1.
《Polymer Composites》2017,38(8):1749-1755
Wood flour (WF)‐filled composites based on a polypropylene (PP)/recycled polyethylene terephthalate (r‐PET) matrix were prepared using two‐step extrusion. Maleic anhydride grafted polypropylene (MAPP) was added to improve the compatibility between polymer matrices and WF. The effects of filler and MAPP compatibilization on the water absorption, mechanical properties, and morphological features of PP/r‐PET/WF composites were investigated. The addition of MAPP significantly improved mechanical properties such as tensile strength, flexural strength, tensile modulus, and flexural modulus compared with uncompatibilized composites, but decreased elongation at break. Scanning electron microscopic images of fracture surface specimens revealed better interfacial interaction between WF and polymer matrix for MAPP‐compatibilized PP/r‐PET/WF composites. MAPP‐compatibilized PP/r‐PET/WF composites also showed reduced water absorption due to improved interfacial bonding, which limited the amount of absorbable water molecules. These results indicated that MAPP acts as an effective compatibilizer in PP/r‐PET/WF composites. POLYM. COMPOS., 38:1749–1755, 2017. © 2015 Society of Plastics Engineers  相似文献   

2.
BACKGROUND: Renewable resources and recyclable thermoplastic polymers provide an attractive eco‐friendly quality as well as environmental sustainability to the resulting natural fibre‐reinforced composites. The properties of polypropylene (PP)‐based composites reinforced with rice hulls or kenaf fibres were investigated with respect to their recyclability. Rice hulls from rice processing plants and natural lignocellulosic kenaf fibres from the bast of the plant Hibiscus cannabinus represent renewable sources that could be utilized for composites. Maleic anhydride‐grafted PP was used as a coupling agent to improve the interfacial adhesion between fillers and matrix. Composites containing 30 wt% reinforcement were manufactured by melt mixing and their mechanical and thermal properties were determined. The composites were then pelletized and reprocessed by melt mixing. Finally, structure/properties relationships were investigated as a function of the number of reprocessing cycles. RESULTS: It is found that the recycling processes do not induce very significant changes in flexural strength and thermal stability of the composites. In particular PP‐based composites reinforced with kenaf fibres are less sensitive to reprocessing cycles with respect to PP‐based composites reinforced with rice hulls. CONCLUSION: The response of PP‐based composites reinforced with rice hulls or kenaf fibres is promising since their properties remain almost unchanged after recycling processes. Moreover, the recycled composites are suitable for applications as construction materials for indoor applications. In fact, the flexural strength and modulus of these materials are comparable to those of conventional formaldehyde wood medium‐density fibreboards. Copyright © 2008 Society of Chemical Industry  相似文献   

3.
Polypropylene (PP) composites filled with wood flour (WF) were prepared with a twin‐screw extruder and an injection‐molding machine. Three types of ecologically friendly flame retardants (FRs) based on ammonium polyphosphate were used to improve the FR properties of the composites. The flame retardancy of the PP/WF composites was characterized with thermogravimetric analysis (TGA), vertical burn testing (UL94‐V), and limiting oxygen index (LOI) measurements. The TGA data showed that all three types of FRs could enhance the thermal stability of the PP/WF/FR systems at high temperatures and effectively increase the char residue formation. The FRs could effectively reduce the flammability of the PP/WF/FR composites by achieving V‐0 UL94‐V classification. The increased LOI also showed that the flammability of the PP/WF/FR composites was reduced with the addition of FRs. The mechanical property study revealed that, with the incorporation of FRs, the tensile strength and flexural strength were decreased, but the tensile and flexural moduli were increased in all cases. The presence of maleic anhydride grafted polypropylene (MAPP) resulted in an improvement of the filler–matrix bonding between the WF/intumescent FR and PP, and this consequently enhanced the overall mechanical properties of the composites. Morphological studies carried out with scanning electron microscopy revealed clear evidence that the adhesion at the interfacial region was enhanced with the addition of MAPP to the PP/WF/FR composites. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010  相似文献   

