首页 | 本学科首页   官方微博 | 高级检索  
     

碳酸盐岩酸蚀裂缝表面形态特征的实验研究
引用本文:冯炜,杨晨,陶善浔,王财忠,陆彦颖,张路锋,周福建.碳酸盐岩酸蚀裂缝表面形态特征的实验研究[J].岩性油气藏,2020,32(3):166-172.
作者姓名:冯炜  杨晨  陶善浔  王财忠  陆彦颖  张路锋  周福建
作者单位:1. 中国石油大学(北京)石油工程学院, 北京 102249;2. 意大利帕多瓦大学 地球科学学院, 帕多瓦 35131;3. 油气资源与探测国家重点实验室, 北京 102249;4. 华北水利水电大学 水利学院, 郑州 450046;5. 中国石油集团川庆钻探工程有限公司 钻采工程技术研究院, 四川 广汉 618300
基金项目:国家科技重大专项“超深裂缝性气藏井筒失稳机理及转向工艺优化研究”(编号:2016ZX05051)资助。
摘    要:酸压是碳酸盐岩储层改造的常规手段,酸液对岩石的非均质刻蚀使得裂缝表面呈现独特的形态特征,目前针对酸蚀前后裂缝表面形态特征的研究还不够深入。因此,通过室内实验借助3D扫描技术获得真实酸蚀裂缝表面几何形态数据,引入新的表征参数hnεh,定量描述了裂缝表面的起伏程度,对比了酸蚀前后裂缝表面形态的变化。结果表明:酸蚀反应掉水力裂缝的槽点;沿酸液流动方向形成明显的沟槽,凸起部分变缓,曲折比减小,总体起伏程度增大;垂直酸液流动方向上形成了连续的上下波动,曲折比和起伏程度均增大。

关 键 词:酸岩反应  裂缝表面形态  表征参数  起伏程度  
收稿时间:2019-08-01

Experimental study on the surface feature of acid-etched fractures in carbonate rocks
FENG Wei,YANG Chen,TAO Shanxun,WANG Caizhong,LU Yanying,ZHANG Lufeng,ZHOU Fujian.Experimental study on the surface feature of acid-etched fractures in carbonate rocks[J].Northwest Oil & Gas Exploration,2020,32(3):166-172.
Authors:FENG Wei  YANG Chen  TAO Shanxun  WANG Caizhong  LU Yanying  ZHANG Lufeng  ZHOU Fujian
Affiliation:(College of Petroleum Engineering,China University of Petroleum(Beijing),Beijing 102249,China;Department of Geosciences,University of Padova,Padova 35131,Italy;State Key Laboratory of Petroleum Resources and Prospecting,China University of Petroleum(Beijing),Beijing 102249,China;School of Water Conservancy,North China University of Water Resources and Electric Power,Zhengzhou 450046,China;CCDCDrilling and Production Technology Research Institute,Guanghan 618300,Sichuan,China)
Abstract:Acid fracturing is a common method for stimulating carbonate reservoir.The surface characteristics of acid-etched fracture is unique due to the non-uniform acid-etching.At present,the research on geometric feature of fracture surface before and after etching is not enough.In this paper,advanced experimental devices were used to obtain real acid-etched fracture samples,then the geometric characteristics of the fracture surface were analyzed by using 3D scanning data,and the new parameters hn andεh were defined to quantitatively describe the fluctuation degree.Furthermore,the change of fracture surface patterns before and after acid-etching were compared.The results show that gullies and holes were formed on the fracture surface and the fluctuation degree increased,the tortuosity decreased along the flow direction and increased vertically to flow direction after acid-etching.
Keywords:
本文献已被 CNKI 维普 等数据库收录!
点击此处可从《岩性油气藏》浏览原始摘要信息
点击此处可从《岩性油气藏》下载全文