ICP—AES法测定合金中的杂质元素   总被引:5,自引:0,他引:5  
刘继升 《贵金属》1998,19(3):46-50
研究了Au-Ni(Y,Gd),Au-Cu,Au-Ni-Cu,Au-Cu-Ni-Zn(Mn)合金中的杂质元素(Pb,Sb,Bi,As,Sn,Fe,Al,Zr,Be,V,Ti,In)用Y作载体的共沉淀分离富集方法,富集物转成盐酸液后用ICP-AES法测定,试液中共存元素间的干扰用等效浓度法校正,取试样1.25克时分析范围0.0004%~0.20%,RSD一般不超出±10%。  相似文献   

2.
ICP-AES法测定金合金中的杂质元素   总被引:1,自引:0,他引:1  
研究了Au-Ni((Y、Gd)、Au-Cu、Au-Ni-Cu、Au-Cu-Ni-Zn(Mn)合金中的杂质元素(Pb、Sb、Bi、As、Sn、Fe、Al、Zr、Be、V、Ti、In)用Y作载体的共沉淀分离富集方法。富集物转成盐酸溶液后用ICP-AES法测定,试液中共存元素间的干扰用等效浓度法校正。取试样125克时分析范围00004%~020%。RSD一般不超出±10%。  相似文献   

3.
溴化碲分光光度法测定钛铝合金中微量碲   总被引:5,自引:0,他引:5  
溴化碲分光光度法应用于钛铝合金中微量碲的测定,取得了良好的效果。干扰试验表明,在所选定条件下,Zn,Mn,Mg,Pb,Mo,As,Y,Sn,Nb,Sb,P,Co,Ni,Ca,Si,Cd,Bi,Ce,Zr,W,V各1mg,Cu,Cr各0.1mgFe为0.2mg,对100μgTe的测定基本无干扰,TiAl基体的轻微干扰可以用同量的TiAl作参比而消除。分别对含Te0.100%和0.020%的两组合成试  相似文献   

4.
THERMODYNAMICSOFCu-Ce-M(M=Sn,Zn,Pb)LIQUIDSOLUTIONSDu,Ting;Li,Guodong(CentralIronandSteelResearchInstituteMinistryofMetallurgi...  相似文献   

5.
THERMODYNAMICSOFCu-Y-M(M=Al,Si,Ti,Fe)LIQUIDSOLUTIONS¥Du,Ting;Li,Guodong(CentralIronandSteelResearchInstitute,Beijing100081)Ab...  相似文献   

6.
用中子衍射分析法研究了Cr,Mo,Ti,Ni,Mn,Si等代位合金元素当量成分,DO3结构Fe3Al金属间化合物亚点阵中的原子占位及其对单胞中Fe原子磁矩,DO3-B2转变行为的影响。  相似文献   

7.
Mn—Fe熔体的脱Si过程及Mn—Fe熔体氧位研究   总被引:2,自引:0,他引:2  
通过实验(1350℃ )测定 Mn-MnO2平衡体系 Mn液氧位,验证了 ZrO2(MgO)固体电解质定氧探头可用于测定 Mn-Fe熔体和锰液氧位.电动势-氧位换算关系式为 ln po2-31.56-(69548.8+46427.7×E)/T.使用 BaCO370%-MnO25%-(Fe2O3+BaF2)25%(质量分数)的熔剂对高炉 Mn-Fe脱 Si时,与最高脱 Si率(75%)对应的 Fe2O3含量是12%; Mn-Fe熔体中氧位和 C的活度关系式为 po2× 1012=35.812-0.106×ac; Mn-Fe熔体中氧位和 Mn损( [Mn])关系为po2×1012=6.238+0.679× [Mn].使用 BaCO360%-BaF210%-MnO215%-Fe2O315%熔剂对高炉 Mn-Fe脱Si时, 最高脱 Si率(88.9%)和最高氧位(8.31×10-12 Pa)对应的脱 Si时间为 15 min.脱 Si实验结果表明:脱 Si过程中Mn-Fe熔体的氧位是由熔体中碳氧反应控制的;脱 Si保 Mn的最高氧位是 6.238×10-12 Pa.  相似文献   

