介绍一种新型环保水剂玻璃蒙砂粉的开发思路,对该蒙砂粉进行了研究,根据水利玻璃蒙砂粉蒙砂特点拟定了无废液排放的蒙砂工艺。 相似文献
2.
3.
《建筑玻璃与工业玻璃》2009,(3)
一种亚光玻璃表面油光效果处理的方法及其产品;亚光立体图案玻璃的生产方法;一种玻璃蒙砂机;绸缎玻璃的生产方法;玻璃蒙砂机械用的新型布料结构;蒙砂亮光工艺图案玻璃的生产工艺;平置法生产蒙砂玻璃的方法;一种玻璃丝印蒙砂膏的制备方法 相似文献
4.
5.
6.
7.
9.
10.
11.
12.
Short glass fibers were added to poly(vinyl chloride) (PVC)/wood flour composites as reinforcement agents. Unnotched and notched impact strength of PVC/wood flour/glass fiber hybrid composites could be increased significantly without losing flexural properties by adding type L glass fibers and over 40% of PVC. There was no such improvement when using type S glass fiber. The impact strength of hybrid composites increased along with the increment of the type L glass fiber content at a 50% PVC content. At high PVC contents, impact fracture surfaces were characterized by wood particle, glass fiber breakage and pullout, whereas interfacial debonding was the dominant fracture mode at higher filler concentrations. The significant improvement in impact strength of hybrid composites was attributed to the formation of the three‐dimensional network glass fiber architecture between type L glass fibers and wood flour. 相似文献
13.
石英玻璃相对于金属、晶体、陶瓷等大多数固体材料具有更小的机械振动能量损耗,是许多精密测量器件的首选材料。本文测试对比了四种类型(Ⅰ类、Ⅱ类、Ⅲ类和Ⅳ类)石英玻璃的振动能量损耗特性,从材料化学组分和结构缺陷方面分析了石英玻璃本征损耗的影响因素及作用机理。结果表明:Ⅰ类和Ⅱ类石英玻璃的本征损耗显著大于Ⅲ类和Ⅳ类石英玻璃,主要是由金属杂质含量高和气泡等级低造成的;羟基含量不是影响石英玻璃本征损耗的主要因素;表面损耗是石英玻璃器件振动能量损耗的主要来源之一,可以通过湿法刻蚀消除。 相似文献
14.
15.
16.
简要介绍了标准PVB中间膜挡风玻璃的结构和原理,重点介绍了一种首孚信^TM公司新开发的增强型隔音PVB中间膜挡风玻璃,分析、比较了两种挡风玻璃的声传递特性。因为柴油引擎发出的噪音大于汽油动力的引擎,所以本文通过在柴油车上测试隔音PVB中间膜挡风玻璃是否能和在汽油动力汽车上一样降低风噪和公路噪音,结果表明,增强型隔音PVB中间膜挡风玻璃隔音降噪效果好,且重量更轻,可满足汽车改善车内环境、节能的要求。 相似文献
17.
18.
19.
20.
《Journal of the European Ceramic Society》2014,34(11):2675-2685
In order to characterise the design strength of an innovative type of glass–ceramic with a view to structural applications, 4-point-bending and Ring-on-Ring biaxial bending tests have been performed. Strength is comparable with that of tempered glass but remarkably, the material breaks into large pieces like annealed glass. Interpreted through Weibull-type probability distributions, the data show much lower dispersion with respect to glass. Additional tests performed at different load rates have allowed an evaluation of the effects of static fatigue. Using a phenomenological model of equivalent-crack growth, a method is presented to calculate the decay of strength with loading time. As expected, this material is proven to be less sensitive than glass to this type of degradation. 相似文献