基金项目:supported by a grant from the Metals Bank by the Ministry of Knowledge Economy and a grant-in-aid for the National Core Research Center Program (No.R15-2006-022-02001-0)
摘    要:The effects of Ca and Sr addition on the microstructure and creep properties of Mg-4Al-2Sn alloys were examined.Tensile tests at 25℃ and 200℃ and creep tests at 150℃ and 200℃ were carried out to estimate the room temperature and high temperature mechanical properties of these alloys.The microstructure of the Mg-4Al-2Sn alloy showed dendriticα-Mg,Mg17Al12 and Mg2Sn phases.The latter two phases precipitated along the grain boundaries.The addition of Ca and Sr resulted in the formation of ternary CaMgSn and SrMgSn phases within the grain.The grain size was reduced slightly with the addition of Sr and Ca.The tensile strength was decreased by the addition of Ca and Sr at room temperature.However,the high temperature tensile strength was increased.The creep strength was improved by the addition of Ca and Sr.

关 键 词:蠕变性能  合金  高温拉伸强度    铸造    高温力学性能  显微组织
收稿时间:23 September 2009

Microstructure and creep properties of Mg-4Al-2Sn-1(Ca,Sr) alloys
B.H.KIM,K.C.PARK,Y.H.PARK,I.M.PARK.Microstructure and creep properties of Mg-4Al-2Sn-1(Ca,Sr) alloys[J].Transactions of Nonferrous Metals Society of China,2010,20(7):1184-1191.
Authors:BHKIM  KCPARK  YHPARK  IMPARK
Affiliation:B.H.KIM,K.C.PARK,Y.H.PARK,I.M.PARK Department of Material Science and Engineering,Pusan National University,San 30 Jangjeon-dong,Geumjeong-gu,Busan 609-735,Korea
Abstract:The effects of Ca and Sr addition on the microstructure and creep properties of Mg-4Al-2Sn alloys were examined. Tensile tests at 25 ℃ and 200 ℃ and creep tests at 150 ℃ and 200 ℃ were carried out to estimate the room temperature and high temperature mechanical properties of these alloys. The microstructure of the Mg-4Al-2Sn alloy showed dendritic α-Mg, Mg17Al12 and Mg2Sn phases. The latter two phases precipitated along the grain boundaries. The addition of Ca and Sr resulted in the formation of ternary CaMgSn and SrMgSn phases within the grain. The grain size was reduced slightly with the addition of Sr and Ca. The tensile strength was decreased by the addition of Ca and Sr at room temperature. However, the high temperature tensile strength was increased. The creep strength was improved by the addition of Ca and Sr.
Keywords:magnesium alloys  Ca  Sr  void initiation  mechanical properties  creep mechanism