晋45断块高温油井腐蚀化学治理技术
引用本文:杜清珍,孙玉民,李翠琴,魏爱军,杨梅红,杨俊怀.晋45断块高温油井腐蚀化学治理技术[J].石油钻采工艺,2012,34(5):98-101.
作者姓名:杜清珍  孙玉民  李翠琴  魏爱军  杨梅红  杨俊怀
作者单位:1.华北油田公司采油工程研究院,河北任丘?062552
摘    要:针对晋45断块高温油井腐蚀严重影响油田正常生产问题,在明确油井腐蚀原因基础上,通过正交实验有针对性地研制出了以咪唑啉衍生物、有机胺等组分为主,辅以耐高温氟碳咪唑啉组分的YHZ系列缓蚀剂,其缓蚀性能良好,平均缓蚀率达90%,解决了高温油藏(大于100 ℃)油井井筒腐蚀问题,经现场应用取得了较好效果。

关 键 词:晋45断块    油井腐蚀    绿色缓蚀
收稿时间:2019-05-22

Research and application of chemical control technology for high temperature well corrosion in Fault-block Jin45
DU Qingzhen , SUN Yumin , LI Cuiqin , WEI Aijun , YANG Meihong , YANG Junhuai.Research and application of chemical control technology for high temperature well corrosion in Fault-block Jin45[J].Oil Drilling & Production Technology,2012,34(5):98-101.
Authors:DU Qingzhen  SUN Yumin  LI Cuiqin  WEI Aijun  YANG Meihong  YANG Junhuai
Affiliation:1.Production Technology Research Institute, Huabei Oilfield Company, Renqiu 062552, China2.No.5 Oil Production Plant,Huabei Oilfield Company, Xinji 052300, China3.Environment Monitoring Center, Huabei Oilfield Company, Renqiu 062552, China4.Operation Area, Erlian Branch Company, Huabei Oilfield Company, Xilin Hot 026017, China
Abstract:Regarding the problem of high temperature well corrosion serious influencing the normal production in oilfields, figuring out the reason to well corrosion, an YHZ series corrosion inhibitor was developed through orthogonal experiment. The formula is mainly the imidazoline derivatives and organic amine group, supplemented by high temperature resistant fluorocarbon imidazoline group. This agent shows good corrosion inhibition performance with average corrosion inhibition rate of 90 percent, which solve the problem of well corrosion in reservoirs with high temperature (higher than 100 degree). Field application has achieved obvious effect and has shown a longer maintenance period of pumping wells.