8.
航空结构用高纯高韧性铝合金的进展(2)   总被引:5,自引:0,他引:5  
张君尧 《轻金属》1994,(8):59-63
航空结构用高纯高韧性铝合金的进展(2)张君尧(东北轻合金加工厂黑龙江哈尔滨市150060)27XXX系高纯铝合金在AI—Zn—Mg—Cu系合金中,由于存在Fe、St杂质,可能生成(FeCrhsiAll。、(Fe,Mn,Cu)Ale、Cu。FeAI,和...  相似文献   

9.
生产电解二氧化锰用钛合金阳极的抗钝化性能   总被引:2,自引:0,他引:2  
研究了Ti-1.5Ni、Ti-0.5Fe、Ti-1.5Ni-0.5Cu、Ti-1.5Ni-0.5Fe-0.3Cu4种合金在95℃,40g/L H2SO4+80g/L MnSO4电解二氧化锰溶液中作阳极时的抗钝化性能。研究表明:以上4种合金都具有比TA2优异的抗钝化性能,TiNiFe的最为优异,在电流密度低于80A/m^2时,阳极表面不生成氧化膜,析出相Ti2Ni对提高抗钝化性起关键作用。TiNiF  相似文献   

10.
高强度锌铝合金摩擦磨损特性的试验研究   总被引:5,自引:1,他引:5  
采用MM200磨损试验机,测定和对比了铸造锌铝合金(ZZnAl27Cu2A和ZZnAl27Cu2D)和工业上常用铜合金(ZCuSn6Zn6Pb3,ZCuA110Fe3和ZCuZn33Mn2Pb2)的摩擦磨损特性。试验测定了合金在不同载荷和转速条件下的摩擦系数和磨损量及其对配对材料的磨损,结果表明,锌铝合金是一种更适于在重载低速条件下使用的减摩材料  相似文献   

11.
采用热力学研究方法 ,计算分析了稀土元素Ce与Ag -Cu -Zn系钎料合金中杂质元素Pb、Bi的活度系数与Ce、Pb、Bi浓度的关系。热力学计算表明 ,在以Ce、Pb或Bi为溶质 ,Ag、Cu或Zn为溶剂的金属熔体中 ,溶质元素的活度系数在Ce的某一浓度范围内出现“等活度系数”现象 ,此时溶质元素的活度系数与溶质元素的浓度无关 ,这一新的发现表明 ,热力学研究结果与金属学研究结果完全吻合。  相似文献   

12.
周惦武  邵斌  刘金水  苏华  李冬珍  代德利  胡国良  吴正喜 《铸造》2012,61(8):908-912,916
探讨了大断面QT600-3球铁件电炉熔炼生产工艺的技术要点,检测了试生产条件下球铁单铸试块与本体试块的化学成分、金相组织与力学性能,基于石墨结晶核心和石墨形态的分析,探讨了石墨畸变机理。生产试验结果表明:炉外增Si预处理增加铁液成核,轻、重稀土混合使用作为球化剂,侧重后期孕育,适当降低浇注温度,合理使用Cu元素,是电炉熔炼工艺生产大断面球铁件的重要环节;采用电炉熔炼工艺生产大断面球铁件,球化等级与化学成分稳定控制有关,抗拉强度、伸长率等力学性能与化学成分、基体组织有关;Y在铁液中形成高熔点Y2O3作为石墨析出的核心,可获得良好石墨形态;大断面球铁件中,Ti、Cu元素的偏析和球化元素Mg或稀土(Y、La、Ce)的氧化,破坏了奥氏体壳的稳定性,是造成石墨畸变的主要原因。  相似文献   

