Characteristics of electrodeposited RE-Ni-W-B-B_4C-MoS_2 composite coating
作者姓名:马克毅  郭忠诚  朱晓云  徐瑞东
作者单位:Faculty of Materials and Metallurgical Engineering Kunming University of Science and Technology,Kunming 650093,China,Faculty of Materials and Metallurgical Engineering Kunming University of Science and Technology,Kunming 650093,China,Faculty of Materials and Metallurgical Engineering Kunming University of Science and Technology,Kunming 650093,China,Faculty of Materials and Metallurgical Engineering Kunming University of Science and Technology,Kunming 650093,China
摘    要:1 INTRODUCTIONByuseofthecompositeelectrodepositingtech nique ,codepositionofsolidhardparticleswithmetalmatrixonthesurfacetoformacompositecoatingisoneoftheeffectivemethodstoimprovetheabrasionresistanceofmaterialsurface16 ] .Furthermore ,thecompositeelectrodepositingtechniquehasmanyad vantages ,suchassimpleprocess ,lowcost,operationatambienttemperatureanduninfluenceontheprop ertiesoftheinsidematrixmaterial,soitholdsanim portantstatusintheresearchanddevelopmentofabrasion resistantandantifri…


Characteristics of electrodeposited RE-Ni-W-B-B4C-MoS2 composite coating
MA Ke yi,GUO Zhong cheng,ZHU Xiao yun,XU Rui dong.Characteristics of electrodeposited RE-Ni-W-B-B_4C-MoS_2 composite coating[J].Transactions of Nonferrous Metals Society of China,2003,13(5).
Authors:MA Ke yi  GUO Zhong cheng  ZHU Xiao yun  XU Rui dong
Abstract:The high temperature oxidation resistance of RE-Ni-W-B-B4C-MoS2 composite coating, the effects of electrodeposition conditions on the morphologies of the coating and the effect of heat treatment temperature on its hardness, abrasion resistance and phase structure were investigated by using scanning electron microscope(SEM), X-ray diffractometer, microhardness tester and abrasion machine. The results show that the oxidation degree of RE-Ni-W-B-B4C-MoS2 composite coating is small when the temperature is lower than 700 ℃, but it increases sharply when the temperature is higher than 700 ℃. The hardness of RE-Ni-W-B-B4C-MoS2 composite coating increases with increasing heat treatment temperature, it comes up to the maximum value at 400 ℃,but it decreases gradually if the temperature rises continuously. The most favourable abrasion resistance was attained after RE-Ni-W-B-B4C-MoS2 composite coating being heat treated at 400 ℃. Without heat treating, it is mainly amorphous and partially crystallized, but wholly crystallized after being heat treated at 500 ℃. RE in the composite coating is in the form of CeO2 and additions of CeO2 and B4C can enhance the thermostability of RE-Ni-W-B-B4C-MoS2 composite coating.
Keywords:electrodeposition  RE Ni  W B  B  4C  MoS 2 composite coating  characteristics