×10-6 S/cm升高至6.96×10-4 S/cm。

关 键 词:碳纳米管  聚乙二醇  聚乙烯醇  水凝胶  微观结构  拉伸强度  电导率  
收稿时间:2016-07-14

Preparation and properties of MWCNTs reinforced polyethylene glycol-polyvinyl alcohol composite hydrogel
XU Zhaoyang,LI Jianyu,JIANG Xiangdong,ZHOU Huan,SHI Xiaomei.Preparation and properties of MWCNTs reinforced polyethylene glycol-polyvinyl alcohol composite hydrogel[J].Acta Materiae Compositae Sinica,2017,34(6):1191-1198.
Authors:XU Zhaoyang  LI Jianyu  JIANG Xiangdong  ZHOU Huan  SHI Xiaomei
Affiliation:College of Materials Science and Engineering, Nanjing Forestry University, Nanjing 210037, China
Abstract:Carboxy-functionalized multi-walled carbon nanotubes(MWCNTs)/polyethylene glycol (PEG)-poly-vinyl alcohol (PVA) composite hydrogels were prepared by the freezing/thawing method.The microstructure,swelling property,tensile strength,thermal stability and conductivity of MWCNTs/PEG-PVA composite hydrogels with different mass ratios were studied.The results show that the MWCNTs/PEG-PVA hydrogel still has a porous 3D structure,but the pore size becomes smaller after the addition of MWCNTs.When the mass ratio of MWCNTs to PVA is larger than 1.0:100,the uniformity of the porous structure of the MWCNTs/PEG-PVA hydrogel decreases.With the increment of MWCNTs content,the swelling degree and tensile strength of the MWCNTs/PEG-PVA composite hydrogel increase first and then decrease.When the mass ratio of MWCNTs to PVA is 1.0:100,the swelling degree and porosity of the MWCNTs/PEG-PVA hydrogel reach the maximum (1450% and 75.8%,respectively).The tensile strength and elongation reach a maximum value of 0.97 MPa and 384.0%,respectively.The addition of MWCNTs improves the thermal stability of the composite hydrogel,and the initial thermal decomposition temperature of MWCNTs/PEG-PVA composite hydrogel increases from 235℃ to 260℃.With the increment of the amount of MWCNTs,the conductivity of the composite hydrogel increases from 1.10×10-6 S/cm to 6.96×10-4 S/cm.
Keywords:carbon nanotubes  polyethylene glycol  polyvinyl alcohol  hydrogel  microstructure  tensile strength  conductivity
本文献已被 CNKI 万方数据 等数据库收录!
点击此处可从《复合材料学报》浏览原始摘要信息
点击此处可从《复合材料学报》下载全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号