13.
薛松柏  陈燕  吕晓春 《焊接学报》2005,26(4):45-47,80
采用周模型计算分析了Sn-Ce-Me(Me=Pb、Bi、zn、Sb、Ag、Cu、Cd)三元合金系中,Ce与Sn以及Ce与Me之间的活度相互作用系数。计算结果表明,不仅在Sn-Pb-Ce中,Ce存在“亲Sn”现象,在其它6个三元无铅钎料合金体系中,如Sn-Bi-Ce、Sn-Sb-Ce、Sn-zn-Ce、Sn-Cd-Ce、Sn-Ag-Ce、Sn-Cu-Ce,Ce也同样存在着“亲Sn”现象。其研究结果可为新型无铅钎料的研究提供理论分析依据。  相似文献   

14.
Development on research of advanced rare-earth aluminum alloy   总被引:9,自引:0,他引:9  
1 INTRODUCTIONTheeffectofrareearthandtransitionelementsonthealuminumalloyisevidentfortheirspecialelec tronicstructures ,andthishasattractedattentionsofmanyscientists .Inthepast ,theresearchontherareearthaluminumalloyswascarriedoutmainlyonthebasisofassignmentofthespecifictypeandstrategy ,especiallyinChina ,andexplorationsoftheapplica tionoftherareearths (richresourceinChina)inalu minumalloysweremostlyconcentratedontheeffectofmischmetalonsomecommercialaluminumalloys ,whichwasthecertainoffs…  相似文献   

15.
稀土元素和Ti对ZM5镁合金组织和性能的影响   总被引:1,自引:0,他引:1  
用金相显微镜、X射线衍射仪分析了添加稀土元素Y、Nd和钛中间合金的Mg-8.5Al-0.5Zn(ZM5)合金的组织和相组成,测试了合金的室温力学性能。结果表明,添加稀土元素Y、Nd的ZM5镁合金中出现了新的镁.稀土相MgY、Mg12Nd,而在同时添加稀土元素Y、Nd和钛中间合金的合金中,还出现了新相Ti2Mg3Al18;添加稀土元素Y、Nd的ZM5镁合金在拉伸性能、硬度以及组织都明显优于ZM5镁合金,而同时添加稀土元素和Ti合金的镁合金其性能又显著优于单独添加Y或Nd的合金。  相似文献   

16.
The degradation of a variety of alumina‐forming Fe20Cr5Al based alloys has been investigated at temperatures ranging from 1100°C to 1300°C for up to 4000 h (100 h/cycle) in different oxidising environments such as laboratory air, air + 10 vol% H2O, air + 60 vol% H2O and simulated automotive exhaust gas. Seven model alloys with controlled levels of impurities such as P, S and C and carefully controlled levels of additional elements (Y, Zr, Ti, Hf, Si, La, etc.) and two different commercial alloys (Aluchrom YHfAl and Kanthal APMT) were chosen for this study. The investigation showed that the model alloys containing La, Y + Si and Y with added C, and the commercial alloy APMT usually had the lowest initial oxidation growth rates, whereas model alloys containing Y plus Zr, and the commercial alloy YHfAl had the higher oxidation rates regardless of the different oxidising environments. Scale spallation was more prevalent in the case of alloys with low oxide growth rates but changing the levels of water vapour in the oxidising atmospheres had only a minor influence on the degree of spallation or the oxide morphology. The scales formed on the alloys containing La, Y + Si and high C spalled in an adhesive manner (at the scale/metal interface), whereas scales formed on alloys containing Y plus Hf, Zr or Ti cracked and spalled in a cohesive manner (within the scale). Inhomogeneities in the distribution of the alloying additions led to greater changes in the oxide morphologies than any difference in oxidising atmosphere, but the crystallographic textures of all the oxides were similar. This pilot study enabled us to rank the alloys according to their resistance to spallation and also to determine the influence of minor elements when added as tightly controlled single or multiple element additions. Some of these alloys were then used as mechanically weak PVD coatings on a strong (APMT) substrate, and further oxidation experiments confirmed that the coatings then oxidised in a similar way to the bulk alloys.  相似文献   