4.
In this study, the main focus was on the effect of wood fiber (WF) content and particle size on the morphology and mechanical, thermal, and water‐absorption properties of uncompatibilized and ethylene glycidyl methacrylate copolymer (EGMA) compatibilized ethylene vinyl acetate copolymer–WF composites. For uncompatibilized composites, the tensile strength decreased with increasing WF content, whereas for compatibilized composites, the tensile strength initially decreased, but it increased for composites containing more than 5% WF. Small‐WF‐particle‐containing composites had higher tensile strengths than composites containing larger WF particles, both in the presence and absence of EGMA. WF particle size did not seem to have much influence on the degradation behavior of the composites, whereas water absorption by the composites seemed to be higher in composites with smaller particle sizes for both compatibilized and uncompatibilized composites. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 103: 3645–3654, 2007  相似文献   

5.
Montmorillonite is a promising substitute for aluminum trihydroxide in flame‐retardant polypropylene/aluminum trihydroxide (PP/ATH) composites. Study was made of the partial substitution of organoclay for ATH in PP/ATH composites. The total concentration of filler was kept at 30 wt%. The composites were compatibilized with two types of compatibilizer: commercial maleic anhydride functionalized polypropylene (PP‐g‐MA) and hydroxyl‐functionalized polypropylene (PP‐co‐OH) prepared with metallocene catalyst. The effect of compatibilization on the morphology was studied by the transmission electron microscopy and the scanning electron microscopy. Mechanical properties were characterized by tensile and impact measurements, and flammability properties with a cone calorimeter. Addition of compatibilizer and stearic acid (SA) treatment of the ATH particles contributed to the dispersion of the fillers. Both compatibilizers produced organoclay with exfoliated structure and improved adhesion between the fillers and the matrix. Toughness improved and decomposition and flammability were reduced. POLYM. ENG. SCI. 45:1568–1575, 2005. © 2005 Society of Plastics Engineers  相似文献   

6.
The scope of the article was to study the perspectives of the using of wood derived fillers (WDF) from waste of different origin as fillers of polypropylene. The WDF used in this study was hard wood flour (HW), birch veneer polishing dust (VD) and tetra‐pack carton cellulose fiber (TC). Some mechanical strength parameters, water uptake in the static and cyclic test and resistance to fungal decay of polypropylene (PP) composites containing these three types of WDF were studied and compared with similar loading (40 wt %) talc‐filled PP. Composites containing TC and VD fibers as filler showed the highest flexural strength at three test temperatures (?40, +20, and +40°C) and flexural modulus and tensile strength at plus temperatures. On the other hand talc‐filled PP exhibited greatest flexural modulus at minus temperature, greatest impact strength at room temperature and best flow ability. Significant difference was observed between PP composites with HW and VD fillers regarding water uptake in cyclic tests, however flexural strength and modulus change of composites were reversible after drying. No weight loss of WDF/PP composites was observed after 6 week exposure to brown‐ and white‐rot fungi, however, degradation of the surface of samples was detected by SEM. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010  相似文献   

7.
Polypropylene (PP) hybrid composites have been produced by compounding two types of mineral fillers, viz., talc and kaolin with PP copolymer using a twin screw extruder. The PP hybrid composite was injection‐molded into dumbbell specimen for tensile, flexural, and impact properties characterizations. MFI and SEM studies were used to characterize the flow and morphological properties of the PP hybrid composites. The result shows that most of the hybrid composites showed a significant decrease in flow, tensile, flexural, and impact properties compared with the single filler‐filled PP composites. However, a hybridization effect was seen for the PPT20K10 hybrid composites, through the synergistic coalescence of positive characteristics from 20 wt % of talc and 10 wt % of kaolin. This hybrid formulation have given an economically advantageous material with the mechanical properties (tensile, flexural, and impact) comparable to those of the talc‐filled PP composites. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci 104: 434–441, 2007  相似文献   

8.
9.
In this article, a solid‐state mechanochemical method based on a pan‐mill equipment was used to prepare 60 wt % loading of wood flour (WF) incorporated polypropylene (PP) wood–plastic composite (WPC) with good comprehensive performance. The particle size distribution, crystallization, microstructure, and properties of the prepared WPC were accordingly investigated. The results show that under co‐effects of the strong shear force field of pan milling and the compatibilization of PP grafted maleic anhydride (PP‐g‐MAH), the mixture of PP and WF is effectively pulverized and homogeneously mixed. Meanwhile, the WF particles are adequately activated by exposure of their characteristic functional groups, which is beneficial to the interfacial mechanochemical reaction. PP‐g‐MAH and PP prove to be in situ grafted onto WF particles surface during pan milling, thus resulting in the substantial enhancement in both the dispersion of the added WF fillers in PP matrix and the interfacial bonding. The mechanochemical effects of pan milling could also remarkably promote the heterogeneous nucleation effect of WF particles on PP crystallization and influence the dynamic mechanical behavior of composite. Compared with the unmilled and uncompatibilized composite, the milled and compatibilized WPC material possesses greatly enhanced mechanical performance and shows good application prospects. © 2015 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2016 , 133, 43108.  相似文献   

