The Shubnikov–de Haas effect and the Hall effect in n-Bi2–xTlxSe3 (x = 0, 0.01, 0.02, 0.04) and p-Sb2–xTlxTe3 (x = 0, 0.005, 0.015, 0.05) single crystals are studied. The carrier mobilities and their changes upon Tl doping are calculated by the Fourier spectra of oscillations. It is found shown that Tl doping decreases the electron concentration in n-Bi2–xTlxSe3 and increases the electron mobility. In p-Sb2–xTlxTe3, both the hole concentration and mobility decrease upon Tl doping. The change in the crystal defect concentration, which leads to these effects, is discussed.  相似文献   

2.
Glass with compositions xK2O-(30 ? x)Li2O-10WO3-60B2O3 for 0 ≤ x ≤ 30 mol.% have been prepared using the normal melt quenching technique. The optical reflection and absorption spectra were recorded at room temperature in the wavelength range 300–800 nm. From the absorption edge studies, the values of the optical band gap (E opt) and Urbach energy (ΔE) have been evaluated. The values of E opt and ΔE vary non-linearly with composition parameter, showing the mixed alkali effect. The dispersion of the refractive index is discussed in terms of the single oscillator Wemple Di-Domenico model.  相似文献   

3.
(1???x)K0.5Na0.5NbO3-x(Bi0.5K0.5)ZrO3 [abbreviated as (1???x)KNN-xBKZ, 0?≤?x?≤?0.08] lead-free ceramics have been fabricated by a solid-state processing route. Based on the x-ray diffraction data and temperature-dependent dielectric characteristics, an orthorhombic phase for x?≤?0.03 and single rhombohedral one for x?≥?0.05 at room temperature were determined. The cell volume firstly increases, then decreases and finally increases with increasing BKZ, depending on ionic size and crystallographic structure. For the sample of x?=?0.05, a temperature-stable high permittivity (~?1736?±?15%) along with low dielectric loss tangent (≤?5%) is recorded from 158°C to 407°C. In addition, the activation energies of dielectric relaxation and dc conductivity at high temperatures were characterized by impedance spectroscopy. A combined effect of lattice distortion and oxygen vacancies on the magnitude of activation energies was discussed.  相似文献   

4.
Synthesis and also the structural and photoluminescence properties of nanocrystals with natural faceting of the “cesium–lead–halogen” system with crystalline structure of the perovskite type are examined. The possibility of continuously changing the position of the maximum in the photoluminescence spectrum in the wavelength range of 400–700 nm is demonstrated. Features of the formation of the continuous series of solid solutions CsPb(Cl1–x Br x )3 and CsPb(Br1–x I x )3 due to the aftergrowth treatment of CsPbBr3 nanocrystals as a result of anion exchange at room temperature are studied. The corresponding range of frequency change for the maximum of the photoluminescence spectrum amounts to 410–690 nm.  相似文献   

5.
The electrical properties in the temperature range 295–430 K and low-temperature (4.2 K) photoluminescence of Cd1?xZnxTe:Cl semi-insulating crystals grown from melts with a variable impurity content (C Cl 0 = 5 × 1017–1 × 1019 cm?3) are investigated. Nonequilibrium processes leading to a decrease in carrier concentration are observed in all the samples at low temperatures (T = 330–385 K). These changes are reversible. The activation energy of these processes E a is found to be 0.88 eV. As with semi-insulating CdTe:Cl, the observed phenomena can be explained by a change in the charge state of background copper atoms: CuCd ? Cui. The introduction of Zn changes the ratio of the concentrations of shallow-level donors Cui and ClTe from their levels in the initial material.  相似文献   

6.
Nd/Nb-co-substituted Bi3.15Nd0.85Ti3?x Nb x O12 (BNTN x , x = 0.01, 0.03, 0.05 and 0.07) thin films were grown on Pt/Ti/SiO2/Si (100) substrates by chemical solution deposition. The effects of Nb content on the micro-structural, dielectric, ferroelectric, leakage current and capacitive properties of the BNTN x thin films were investigated. A low-concentration substitution with Nb ions in BNTN x can greatly enhance its remanent polarization (2P r) and reduce the coercive field (2E c) compared with those of Bi4Ti3O12 (BIT) thin film. The highest 2P r (71.4 μC/cm2) was observed in the BNTN0.03 thin film when the 2E c was 202 kV/cm. Leakage currents of all the films were on the order of 10?6 to 10?5 A/cm2, and the BNTN0.03 thin film has a minimum leakage current (2.1 × 10?6 A/cm2) under the high electric field (267 kV/cm). Besides, the CV curve of the BNTN0.03 thin film is the most symmetrical, and the maximum tunability (21.0%) was also observed in this film. The BNTN0.03 thin film shows the largest dielectric constant and the lowest dielectric loss and its maximum Curie temperature is 410 ± 5°C.  相似文献   