17.
为了控制Zr(-Ti)-Cu-Ni-Al非晶合金中的O含量,进而改善其玻璃形成能力和力学性能,本研究基于稀土元素与O的强相互作用,向合金中添加Y、Gd、La和Ce等元素。使用铜模浇铸制备非晶合金,利用DSC、XRD和TEM对其非晶形成能力和微观结构进行分析,通过压缩试验和SEM对其力学性能及断裂方式进行表征。结果表明:Y的添加对合金的非晶形成能力具有较大的提升,在相对较低真空的气氛下,可制备出直径10mm以上的块体非晶,抗压缩断裂强度达1950 MPa。  相似文献   

18.
采用基于密度泛函理论的第一性原理方法,计算Fe8Al8及(Fe7X)Al8(X=Pb,Sn,Ti,Cu,Mn,Si,Zn)超胞模型的弹性模量与电子结构,在分析合金化元素改善FeAl金属间化合物力学性质的基础上,选取降低脆性效果较好的Cu和最好的Pb,对1.2 mm厚DC56D+ZF镀锌钢和1.15 mm厚6016铝合金平板试件进行加入中间夹层Cu和Pb的激光搭接焊试验。结果表明:FeAl金属间化合物为脆性相,其电子结构根源在于Fe的sd态与Al的sp态存在电子轨道杂化,为明显的共价键特征;FeAl合金化后,脆性降低,相应脆性由低到高的顺序为(Fe7Pb)Al8、(Fe7Sn)Al8、(Fe7Ti)Al8、(Fe7Cu)Al8、(Fe7Mn)Al8、(Fe7Si)Al8、(Fe7Zn)Al8、Fe8Al8,Pb合金化降低脆性效果最好,激光搭接焊加入中间夹层Pb,钢侧母材与焊缝界面区由母材侧较大晶粒和焊缝的细小晶粒交错形成,熔池金属与母材铝之间没有明显的分界线,焊接接头界面熔合良好;与未加夹层相比,加入中间夹层Cu和Pb后,焊接接头力学性能提高,其中Pb的作用优于Cu的,试样断口均具有韧性断裂特征。  相似文献   

19.
稀土元素Ce和La合金化对AM60镁合金腐蚀行为的影响   总被引:3,自引:0,他引:3  
采用电子探针-能谱分析,场发射扫描电镜X射线衍射等方法研究了稀土元素Ce和La合金化对AM60镁合金结构和耐蚀性能的影响.结果表明,Ce和La的加入可在AM60镁合金中形成了富含稀土元素的γ相(MgAlRE);能有效抑制析氢,提高镁合金的耐蚀性能;改善镁合金在含Cl-溶液中的耐蚀性能;腐蚀产物膜的晶态主要成分为铝和锰的氧化物,并含有少量的稀土氧化物和氢氧化物.  相似文献   

20.
M.A. Dudek  N. Chawla 《Acta Materialia》2009,57(15):4588-4599
It has recently been documented that Pb-free solder alloys doped with trace amounts of rare earth (RE) elements show a very strong propensity to grow Sn whiskers. In this work, we have investigated the effect of the addition of 2 wt.% Ce, La or Y on the whiskering behavior of Sn–3.9Ag–0.7Cu. Hillock-type whiskers around particle peripheries were observed in water-quenched alloys with smaller RESn3 particles, while furnace-cooled alloys with larger RESn3 particles formed needle-like whiskers from within the particle. Phase separation between Sn and RE oxides occurred during oxidation of the RESn3 intermetallics. A focused ion beam serial sectioning approach was used to visualize the Sn whiskers and the oxide structure. We show that the driving force for whisker growth is related to the compressive stresses that develop in these particles during the oxidation of the RE intermetallic phases.  相似文献   

设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号