10.
The recycling of construction materials has been the subject of much research in past years. In this study, the use of construction and demolition wastes (CDWs) as mineral fillers in hybrid wood–polymer composites was studied. Two types of waste materials were used as fillers in the composites: (1) a mixture consisting of waste mineral wool (MW) and plasterboard (PB) and (2) mixed CDWs. The performance of the composites was evaluated from their mechanical properties and water‐absorption behavior. We found in the study that the addition of mineral fillers decreased the flexural strength and modulus values of the wood–polypropylene (PP) composites. On the other hand, the exchange of part of the wood with a mineral filler resulted in an increase in the impact strength of the composite. The composite manufactured with the combination of MW and PB had the lowest water absorption. The decrease in wood loading resulted in improved dimensional stability in the hybrid wood–mineral filler–PP composites. © 2016 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2016 , 133, 43412.  相似文献   

11.
The investigation of the economical use of lignocellulose waste, which is one of the environmental problems facing nations, is ongoing. In this study, waste cardboard paper fiber reinforcing polypropylene (PP) composites was developed. In order to modify the PP matrix maleated PP (MA‐g‐PP) a 5 wt% and a grafting rate of 1 and 2 wt% was used as a compatibilizer. The effects of fiber and compatibilizer content as well as graft content are evaluated by mechanical, thermal property measurements, and scanning electron microscopy (SEM). The compatibilizer improved all mechanical properties significantly. Thus, the tensile strength of MA‐g‐PP‐containing composites increases compared to PP/cardboard composites paper content increases. However, the tensile modulus of a PP‐based composite increases with an increase in paper fiber with the compatibilizer having little effect. SEM revealed that the addition of MA‐g‐PP generates strong interactions between a PP matrix and paper fibers. However, the addition of the MA‐g‐PP compatibilizing agent gives a significant improvement on the crystallization of the composites, whereas the compatibilized PP/old corrugated cardboard (OCC) composites have higher crystallinity (Xc) than uncompatibilized PP/OCC composites. The MA‐g‐PP also diminished the water absorption in the composites. J. VINYL ADDIT. TECHNOL., 22:231–238, 2016. © 2014 Society of Plastics Engineers  相似文献   

12.
In this article, the influence of ammonium polyphosphate (APP) and ammonium polyphosphate modified with 3‐(Methylacryloxyl) propyltrimethoxy silane (M‐APP) on mechanical properties, flame retardancy, and thermal degradation of wood flour–polypropylene composites (WF/PP composites) have been investigated. Polypropylene grafted with m‐isopropenyl‐α,α‐dimethylbenzyl‐isocyanate (m‐TMI‐g‐PP) was used to improve the adhesion of WF/PP composites. APP and M‐APP were used as flame retardants. The experimental results demonstrated that addition of M‐APP obviously enhanced mechanical properties of WF/PP composites. According to cone calorimetry results, M‐APP is also an effective flame retardant for WF/PP composites, compared to that of APP. It was also found that M‐APP decreased the 1% weight loss temperature and increased char residue. The thermal degradation of wood flour based upon the first peak temperature of wood decreased from 329.3 to 322.9°C and the thermal degradation of PP based upon the second peak temperature of PP improve from 518.0 to 519.6°C, when M‐APP was added to the WF/PP composites. From SEM results the char layer of the 25% M‐APP systems is much more intumescent than that of the 25% APP systems, indicating that 3‐(Methylacryloxyl) propyltrimethoxy silane can improve the char‐forming ability of WF/PP composites. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2011  相似文献   