7.
Sintered Bi0.5(Na0.8K0.2)0.5TiO3 + x wt.% ZnO nanoparticle (BNKT–xZnOn) ceramics have been fabricated by conventional annealing with the aid of ultrasound waves for preliminary milling. Because of the presence of the liquid Bi2O3–ZnO phase at the eutectic point of 738°C, the sintering temperature decreased from 1150°C to 1000°C, and the morphology phase boundary of BNKT–xZnOn ceramics can be clarified by two separated peaks at (002)T and (200)T of 2θ in the x-ray diffraction (XRD) patterns. The improvement of ferroelectric properties has been obtained for BNZT–0.2 wt.% ZnOn ceramics by the increase of remanent polarization up to 20.4 μC/cm2 and a decrease of electric coercive field down to 14.2 kV/cm. The piezoelectric parameters of the ceramic included a piezoelectric charge constant of d 31 = 78 pC/N; electromechanical coupling factors k p = 0.31 and k t = 0.34, larger than the values of 42 pC/N, 0.12 and 0.13, respectively, were obtained for the BNKT ceramics.  相似文献   

8.
Deposition of SiO x layers of variable composition onto silicon wafers was performed by co-sputtering of spaced Si and SiO2 targets in argon plasma. Coordinate dependences of the thickness and refractive index of separately deposited Si and SiO2 layers and the SiO x layer grown during co-sputtering of targets were determined using optical techniques. It was shown that the SiO x layer composition is not equal to a simple sum of thicknesses of separately deposited Si and SiO2 layers. The coordinate dependences of the Si and SiO2 layer thicknesses were calculated. To fit the calculated and experimental data, it is necessary to assume that no less than 10% of silicon is converted to dioxide during co-sputtering. A comparison of the coordinate dependences of the IR absorbance in SiO2 and SiO x layers with experimental ellipsometric data confirmed the presence of excess oxygen in the SiO x layer. Taking into account such partial oxidation of sputtered silicon, composition isolines in the substrate plane were calculated. After annealing of the SiO x layer at 1200°C, photoluminescence was observed in a wafer area predicted by calculations, which was caused by the formation of quantum-size Si nanocrystallites. The photoluminescence intensity was maximum at x = 1.78 ± 0.3, which is close to the composition optimum for ion-beam synthesis of nanocrystals.  相似文献   

9.
The results of investigations of electrical, optical, and photoelectric properties of CdIn2Te4 crystals, which were grown by the Bridgman method are presented. It is shown that electrical conductivity is determined mainly by electrons with the effective mass mn = 0.44m0 and the mobility 120–140 cm2/(V s), which weakly depends on temperature. CdIn2Te4 behaves as a partially compensated semiconductor with the donor-center ionization energy Ed = 0.38 eV and the compensation level K = Na/Nd = 0.36. The absorption-coefficient spectra at the energy < Eg = 1.27 eV are subject to the Urbach rule with a typical energy of 18–25 meV. The photoconductivity depends on the sample thickness. The diffusion length, the charge-carrier lifetime, and the surface-recombination rate are determined from the photoconductivity spectra.  相似文献   

10.
Surface-barrier diodes based on the CdxHg1?x Te alloy (x ~ 0.8) sensitive in the wavelength range 0.3–1.1 μm, which were obtained by etching (bombardment) of the surface of the p-type crystal with argon ions, are studied. Using the measured spectral absorption and reflection curves, as well as the parameters of the diode structure, which were found from electrical characteristics, the spectra of photoelectric quantum efficiency of diodes are calculated. The results of the calculation of photoelectric parameters of the Gd0.8Hg0.2Te-based diodes are given in comparison with the CdTe-based and Si-based solar cells. For the AM1.5 solar irradiation conditions, the open-circuit voltage and short-circuit current, as well as values of limiting efficiency, are determined.  相似文献   

11.
Using optical methods, data on optical constants are obtained for silicon nitride films synthesized by plasma-chemical vapor deposition (PCVD). Models for calculating the permittivity in the model of inhomogeneous phase mixture of silicon and silicon nitride are considered. It is found that the optical-absorption edge (E g) and the photoluminescence peak shift to longer wavelengths with increasing nitrogen atomic fraction x in sin x films. When x approaches the value 4/3 characteristic for stoichiometric silicon nitride Si3N4, a nonlinear sharp increase in E g is observed. Using Raman scattering, Si-Si bonds are revealed, which confirms the direct formation of silicon clusters during the film deposition. The relation between the composition of nonstoichiometric silicon nitride films, values of permittivity, and the optical-band width is established for light transmission.  相似文献   

