摘    要:以新疆燃煤电站典型粉煤灰为研究对象,应用不同烧结剂与粉煤灰分别混合高温煅烧,通过盐酸和硫酸浸出锂,研究了烧结剂种类、煅烧温度、烧结剂添加量、浸出剂种类对锂浸出的影响。另外本文将微波技术应用于锂的浸出,对比研究了微波加热及传统水浴加热对锂浸出的效果。结果表明:碳酸钾、碳酸钠、乙酸钠、氯化钠作为烧结剂活化粉煤灰使锂的浸出效果较好;对于碳酸钠和碳酸氢钠等浸出效果较好的烧结剂,800℃较适宜作为其煅烧温度;盐酸比硫酸溶液更适合作为浸出剂浸出粉煤灰中的锂;微波加热对锂浸出有非常大的优势,微波4min比水浴4h 锂浸出量增加了55%;碳酸钠与碳酸钾混合烧结剂比单一烧结剂表现出更好的活化性能,应用30%碳酸钠和70%碳酸钾混合烧结剂煅烧活化粉煤灰后使灰中锂的浸出率达93%。

关 键 词:粉煤灰    烧结剂  微波  固废回收
收稿时间:2018-05-16

The effect of activator on lithium extraction from Xinjiang fly ash
Hui DONG,Juan CHEN,Xiaoyu LI,Li SHAO. The effect of activator on lithium extraction from Xinjiang fly ash[J]. Chemical Industry and Engineering Progress, 2019, 38(3): 1538-1544. DOI: 10.16085/j.issn.1000-6613.2018-1020
Authors:Hui DONG  Juan CHEN  Xiaoyu LI  Li SHAO
Affiliation:School of Energy and Power Engineering, Shandong University, Jinan 250061, Shandong, China
Abstract:The extraction of lithium from a typical Xinjiang fly ash was studied in this paper. Five kinds of activators including carbonate, acetate, bicarbonate, chloride and sulfate were mixed with the fly ash for calcination and activation. The effects of calcination temperature, addition percent of activator and leaching agent on lithium extraction were investigated. Moreover, microwave heating was used on lithium extraction in this paper. The comparison between microwave and traditional water bath heating on Li extraction was discussed. The results show that potassium carbonate, sodium carbonate, sodium acetate, or sodium chloride as activator exhibited high abilities for lithium extraction. For most activators with good leaching effect, 800℃ is suitable as the calcination temperature. Hydrochloric acid was better than sulfuric acid as a leaching agent for lithium extraction from coal-ash. It was found that microwave increased lithium extraction by 55% compared to water bath heating. The mixed activator of Na2CO3 and K2CO3 showed better activation performance than either as a single activator. The extraction ratio of Li in ash reached 93% by using a 30% Na2CO3 and 70% K2CO3 mixture as the activator.
Keywords:coal-fired ash  lithium  activator  microwave  solid waste recycling  
本文献已被 CNKI 万方数据 等数据库收录!
点击此处可从《化工进展》浏览原始摘要信息
点击此处可从《化工进展》下载免费的PDF全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号