13.
In this research, the reinforcing effect of fillers including canola stalk, paulownia and nanoclay, in polypropylene (PP) has been investigated. In the sample preparation, 50 wt% of lignocellulosic materials and 0, 3, and 5 wt% of nanoclay particles were used. The results showed that while flexural and tensile properties were moderately enhanced by the addition of nanoclay in the matrix, notched Izod impact strengths decreased dramatically. However, with increase in the nanoclay content (5 wt%), the flexural and tensile properties decreased considerably. The mechanical properties of composites filled with paulownia are generally greater than canola stalk composites, due to the higher aspect ratio. The thickness swelling and water absorption of the composites significantly decreased with the increase in nanoclay loading. Except tensile modulus, the differences between the type of fibrous materials and nanoclay contents had significant influence on physicomechanical properties. Morphologies of the composites were analyzed using transmission electron microscopy (TEM) and X‐ray diffraction (XRD), and the results showed increased d‐spacing of clay layers indicating enhanced compatibility among PP, clay, and lignocellulosic material. TEM micrographs also confirmed that the composites containing 3 wt% nanoclay had uniform dispersion and distribution of clay layers in the polymer matrix. © 2012 Wiley Periodicals, Inc. J. Appl. Polym. Sci., 2013  相似文献   

14.
《Polymer Composites》2017,38(6):1194-1205
Two staining methods of wood flour/polypropylene composites in an attempt to improve the color stability of wood‐plastic composites (WPCs) were investigated. The first was to dye wood flour (WF) before compounding with polypropylene (PP) to make stained composites. The second method involved mixing pigments directly with WF and PP. Nine groups of composites were weathered in a QUV accelerated weathering tester for 960 h. Their surface color, surface gloss, washing resistance, and flexural properties were tested during weathering. Additionally, the weathered surface was characterized by SEM and ATR‐FTIR. The results revealed that (1) the washing resistance of composites were improved after staining treatments; (2) composites made of dyed WF showed higher surface gloss values and less cracks on weathered surface at the early stage of weathering; while composites containing pigments displayed brighter color, less color change, and less loss of flexural properties during weathering; and (3) weathering resulted in the protrusion of WF and photodegraded lignin on exposed surface. Adding pigments was proven to be more effective staining method for improving composite color stability during weathering. POLYM. COMPOS., 38:1194–1205, 2017. © 2015 Society of Plastics Engineers  相似文献   

15.
A natural fiber hybrid composite containing equal proportions of kenaf fibers (KFs) and wood flour (WF) as the reinforcements and polypropylene (PP) as the polymer matrix was prepared, and its static and dynamic mechanical properties were compared with KF/PP and WF/PP composites. Static tensile and flexural tests and dynamic mechanical analysis (DMA) were carried out. The hybrid composite exhibited tensile and flexural moduli and strength values closer to those of the KF composite, which indicated a higher reinforcing efficiency of KFs compared with WF. DMA revealed that although the glass‐transition temperature remained unchanged by the replacement of half of the WF by KFs, the α‐transition temperature of the hybrid composite was identical to that of WF composite. The magnitudes of both the α and β (glass) transitions of the hybrid composite were comparable to that of the WF/PP composite. © 2005 Wiley Periodicals, Inc. J Appl Polym Sci 98: 665–672, 2005  相似文献   

16.
The main aim of this work was to study and compare the mechanical and thermal properties of hybrid polypropylene (PP) composites and single‐filler PP composites. With two main types of mineral fillers—calcium carbonate (CaCO3) and talc—PP composites of different filler weight ratios (talc/CaCO3) were compounded with a twin‐screw extruder and then injection‐molded into dumbbell specimens with an injection‐molding machine. Tensile, flexural, and impact tests were performed to determine and compare the mechanical properties of the hybrid and single‐filler PP composites. A synergistic hybridization effect was successfully achieved; the flexural strength and impact strength were highest among the hybrids when the PP/talc/CaCO3 weight ratio was 70:15:15. The nucleating ability of the fillers and its effects on the mechanical properties were also studied with differential scanning calorimetry. Because of the influence of talc as the main nucleating agent, the hybrid fillers showed significant improvements in terms of the nucleating ability, and this contributed to the increase in or retention of the mechanical properties of the hybrid composites. © 2004 Wiley Periodicals, Inc. J Appl Polym Sci 91: 3327–3336, 2004  相似文献   