12.
With a view to creating Si LEDs, the structural and luminescent properties of SiO x N y films containing Si nanocrystals in the SiO x N y matrix are studied experimentally. It is found that the film structure (nanocrystal size and concentration, the presence of an amorphous phase, etc.) and the spectrum and intensity of photoluminescence (PL) and electroluminescence (EL) are strongly dependent on the Si stoichiometric excess δ and annealing conditions. At δ≈ 10%, unannealed films are amorphous and contain Si clusters of size < 2 nm, as deduced from the TEM and microdiffraction data obtained. Annealing at 800–1000°C for 10–60 min produces Si crystals 3–5 nm in size with a concentration of ≈1018 cm?3. The annealed films exhibit room-temperature PL and EL over the wavelength range 400–850 nm with intensity peaks located at 50–60 and 60–70 nm, respectively. The PL and EL spectra are found to be qualitatively similar. This suggests that both the PL and the EL should be associated with the formation of luminescent centers at nanocrystal–matrix interfaces and in boundary regions. However, the two phenomena should differ in the mechanism by which the centers are excited. With the EL, excitation should occur by impact processes due to carrier heating in high electric fields. It is found that as δ increases, so does the proportion of large amorphous Si clusters with a high density of dangling bonds. This enhances nonradiative recombination and suppresses luminescence.  相似文献   

13.
TlCrS2 and TlCrSe2 crystals were synthesized by solid-state reaction. X-ray diffraction analysis showed that TlCrS2 and TlCrSe2 compounds crystallize in the hexagonal crystal system with lattice parameters a = 3.538 Å, c = 21.962 Å, c/a ≈ 6.207, z = 3; a = 3.6999 Å, c = 22.6901 Å, c/a ≈ 6.133, z = 3; and X-ray densities ρ x = 6.705 and 6.209 g/cm3, respectively. Magnetic and electric studies in a temperature range of 77–400 K showed that TlCrS2 and TlCrSe2 are semiconductor ferromagnets. Rather large deviations of the experimental effective magnetic moment of TlCrS2 (3.26 μB) and TlCrSe2 (3.05 μB) from the theoretical one (3.85 μB) are attributed to two-dimensional magnetic ordering in the paramagnetic region of strongly layered ferromagnets TlCrS2 and TlCrSe2. The effect of the magnetic phase’s transition on the charge transport in TlCrS2 and TlCrSe2 is detected.  相似文献   

14.
The photoluminescence and composition of amorphous As2Se3 films modified with an Er(thd)3 complex compound have been studied. A band centered at 1.54 μm, characteristic of photoluminescence from Er embedded in amorphous matrices, has been revealed at room temperature. The composition of thin amorphous As2Se3 films modified with an Er(thd)3 complex compound has been examined by methods of nuclear microanalysis: Rutherford backscattering and nuclear resonant reactions. Dependences of the concentrations of Er ions, oxygen, and carbon on the growth conditions of the films are obtained. It is shown that the Er concentration in a thin film varies nonlinearly as the relative concentration of the starting complex compound increases. In addition, the increase in the Er content of a film is accompanied by a simultaneous rise in the content of such light elements as oxygen and carbon. Comparative analysis of the nuclear microanalysis data and IR spectra demonstrates that, in modification of As2Se3 with the Er(thd)3 complex compound by the given method, the nearest environment of Er in the complex compound is partly preserved.  相似文献   

15.
The poorly known AgCd2GaS4 single-crystal compounds that crystallize in a rhombic structure (space group Pmn21) are studied. Deviations from the stoichiometric composition of the samples and random occupation of the cation sublattice sites by Ag and Ga ions result in violation of long-range order in the atomic arrangement and make the AgCd2GaS4 compounds structurally closer to disordered systems. In this case, it is found that the fundamental optical-absorption edge is smeared and shifted to longer wavelengths, and is adequately described by the Urbach rule. In addition, a broadening of the spectral peaks of photoconductivity and luminescence is observed. The concentration of charged point defects responsible for the smearing of the absorption edge is calculated. It is found to be 1.2×1020 cm?3. The AgCd2GaS4 single crystals are photosensitive semiconductors. From the position of the absorption edge, the optical band gap of the compound is estimated (E g0 = 2.28 eV at T = 297 K). The photoluminescence spectra of the AgCd2GaS4 single crystals are similar to the spectra of defect-containing CdS single crystals; for the AgCd2GaS4 crystals, the emission peaks are shifted to longer wavelengths with respect to the peaks for CdS crystals by Δλ = 0.06?0.1 μm. From the analysis of the experimental data, some conclusions on the nature of photoactive centers in AgCd2GaS4 compounds are drawn.  相似文献   

16.
The current–voltage (I–V) and photocurrent–light intensity (I pc –Φ) characteristics and the photoconductivity relaxation kinetics of TlInSe2 single crystals are investigated. Anomalously long relaxation times (τ ≈ 103 s) and some other specific features of the photoconductivity are observed, which are explained within the barrier theory of inhomogeneous semiconductors. The heights of the drift and recombination barriers are found to be, respectively, E dr ≈ 0.1 eV and E r ≈ 0.45 eV.  相似文献   

17.
In single crystals of copper-doped and undoped Bi2Te2.85Se0.15 solid solutions with an electron concentration close to 1 × 1019 cm?3, the temperature dependences are investigated for the Hall (R 123, R 321) and Seebeck (S 11) kinetic coefficients, the electrical-conductivity (σ 11), Nernst-Ettingshausen (Q 123), and thermalconductivity (k 11) coefficients in the temperature range of 77–400 K. The absence of noticeable anomalies in the temperature dependences of the kinetic coefficients makes it possible to use the one-band model when analyzing the experimental results. Within the framework of the one-band model, the effective mass of density of states (m d ≈ 0.8m 0), the energy gap (εg ≈ 0.2 eV), and the effective scattering parameter (r eff ≈ 0.2) are estimated. The obtained value of the parameter r eff is indicative of the mixed electron-scattering mechanism with the dominant scattering by acoustic phonons. Data on the thermal conductivity and the lattice resistivity obtained by subtracting the electron contribution according to the Wiedemann-Franz law are presented.  相似文献   

18.
A BiCu2PO6 microwave dielectric ceramic was prepared using a solid-state reaction method. As the sintering temperature increased from 800°C to 880°C, the bulk density of BiCu2PO6 ceramic increased from 6.299 g/cm3 to 6.366 g/cm3; the optimal temperature was 860°C. The best microwave dielectric properties [permittivity (? r ) = ~16, a quality factor (Q × f) = ~39,110 GHz and a temperature coefficient of resonant frequency (τ f ) = ~?59 ppm/°C] were obtained in the ceramic sintered at 860°C for 2 h. Then, TiO2 with a positive τ f (~+400 ppm/°C) was added to compensate the τ f value. The composite material was found to have a near-zero τ f (+2.7 ppm/°C) and desirable microwave properties (? r  = 19.9, Q × f = 24,885 GHz) when synthesized at a sintering temperature of 880°C. This system could potentially be used for low-temperature co-fired ceramics technology applications.  相似文献   

19.
Boron diffusion and the vapor-phase deposition of silicon layers are used to prepare ultrashallow p+-n junctions and p+-Si-n-CdF2 heterostructures on an n-CdF2 crystal surface. Forward portions of the IV characteristics of the p+-n junctions and p+-Si-n-CdF2 heterojunctions reveal the CdF2 band gap (7.8 eV), as well as allow the identification of the valence-band structure of cadmium fluoride crystals. Under conditions in which forward bias is applied to the p+-Si-n-CdF2 heterojunctions, electroluminescence spectra are measured for the first time in the visible spectral region.  相似文献   

20.
The effect of chemical treatment in saturated vapors of ammonia and acetone on the spectral composition and intensity of photoluminescence in porous SiO x films containing Si nanocrystals (nc-Si) is studied. The porosity of the SiO x films is provided by oblique vacuum deposition of thermally evaporated silicon or silicon monoxide on polished silicon substrates. The kinetics of adsorption of the vapors is monitored by variations in the frequency of a quartz oscillator on which the films to be studied are deposited. As a result of chemical treatment followed by high-temperature annealing of the SiO x films at the temperature 950°C, a new band, absent from the as-prepared films, appears in the photoluminescence spectrum at shorter wavelengths. The peak position and intensity of the band depend, correspondingly, on the composition of the film and on the time duration of the treatment. It is found that the new photoluminescence band is quenched upon exposure to laser radiation at the wavelength 488 nm. The quenching is more pronounced at the band peak. The possibility of controlling the characteristics of photoluminescence of the porous structures by chemical treatment is shown.  相似文献   