17.
《Polymer Composites》2017,38(7):1231-1240
The main objective of this research is to study the effect of recycled low density polyethylene (r‐LDPE) matrix on the tensile, impact, and flexural properties of the novel textile waste cotton fiber reinforced (T‐FRP) composites. For this purpose, the T‐FRP composites were manufactured by using two different matrix types; namely, virgin LPDE (v‐LDPE) and r‐LDPE, with different waste cotton fiber content. All composites were compatibilized by maleic anhydride‐LDPE (MA‐LDPE) in order to increase the interfacial adhesion between fibers and matrices. Differential scanning calorimetry, Fourier transform infrared spectroscopy, scanning electron microscopy, dynamic mechanical analyzer studies were performed in order to characterize the materials. The results have shown that best tensile and flexural properties have been obtained from the composites with the content of 30 wt% cotton fiber, 5 wt% maleic anhydride‐LDPE, and 65 wt% recycled LDPE matrix. However, the impact properties of the composites were decreased drastically compared to the pure LDPE matrix. POLYM. COMPOS., 38:1231–1240, 2017. © 2015 Society of Plastics Engineers  相似文献   

18.
The mechanical, morphological behavior and water absorption characteristics of polypropylene (PP) and silica, or PP and rice‐husk, composites have been studied. The silica used in this study as filler was a commercial type produced from soluble glass or rice husks. The compatibilizing effect of PP grafted with monomethyl itaconate (PP‐g‐MMI) and/or with vinyltriethoxysilane (PP‐g‐VTES) as polar monomers on the mechanical properties and water absorption was also investigated. In general, a high loading of the studied fillers in the polymer matrix increases the stiffness and the water absorption capacity. This effect is more noticeable in the tensile modulus of the PP/silica composite with PP‐g‐VTES as compatibilizer. However, the increase of the rice‐husk charge as a natural filler in the PP matrix decreases the stiffness, and in the presence of PP‐g‐MMI as compatibilizer in PP/rice‐husk, the tensile modulus and water absorption of the composite were improved. The better adhesion and phase continuity in the PP/silica and PP/rice‐husk composites with different compatibilizers was confirmed by the morphological study. Copyright © 2004 Society of Chemical Industry  相似文献   

19.
This work focused on two difficulties associated with preparation of polypropylene/wood flour (PP/WF) composites, viz. the compatibility of PP with WF and processing of the composites with high melt viscosity. Maleic anhydride‐grafted polypropylene (MAPP) was used in the preparation of PP composites to provide the compatibility between polymer and filler. Hyperbranched polyester (HBPE) was incorporated to check feasibility of it as a processing aid in the same. The PP/WF composites were formulated by melt compounding on a Brabender Plastograph EC. Blending effect of compatibilizer and processing aid HBPE on PP/WF biocomposites have been carried out on the basis of torque analysis, mechanical properties, morphology, and thermal stability. The investigation showed that HBPE improves the processibility of PP/WF composites than MAPP with respective to torque value. The mechanical and thermal properties slightly vary with change in relative proportion of MAPP and HBPE. J. VINYL ADDIT. TECHNOL., 24:179–184, 2018. © 2016 Society of Plastics Engineers  相似文献   

20.
The aim of this study is to investigate the effect of surface free energy of wood flour (WF) and silanized WF on the mechanical properties and interface of wood/polypropylene (PP) composites. The contact angles of three probe liquids against unmodified and modified spruce WF were tested by capillary rise method based on the Washburn equation. Then the surface free energy and its corresponding dispersion and polar components were calculated according to the method developed by Owens–Wendt–Kaelble. The tensile strength and flexural strength of the wood/PP composite samples made with unmodified and modified WF were tested and the flexural fracture surfaces were analyzed by scanning electron microscopy (SEM). The results showed that the surface free energy of WF increased from 26.0 to 36.1?mJ/m2, which was higher than that of PP (29.4?mJ/m2), and its corresponding polar component decreased from 13.1 to 4.4?mJ/m2, and the dispersion component increased from 12.9 to 31.7?mJ/m2 after the modification with 4 wt.% vinyltriethoxy silane, which makes it possible for spreading of PP on the surface of WF, the tensile strength and flexural strength of wood/PP composites made with modified WF were obviously improved. In addition, the improved compatibility between WF and PP was well confirmed by SEM.  相似文献   